journal article·2009-11

Colorimetric and vibrational spectroscopic characterization of weathered surfaces of wood and rigid polyvinyl chloride–wood flour composite lumber

Paul Filson, Benjamin E. Dawson-Andoh, Laurent Matuana

Wood Science and Technology· Volume 43· Issue 7-8
Publisher page

Abstract

Rigid polyvinyl chloride-wood flour composite lumber containing either pine or maple wood flour and pine and maple lumber was subjected to accelerated weathering according to the ASTM Standard G 53 protocol. Non-weathered and weathered surfaces of all specimens were analyzed using colorimetric methods, reflectance infrared Fourier transform and Raman spectroscopic techniques. In the FT-IR spectra, conjugated ketones (1,744 cm⁻¹) of lignin as evidenced by their skeletal vibrations (1,560-1,500 cm⁻¹) and stretching (1,440-1,500 cm⁻¹) were reduced in weathered specimens. Cellulose was largely unaffected by weathering. C-O bending vibrations at 1,040 cm⁻¹ from holocellulose in pine specimens and intensity bands at 1,125-1,090 and 1,360 cm⁻¹ (C-O stretching and O-H bending from cellulose) in the maple and wood-plastic composite (WPC)-maple specimens were unaffected. A band at 1,650 cm⁻¹ became prominent after weathering of both pine and maple WPC specimens which is due to C=C-C=C stretching vibration of weathered PVC portion of the specimen. Raman shifts at 530 and 840-900 cm⁻¹ are attributed to C-O and C-C-O stretching in cellulose (remain unchanged). The role of extractives in weathering of pine is shown by the disappearance of Raman shifts at 392 and 434 cm⁻¹ (C=C deformations in pine extractives) in weathered pine. One-Way ANOVA, between-group designs showed significant effect on brightness (L*), redness (a*) and yellowness (b*) for all treatments.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Advanced Cellulose Research Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Anderson EL, Pawlak Z, Owen NL, Feist WC (1991) Infrared studies of wood weathering. Part I: softwoods. Appl Spectrosc 45(4):641–64710.1366/0003702914336930 ↗
2. ASTM Standard G 23 (1996) Practices for operating light-exposure apparatus (carbon-arc type) with and without water for exposure of nonmetallic materials
3. Ayadi N, Lejeume F, Charrier F, Charrier B, Merlin A (2003) Color stability of heat-treated wood during artificial weathering. Holz Roh-Werkst 61:221–22610.1007/s00107-003-0389-2 ↗
4. Bowley HJ, Gerrard DL (1988) The use of laser Raman spectroscopy to study the degradation of poly(vinylchloride). Polym Degrad Stab 20:257–26910.1016/0141-3910(88)90072-9 ↗
5. Dawson-Andoh B, Wieman M, Matuana L, Baumgras J (2004) Infrared and colorimetric characterization of discolored kiln-dried hard maple limber. For Prod J 54(1):53–57
6. Eichhorn SJ, Sirichaisit J, Young RJ (2001) Deformation mechanisms in cellulose fibers, paper and wood. J Mater Sci 36:3129–313510.1023/A:1017969916020 ↗
7. Grupper A, Wilhelm P, Schiller M (2003) Degradation of poly(vinylchloride) with different additives, studies by micro Raman spectroscopy. Polym Polym Compost 11(2):123–132
8. Kuo M-L, McClelland JF, Luo S, Chien P-L, Walker RD, Hse C-Y (1988) Applications of infrared photo-acoustic spectroscopy for wood samples. Wood Fiber Sci 20(1):132–145
9. Nimz HH (1973) Chemistry of potential chromophoric groups in beech lignin. Tappi 56(5):124–126
10. Rowell RM (2005) Weathering of wood. In: Williams S (ed) Handbook of wood chemistry and wood composites. CRC Press, New York10.1201/9780203492437 ↗
11. Silverstein RM, Webster FX (1997) Spectrometric identification of organic compounds, 6th edn. Wiley, New York, pp 84–85
12. Sudiyani Y, Tsujiyama S-I, Imamura Y, Takahashi M, Minato K, Kajita H (1999) Chemical characteristics of surfaces of hardwood and softwood deteriorated by weathering. J Wood Sci 45(4):348–35310.1007/BF00833502 ↗
13. Sudiyani Y, Imamura Y, Doi S, Yamauchi S (2003) Infrared spectroscopic investigations of weathering effects on the surface of tropical wood. J Wood Sci 49:86–9210.1007/s100860300014 ↗
14. Tolvaj L, Faix O (1995) Artificial ageing of wood monitored by DRIFT spectroscopy and CIE L a* b* color measurements. Holzforschung 49(5):397–40410.1515/hfsg.1995.49.5.397 ↗
15. Wypych G (2003) Data on specific polymers. In: Handbook of material weathering, 3rd edn. William Andrew Publishing, New York
16. Yazaki Y, Bauch J, Endeward R (1985) Extractive components responsible for the discoloration of Ilomba (Pycnanthus angolenesis Exell.). Holz Roh-Werkst 43:359–36310.1007/BF02607902 ↗