journal article·2015-05

Hydrogel-based boron salt formulations for wood preservation

Firmin Obounou-Akong, Philippe Gérardin, Marie-France Thévenon, Christine Gérardin-Charbonnier

Wood Science and Technology· Volume 49· Issue 3
Publisher page

Abstract

Mixing boron with two thermoreversible hydrogels, obtained from an amphiphilic tripeptide and a carbamate derivative of glycerol, respectively, allows the formation of a supramolecular network that incorporates boron and significant amounts of water upon gelification of the solution when the temperature decreases. Hydrogels obtained from these gelators were impregnated in pine sapwood blocks using vacuum pressure treatment and subjected to leaching. Results indicated that incorporation of boron salts in the hydrogel network effectively protected the wood from degradation caused by the brown rot fungus Poria placenta and from attack by termites also even after leaching. It is believed that these hydrogels fill the tracheid cell walls and lumens, limiting the leachability of boron salts when the wood is humidified.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Supramolecular Self-Assembly in Materials · Polydiacetylene-based materials and applications · Polymer composites and self-healing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. AWPA (2008) A7-04 Standard for wet ashing procedures for preparing wood for chemical analysis. American Wood Protection Association Standard, Birmingham
2. Baysal E, Ozaki SK, Yalinkilic MK (2004) Dimensional stabilization of wood treated with furfuryl alcohol catalysed by borates. Wood Sci Technol 38(6):405–415
3. Drysdale AJ (1994) Boron treatments for the preservation of wood—a review of efficacy data for fungi and termites. Document No. IRG/WP 94-30037. International Research Group on Wood Preservation, Stockholm
4. Ellis ET (1965) Inorganic elements in wood. In: Côte WA Jr (ed) Cellular ultrastructure of woody plants. Syracuse University Press, New York, pp 181–189
5. European Committee for Standardization (1986) Wood preservatives—determination of toxic values of wood preservatives against wood destroying basidiomycetes cultured on agar medium. NF EN 113. AFNOR
6. European Committee for Standardization (1990) Wood preservatives—determination of toxic values against Reticulitermes santonensis de Feytaud (laboratory method). NF EN 117. AFNOR
7. European Committee for Standardization (1994) Wood preservatives—methods for measuring losses of active ingredients and other preservative ingredients from treated timber—part 2: laboratory method for obtaining samples for analysis to measure losses by leaching into water or synthetic sea water. ENV 1250-2, Brussels, Belgium
8. European Committee for Standardization (2007) Durability of wood and wood-based products—definition of use classes—part 2: application to solid wood. EN 335-2. AFNOR
9. Gezer ED, Michael JH, Morrell JJ (1999) Effects of glycol on leachability and efficacy of boron wood preservatives. Wood Fiber Sci 31(2):136–142
10. Gizzi P, Pasc A, Dupuy N, Parant S, Henry B, Gérardin C (2009) Molecular tailored histidine-based complexing surfactants: from micelles to hydrogels. Eur J Org Chem 23:3953–396310.1002/ejoc.200900137 ↗
11. Kartal SN, Green F (2003) Leachability of boron from wood treated with natural and semi-synthetic polymers and calcium precipitating agent. Holz Roh Werkst 61(5):388–38910.1007/s00107-003-0413-6 ↗
12. Kartal SN, Imamura Y (2004) Effects of N′-N-(1,8-naphthalyl)hydroxylamine (NHA-Na) and hydroxynaphthalimide (NHA-H) on boron leachability and biological degradation of wood. Holz Roh Werkst 62(5):378–38510.1007/s00107-004-0500-3 ↗
13. Kartal SN, Yoshimura T, Imamura Y (2004) Decay and termite resistance of boron-treated and chemically modified wood by in situ co-polymerisation of allyl glycidyl ether (AGE) with methyl methacrylate (MMA). Int Biodeter Biodegr 53:111–11710.1016/j.ibiod.2003.09.004 ↗
14. Kartal SN, Yoshimura T, Imamura Y (2009) Modification of wood with Si compounds to limit boron leaching from treated wood and to increase termite decay resistance. Int Biodegr Biodeter 63(2):187–19010.1016/j.ibiod.2008.08.006 ↗
15. Lloyd JD (1997) International status of borate preservatives systems. Proceeding of Second international conference on wood protection with diffusible preservation and pesticides, Forest Products Society, Mobile, Alabama, USA, pp 45–54
16. Lloyd JD (1998) Borates and their biological applications. Document No. IRG/WP 98-30178. International Research Group on Wood Preservation, Stockholm
17. Lloyd JD, Dickinson DJ, Murphy RJ (1990) The probable mechanisms of action of boric acid and borates as wood preservatives. Document No. IRG/WP 1450. International Research Group on Wood Preservation, Stockholm
18. Loos M, Feringa BL, Van Esch JH (2005) Design and application of self-assembled low molecular weight hydrogels. Eur J Org Chem 17:3615–363110.1002/ejoc.200400723 ↗
19. Mitra RN, Das D, Roy S, Das PK (2007) Structure and properties of low molecular weight amphiphilic peptide hydrogelators. J Phys Chem B 111(51):14107–1411310.1021/jp076495x ↗
20. Mohareb A, Van Acker J, Stevens M (2002) Effect of protective additives on leachability and efficacy of borate treated wood. Document No. IRG/WP 02-30290. International Research Group on Wood Preservation, Stockholm
21. Mohareb A, Thévenon M-F, Wozniak E, Gérardin P (2010) Effects of monoglycerides on leachability and efficacy of boron wood preservatives against decay and termites. Int Biodeter Biodegr 64(2):135–13810.1016/j.ibiod.2009.12.004 ↗
22. Mohareb A, Thévenon M-F, Wozniak E, Gérardin P (2011) Effects of polyvinyl alcohol on leachability and efficacy of boron wood preservatives against fungal decay and termites attack. Wood Sci Technol 45(2):369–38210.1007/s00226-010-0324-8 ↗
23. Mourant D, Yang DQ, Lu X, Riedl B, Roy C (2009) Copper and boron fixation in wood by pyrolytic resins. Bioresour Technol 100(3):1442–144910.1016/j.biortech.2008.08.021 ↗
24. Naskar J, Palui G, Banerjee A (2009) Tetrapeptide based hydrogels: for encapsulation and slow release for an anticancer drug at physiological pH. J Phys Chem B 113(35):11787–1179210.1021/jp904251j ↗
25. Obanda DN, Shupe FT, Barnes HM (2008) Reducing leaching of boron based wood preservatives—a review of research. Bioresour Technol 99(15):7312–732210.1016/j.biortech.2007.12.077 ↗
26. Obounou-Akong F, Gérardin P, Gérardin-Charbonnier C (2012) Smart hydrogels from low molecular weight amphiphilic compounds: toward a solution to decrease leachability and increase efficacy of boron preservatives? Document No. IRG/WP 12-30589. International Research Group on Wood Protection, Kuala Lumpur
27. Obounou-Akong F, Pasc A, Mutlu M, Cosgun S, Gerardin-Charbonnier C (2013a) Hydrogels obtained from an original catanionic system for efficient formulation of boron wood-preservatives. J Int Biodegr Biodeter 77:123–12610.1016/j.ibiod.2012.06.029 ↗
28. Obounou-Akong F, Pasc A, Emo M, Gérardin-Charbonnier C (2013b) A supramolecular hydrogel based on an original pseudopeptidic catanionic surfactant. New J Chem 37:559–56210.1039/C2NJ40960G ↗
29. Pal A, Dey J (2011) Water-induced physical gelation of organic solvents by N-(n Alkylcarbamoyl)-l-alanine amphiphiles. Langmuir 27(7):3401–340810.1021/la105027b ↗
30. Pasc A, Gizzi P, Dupuy N, Parant S, Henry B, Gérardin C (2009) Microscopic and macroscopic anisotropy in supramolecular hydrogels of histidine-based surfactants. Tetrahedron Lett 50(45):6183–618610.1016/j.tetlet.2009.08.093 ↗
31. Pasc A, Obounou-Akong F, Cosgun S, Gérardin C (2010) Differences between β-Ala and Gly-Gly in the design of amino acids-based hydrogels. Beilstein J Org Chem 6:973–97710.3762/bjoc.6.109 ↗
32. Patra T, Pal A, Dey J (2010) A smart supramolecular hydrogel of N-(4-n-Alkyloxybenzoyl)-l-histidine exhibiting pH-modulated properties. Langmuir 26(11):7761–776710.1021/la904540x ↗
33. Pezron E, Richard A, Lafuma F, Audebert R (1988) Reversible gel formation induced by ion complexation. 1. Borax-galactomannan interactions. Macromolecules 21(4):1121–112510.1021/ma00182a045 ↗
34. Sagawa T, Chowdhury S, Takafuji M, Ihara H (2006) Self-assembled nanofibrillar aggregates with amphiphilic and lipophilic molecules. Macromol Symp 237(1):28–3810.1002/masy.200650504 ↗
35. Sangeetha NM, Maitra U (2005) Supramolecular gels: functions and uses. Chem Soc Rev 34(10):821–83610.1039/b417081b ↗
36. Schoeman WM, Lloyd JD (1998) International standardisation: a hypothetical case study with stand-alone borate wood preservatives. Document No. IRG/WP 98-20147. International Research Group on Wood Preservation, Stockholm
37. Steed J (2011) Supramolecular gel chemistry: developments over the last decade. Chem Commun 47(5):1379–138310.1039/C0CC03293J ↗
38. Temiz A, Alfredsen G, Eikenes M, Terziev N (2008) Decay resistance of wood treated with boric acid and tall oil derivates. Bioresour Technol 99(7):2102–210610.1016/j.biortech.2007.08.052 ↗
39. Terech P, Weiss RG (1997) Low molecular mass gelators of organic liquids and the properties of their gels. Chem Rev 97(8):3133–316010.1021/cr9700282 ↗
40. Thévenon M-F, Pizzi A (2003) Polyborate ions’ influence on the durability of wood treated with non-toxic protein borate preservatives. Holz Roh Werkst 61(6):457–46410.1007/s00107-003-0421-6 ↗
41. Thevenon M-F, Pizzi A, Haluk JP (1998) Protein borates as non-toxic, long-term, wide-spectrum, ground-contact wood preservatives. Holzforschung 52(3):241–24810.1515/hfsg.1998.52.3.241 ↗
42. Thévenon M-F, Pizzi A, Haluk JP (1997) Non-toxic albumin and soya protein borates as ground-contact wood preservatives. Holz Roh Werkst 55(5):293–29610.1007/s001070050231 ↗
43. Toussaint-Dauvergne E, Soulounganga P, Gérardin P, Loubinoux B (2000) Glycerol/glyoxal: a new boron fixation system for wood preservation and dimensional stabilization. Holzforschung 54(2):123–12610.1515/HF.2000.021 ↗
44. Yang Z, Xu B (2007) Supramolecular hydrogels based on biofunctional nanofibers of self-assembled small molecules. J Mater Chem 17(23):2385–239310.1039/b702493b ↗