Large-scale and high-resolution visualization of static mechanical properties of wood-adhesive interphase utilizing nanoindentation mapping
Source abstract
Abstract
To improve the mechanical performance of wooden engineered composites, more information is needed to understand the relationship between adhesive infiltration and mechanical properties of wood-adhesive interphase. Nanoindentation mapping (NI Mapping) was hereby used to achieve large-scale and high-resolution visualization of mechanical properties of wood-adhesive interphase for establishing the basic understanding of such correlation, and it showed the convincible reliability (variation less than 3% as compared with commonly applied NI methodology) and exceptional efficiency (180 min of total analysis time as compared with more than 3000 min using the commonly applied NI methodology). Successful investigation into the distribution of mechanical properties of wood-phenolic resin (wood-PF) and wood-polyurethane (wood-PUR) interphases using NI Mapping has confirmed that gradient elevation in mechanical properties of cell wall in wood-adhesive interphase is related to adhesive infiltration. PF adhesive exhibits favored infiltration which led to the enlarged wood-PF interphase region (over 60 μm) and improved micro-/macro-mechanical properties. NI Mapping was also applied for revealing mechanical performance of early wood-adhesive interphase which cannot be characterized by commonly applied NI methodology due to its small size. The mechanical properties of cell wall in early wood-adhesive interphase are poor; however, the interphase region would be enlarged due to the large lumen of early wood. NI Mapping can be a powerful tool to provide significant insights into the mechanical properties of wood-adhesive interphase, and thus, to improve the knowledge of the adhesive infiltration and mechanical properties of cell wall.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Natural Fiber Reinforced Composites · Advanced Cellulose Research Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Aicher S, Hirsch M, Christian Z (2016) Hybrid cross-laminated timber plates with beech wood cross-layers. Constr Build Mater 124:1007–101810.1016/j.conbuildmat.2016.08.051 ↗
2. Altgen D, Grigsby W, Altgen M et al (2019) Analyzing the UF resin distribution in particleboards by confocal laser scanning microscopy. Compos Part A-Appl s 125:10552910.1016/j.compositesa.2019.105529 ↗
3. Baldan A (2012) Adhesion phenomena in bonded joints. Int J Adhes Adhes 38:95–11610.1016/j.ijadhadh.2012.04.007 ↗
4. Beaulieu J, Dutilleul P (2019) Applications of computed tomography (CT) scanning technology in forest research: a timely update and review. Can J Forest Res 49(10):1173–118810.1139/cjfr-2018-0537 ↗
5. Cao Y, Zhang W, Yang P et al (2021) Comparative investigation into the interfacial adhesion of plywood prepared by air spray atomization and roller coating. Eur J Wood Prod 79(4):887–89610.1007/s00107-021-01681-7 ↗
6. Evans P, Morrison O, Senden T et al (2010) Visualization and numerical analysis of adhesive distribution in particleboard using X-ray micro-computed tomography. Int J Adhes Adhes 30(8):754–76210.1016/j.ijadhadh.2010.08.001 ↗
7. Frihart R (2013) Wood adhesion and adhesives. Crc Press-Taylor & Francis Group, Boca Raton
8. Gindl S, Jeronimidis G (2004) The interphase in phenol–formaldehyde and polymeric methylene diphenyldiisocyanate glue lines in wood. Int J Adhes Adhes 24:279–28610.1016/j.ijadhadh.2003.10.002 ↗
9. Gavrilovic-Grmusa I, Dunky M, Miljkovic J et al (2012) Influence of the viscosity of UF resins on the radial and tangential penetration into poplar wood and on the shear strength of adhesive joints. Holzforschung 66(7):849–85610.1515/hf-2011-0177 ↗
10. Gindl W, Sretenovic A, Vincenti A et al (2005) Direct measurement of strain distribution along a wood bond line. Part 2: Effects of adhesive penetration on strain distribution. Holzforschung 59(3):307–31010.1515/HF.2005.051 ↗
11. Herzele S, van Herwijnen G, Edler M et al (2018) Cell-layer dependent adhesion differences in wood bonds. Compos Part A-Appl s 114:21–2910.1016/j.compositesa.2018.07.037 ↗
12. Herzele S, van Herwijnen H, Griesser T et al (2020) Differences in adhesion between 1C-PUR and MUF wood adhesives to (ligno)cellulosic surfaces revealed by nanoindentation. Int J Adhes Adhes 98:10250710.1016/j.ijadhadh.2019.102507 ↗
13. Huang Y, Yang Z, Ren W et al (2015) 3D meso-scale fracture modelling and validation of concrete based on in-situ X-ray Computed Tomography images using damage plasticity model. Int J Solids Struct 67–68:340–35210.1016/j.ijsolstr.2015.05.002 ↗
14. Jakes J, Frihart C, Hunt C et al (2019) X-ray methods to observe and quantify adhesive penetration into wood. J Mater Sci 54(1):705–71810.1007/s10853-018-2783-5 ↗
15. Jakes J, Frihart R, Beecher F et al (2008) Experimental method to account for structural compliance in nanoindentation measurements. J Mater Res 23(4):1113–112710.1557/jmr.2008.0131 ↗
16. Jakes J, Hunt G, Yelle J et al (2015) Synchrotron-based X-ray fluorescence microscopy in conjunction with nanoindentation to study molecular-scale interactions of phenol-formaldehyde in wood cell walls. ACS Appl Mater Interfaces 7(12):6584–658910.1021/am5087598 ↗
17. Jakes J, Stone D (2021) Best practices for Quasistatic Berkovich Nanoindentation of Wood Cell Walls. Forests 12(12):169610.3390/f12121696 ↗
18. Kamke F (2007) Adhesive penetration in wood—a review. Wood Fiber Sci 39(2):205–220
19. Kamke F, Nairn J, Muszynski L et al (2014) Methodology for micromechanical analysis of wood adhesive bonds using X-ray computed tomography and numerical modeling. Wood Fiber Sci 46(1):15–28
20. Kläusler O, Bergmeier W, Karbach A et al (2014) Influence of N, N-dimethylformamide on one-component moisture-curing polyurethane wood adhesives. Int J Adhes Adhes 55:69–7610.1016/j.ijadhadh.2014.07.019 ↗
21. Konnerth J (2014) Effect of plasma treatment on cell-wall adhesion of urea-formaldehyde resin revealed by Nanoindentation. Holzforschung 68(6):707–71210.1515/hf-2013-0130 ↗
22. Konnerth J, Gindl W (2006) Mechanical characterisation of wood-adhesive interphase cell walls by nanoindentation. Holzforschung 60(4):429–43310.1515/HF.2006.067 ↗
23. Konnerth J, Valla A, Gindl W (2007) Nanoindentation mapping of a wood-adhesive bond. Appl Phys a: Mater Sci Process 88(2):371–37510.1007/s00339-007-3976-y ↗
24. Kutukova K, Niese S, Sander C et al (2018) A laboratory X-ray microscopy study of cracks in on-chip interconnect stacks of integrated circuits. Appl Phys Lett 113(9):09190110.1063/1.5031204 ↗
25. Li A, Jiang J, Lu J (2019) Differences in the viscoelastic properties between earlywood and latewood in the growth rings of Chinese fir as analyzed by dynamic mechanical analysis (DMA) in the temperature range between-120 degrees C and 120 degrees C. Holzforschung 73(3):241–25010.1515/hf-2018-0054 ↗
26. Li Q, Li Y, Zhou L (2017) Nanoscale evaluation of multi-layer interfacial mechanical properties of sisal fiber reinforced composites by nanoindentation technique. Compos Sci Technol 152:211–22110.1016/j.compscitech.2017.09.030 ↗
27. Li W, Wang M, Cheng J (2020) Indentation hardness of the cohesive-frictional materials. Int J Mech Sci 180:10566610.1016/j.ijmecsci.2020.105666 ↗
28. Li X, Bhushan B (2002) A review of nanoindentation continuous stiffness measurement technique and its applications. Mater Charact 48:11–3610.1016/S1044-5803(02)00192-4 ↗
29. Liu C, Zhang Y, Wang S et al (2014) Micromechanical Properties of the Interphase in Cellulose Nanofiber-reinforced Phenol Formaldehyde Bondlines. BioResources 9(3):5529–5541
30. Liu H, Shang J, Kamke F et al (2018) Bonding performance and mechanism of thermal-hydro-mechanical modified veneer. Wood Sci Technol 52(2):343–36310.1007/s00226-017-0982-x ↗
31. Liu Z, Zhang J, He B et al (2021) High-speed nanoindentation mapping of a near-alpha titanium alloy made by additive manufacturing. J Mater Res 36(11):2223–223410.1557/s43578-021-00204-7 ↗
32. McKinley P, Kamke F, Sinha A et al (2018) Analysis of adhesive penetration into wood using nano-X-Ray computed tomography. Wood Fiber Sci 50(1):66–7610.22382/wfs-2018-007 ↗
33. Obersriebnig M, Konnerth J, Gindl-Altmutter W (2013) Evaluating fundamental position-dependent differences in wood cell wall adhesion using nanoindentation. Int J Adhes Adhes 40:129–13410.1016/j.ijadhadh.2012.08.011 ↗
34. Obersriebnig M, Veigel S, Gindl-Altmutter W et al (2012) Determination of adhesive energy at the wood cell-wall/UF interface by nanoindentation (NI). Holzforschung 66(6):781–78710.1515/hf-2011-0205 ↗
35. Oliver W, Pharr G (1992) An improved technique for determing hardness and elastic-modulus using load and displacement sensing indentation experiments. J Mater Res 7(6):1564–158310.1557/JMR.1992.1564 ↗
36. Oliver W, Pharr G (2004) Measurement of hardness and elastic modulus by instrumented indentation: Advances in understanding and refinements to methodology. J Mater Res 19(1):3–2010.1557/jmr.2004.19.1.3 ↗
37. Phani P, Oliver W, Pharr G (2021) Measurement of hardness and elastic modulus by load and depth sensing indentation: improvements to the technique based on continuous stiffness measurement. J Mater Res 36(11):2137–215310.1557/s43578-021-00131-7 ↗
38. Qi D, Hu W, Xin K et al. (2020) In-situ synchrotron X-ray tomography investigation of micro lattice manufactured with the projection micro-stereolithography (P mu SL) 3D printing technique: Defects characterization and in-situ shear test. Compos Struct 252 (112710)10.1016/j.compstruct.2020.112710 ↗
39. Serrano E, Enquist B (2005) Contact-free measurement and non-linear finite element analyses of strain distribution along wood adhesive bonds. Holzforschung 59:641–64710.1515/HF.2005.103 ↗
40. Singh A, Nuryawan A, Park B et al (2015) Urea-formaldehyde resin penetration into Pinus radiata tracheid walls assessed by TEM-EDXS. Holzforschung 69(3):303–30610.1515/hf-2014-0103 ↗
41. Szewczykowski P, Skarzynski L (2019) Application of the X-ray micro-computed tomography to the analysis of the structure of polymeric materials. Polimery 64(1):12–2210.14314/polimery.2019.1.2 ↗
42. Vignesh B, Oliver W, Kumar G et al (2019) Critical assessment of high speed nanoindentation mapping technique and data deconvolution on thermal barrier coatings. Mater Des 181:10808410.1016/j.matdes.2019.108084 ↗
43. Wang X, Chen X, Xie X et al (2018a) Effects of thermal modification on the physical, chemical and micromechanical properties of Masson pine wood (Pinus massoniana Lamb.). Holzforschung 72(12):1063–107010.1515/hf-2017-0205 ↗
44. Wang X, Zhao L, Deng Y et al (2018b) Effect of the penetration of isocyanates (pMDI) on the nanomechanics of wood cell wall evaluated by AFM-IR and nanoindentation (NI). Holzforschung 72(4):301–30910.1515/hf-2017-0123 ↗
45. Wang X, Deng Y, Li Y et al (2016) In situ identification of the molecular-scale interactions of phenol-formaldehyde resin and wood cell walls using infrared nanospectroscopy. RSC Adv 6(80):76318–7632410.1039/C6RA13159J ↗
46. Wang X, Wang S, Xie X et al (2017a) Multi-scale evaluation of the effects of nanoclay on the mechanical properties of wood/phenol formaldehyde bondlines. Int J Adhes Adhes 74:92–9910.1016/j.ijadhadh.2017.01.004 ↗
47. Wang X, Zhao L, Xu B et al (2017b) Effects of accelerated aging treatment on the microstructure and mechanics of wood-resin interphase. Holzforschung 72(3):235–24110.1515/hf-2017-0068 ↗
48. Wascher R, Bittner F, Avramidis G et al (2020) Use of computed tomography to determine penetration paths and the distribution of melamine resin in thermally-modified beech veneers after plasma treatment. Compos Part A-Appl S 132:10582110.1016/j.compositesa.2020.105821 ↗
49. Wimmer R, Lucas B (1997) Comparing mechanical properties of secondary wall and cell corner middle lamella in spruce wood. IAWA J 18(1):77–8810.1163/22941932-90001463 ↗
50. Wu Y, Zhang H, Yang L et al (2021) Understanding the effect of extractives on the mechanical properties of the waterborne coating on wood surface by nanoindentation 3D mapping. J Mater Sci 56(2):1401–141210.1007/s10853-020-05347-2 ↗
51. Yu Z, Fan M (2017) Short- and long-term performance of wood based panel products subjected to various stress modes. Constr Build Mater 156:652–66010.1016/j.conbuildmat.2017.09.025 ↗
52. Zauner M, Keunecke D, Mokso R et al (2012) Synchrotron-based tomographic microscopy (SbTM) of wood: development of a testing device and observation of plastic deformation of uniaxially compressed Norway spruce samples. Holzforschung 66(8):973–97910.1515/hf-2011-0192 ↗
53. Zhang T, Bai S, Zhang Y et al (2012) Viscoelastic properties of wood materials characterized by nanoindentation experiments. Wood Sci Technol 46(5):1003–101610.1007/s00226-011-0458-3 ↗
54. Zhang X, Zhao Q, Wang S et al (2010) Characterizing strength and fracture of wood cell wall through uniaxial micro-compression test. Compos Part A-Appl s 41(5):632–63810.1016/j.compositesa.2010.01.010 ↗
55. Zhang Z, Cai S, Li Y et al (2020) High performances of plant fiber reinforced composites-A new insight from hierarchical microstructures. Compos Sci Technol 194:10815110.1016/j.compscitech.2020.108151 ↗