Comparative studies on the durability and moisture performance of wood modified with cyclic N-methylol and N-methyl compounds
Source abstract
Abstract
Abstract Glyoxal-based condensation resins like 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU) have been used to modify wood and improve its resistance against decaying fungi. High biological durability of DMDHEU-treated wood has already been confirmed in laboratory and field tests in the past. However, the modes of protective action behind an improved decay resistance are not fully understood yet. Furthermore, it is questionable how the use of formaldehyde-poor N-methylol and formaldehyde-free N-methyl compounds instead of DMDHEU affects the moisture behavior and durability, respectively. In this study, wood blocks were treated with N-methylol (DMDHEU, methylated DMDHEU) and N-methyl compounds (1,3-dimethyl-4,5-dihydroxyethyleneurea; DMeDHEU). Untreated and modified specimens were exposed to different moisture regimes and wood-destroying fungi in order to study the indicators that control changes in the wetting ability and decay resistance. Both N-methylol and N-methyl compounds decreased the water uptake and release and increased the durability of Scots pine sapwood from ‘not durable’ (DC 5) to ‘very durable to durable’ (DC 1–2). However, high fluctuations were observed in water uptake and release as well as mass loss (ML) caused by fungal decay, when modified specimens were tested without passing through a cold-water leaching. Consequently, a significant effect of the leaching procedure according to EN 84 on the durability classification could be established. The latter appeared more pronounced for treatments with N-methyl compounds compared to N-methylol compounds. Finally, wetting ability (kwa) and resistance indicating factors (kinh) enabled a forecast of high biological durability for both treatments with N-methylol and N-methyl compounds under real service life conditions.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Wood and Agarwood Research · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Alfredsen G, Brischke C, Marais BN, Stein RF, Zimmer K, Humar M (2021) Modelling the material resistance of wood—Part 1: utilizing durability test data based on different reference wood species. Forests 12:55810.3390/f12050558 ↗
2. Alfredsen G, Flæte PO, Militz H (2013) Decay resistance of acetic anhydride modified wood: a review. Int Wood Prod J 4:137–14310.1179/2042645313Y.0000000034 ↗
3. Alfredsen G, Ringman R, Pilgård A, Fossdal CG (2015) New insight regarding mode of action of brown rot decay of modified wood based on DNA and gene expression studies: a review. Int Wood Prod J 6:5–710.1179/2042645314Y.0000000085 ↗
4. Andrews BA, Trask-Morrell BJ (1997) Long term formaldehyde emissions from DMDHEU-finished cotton fabrics. Text Chem Color 29:16–19
5. Bajaj P (2002) Finishing of textile materials. J Appl Polym Sci 83:631–65910.1002/app.2262 ↗
6. Bollmus S (2011) Biologische und technologische Eigenschaften von Buchenholz nach einer Modifizierung mit 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU) [Biological and technological properties of beech after modification with 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU)]. Ph.D. thesis. Goettingen, Germany, University of Goettingen
7. Bollmus S, Bächle L, Brischke C, Militz H (2019) Durability classification of preservative treated and modified wood. The International Research Group on Wood Protection, Stockholm, IRG/WP/19–20659
8. Brelid PL, Westin M (2007) Acetylated wood—results from long-term field tests. In: Proceedings of the 3rd European conference on wood modification, Bangor, United Kingdom, pp 71–78
9. Brischke C, Alfredsen G, Humar M, Conti E, Cookson L, Emmerich L, Flæte PO, Fortino S, Francis L, Hundhausen U, Irbe I, Jacobs K, Klamer M, Kržišnik D, Lesar B, Melcher E, Meyer-Veltrup L, Morrell JJ, Norton J, Palanti S, Presley G, Reinprecht L, Singh T, Stirling R, Venäläinen M, Westin M, Wong AHH, Suttie E (2021) Modeling the material resistance of wood—Part 2: validation and optimization of the Meyer-Veltrup model. Forests 12:57610.3390/f12050576 ↗
10. CEN/TS 15083-2 (2005) Durability of wood and wood-based products - Determination of the natural durability of solid wood against wood-destroying fungi, test methods - Part 2: Soft rotting micro-fungi. CEN (European committee for standardization), Brussels, Belgium
11. Dhiman G, Chakraborty JN (2017) Assessment of durable press performance of cotton finished with modified DMDHEU and citric acid. Fash Text 4:1–1810.1186/s40691-017-0104-2 ↗
12. Emmerich L, Militz H (2020) Study on the impregnation quality of rubberwood (Hevea brasiliensis Müll. Arg.) and English oak (Quercus robur L.) sawn veneers after treatment with 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU). Holzforschung 74:362–37110.1515/hf-2019-0110 ↗
13. Emmerich L, Bollmus S, Militz H (2019) Wood modification with DMDHEU (1.3-dimethylol-4.5-dihydroxyethyleneurea)—state of the art, recent research activities and future perspectives. Wood Mater Sci Eng 14:3–1810.1080/17480272.2017.1417907 ↗
14. Emmerich L, Militz H, Brischke C (2020a) Long-term performance of DMDHEU-treated wood installed in different test set-ups in ground, above ground and in the marine environment. Int Wood Prod J 11:27–3710.1080/20426445.2020.1715553 ↗
15. Emmerich L, Altgen M, Rautkari L, Militz H (2020b) Sorption behavior and hydroxyl accessibility of wood treated with different cyclic N-methylol compounds. J Mater Sci 55:16561–1657510.1007/s10853-020-05224-y ↗
16. Emmerich L, Brischke C, Sievert M, Schulz MS, Jaeger AC, Beulshausen A, Humar M (2020c) Predicting the Outdoor Moisture Performance of Wood Based on Laboratory Indicators. Forests 11:100110.3390/f11091001 ↗
17. Emmerich L, Bleckmann M, Strohbusch S, Brischke C, Bollmus S, Militz H (2021) Growth behaviour of wood-destroying fungi in chemically modified wood: wood degradation and translocation of nitrogen compounds. Holzforschung Ahead-of-Print. https://doi.org/10.1515/hf-2020-025210.1515/hf-2020-0252 ↗
18. EN 84 (2020) Wood preservatives - Accelerated ageing of treated wood prior to biological testing - Leaching procedure. CEN (European committee for standardization), Brussels, Belgium
19. EN 113-2 (2021) Durability of wood and wood-based products – Test method against wood destroying basidiomycetes – Part 2: Assessment of inherent or enhanced durability. CEN (European committee for standardization), Brussels, Belgium
20. EN 252 (2015) Wood preservatives. Field test methods for determining the relative protective effectiveness in ground contact. CEN (European committee for standardization), Brussels, Belgium
21. EN 335 (2013) Durability of wood and wood-based products - Use classes: definitions, application to solid wood and wood-based products. CEN (European committee for standardization), Brussels, Belgium
22. EN 350 (2016) Durability of wood and wood-based products - Testing and classification of the resistance to biological agents, the permeability to water and the performance of wood and wood- based materials. CEN (European committee for standardization), Brussels, Belgium
23. EN 1609 (2013) Thermal insulating products for building applications - Determination of short term water absorption by partial immersion. CEN (European committee for standardization), Brussels, Belgium
24. Frick JG Jr (1985) Bonding in cotton fiber from formaldehyde-free crosslinks. J Appl Polym Sci 30:3467–347710.1002/app.1985.070300827 ↗
25. Frick JG Jr (1986) Effects of crosslink distribution in cotton fibers. Text Res J 56:124–13010.1177/004051758605600210 ↗
26. Gérardin P (2016) New alternatives for wood preservation based on thermal and chemical modification of wood—a review. Ann for Sci 73:559–57010.1007/s13595-015-0531-4 ↗
27. Holme I (1993) New developments in the chemical finishing of textiles. J Text Inst 84:520–53310.1080/00405009308658985 ↗
28. Hill CAS (2009) Why does acetylation protect wood from microbiological attack? Wood Mater Sci Eng 4:37–4510.1080/17480270903249409 ↗
29. Hill CAS (2011) Wood modification: an update. BioResources 6:918–91910.15376/biores.6.2.918-919 ↗
30. Isaksson T, Brischke C, Thelandersson S (2013) Development of decay performance models for outdoor timber structures. Mater Struct 46:1209–122510.1617/s11527-012-9965-4 ↗
31. Isaksson T, Thelandersson S, Jermer J, Brischke C (2014) Beständighet för utomhusträ ovan mark. Guide för utformning och materialval [Durability of wood exposed outdoors above ground. Guideline for design and material selection]. Report TVBK-3066, Division of Structural Engineering, Lund University
32. Jones D, Sandberg D (2020) A Review of Wood Modification Globally-Updated Findings from COST FP1407. Interdisciplinary Perspectives on the Built Environment 1:1–3110.37947/ipbe.2020.vol1.1 ↗
33. Jung HZ, Benerito RR, Gonzales EJ, Berni RJ (1969) Influence of structure of cyclic urea derivatives on their reactivities with cotton. J Appl Polym Sci 13:1949–196310.1002/app.1969.070130914 ↗
34. Krause A (2006) Holzmodifizierung mit N-Methylolvernetzern [Wood modification with N-methylol crosslinking agents]. Ph.D. thesis. Goettingen, Germany, University of Goettingen.
35. Krause A, Jones D, Van der Zee M, Militz H (2003) Interlace treatment—wood modification with N-methylol compounds. In: Proceedings of the first European conference on wood modification, Ghent, Belgium, 317–327
36. Meyer L, Brischke C, Preston A (2016) Testing the durability of timber above ground: a review on methodology. Wood Mater Sci Eng 11:283–30410.1080/17480272.2014.983163 ↗
37. Meyer-Veltrup L, Brischke C, Alfredsen G, Humar M, Flæte PO, Isaksson T, Brelid PL, Westin M, Jermer J (2017) The combined effect of wetting ability and durability on outdoor performance of wood: development and verification of a new prediction approach. Wood Sci Technol 51:615–63710.1007/s00226-017-0893-x ↗
38. Meyer L, Brischke C, Pilgård A (2012) Modified timber in various above ground exposures–durability and moisture performance. In: Proceedings of the 6th European conference on wood modification, Ljubljana, Slovenia, 137–144
39. Militz H (1993) Treatment of timber with water soluble dimethylol resins to improve their dimensional stability and durability. Wood Sci Technol 27:347–35510.1007/BF00192221 ↗
40. Naderpour F, Mirjalili SA, Sharzehee M (2009) The Investigation on the influence of DMDHEU on the Wrinkle and Abrasion Resistance of Cotton Fabrics using Image Processing. Text Res J 79:1571–157710.1177/0040517509104757 ↗
41. Paul R (Ed.) (2014) Functional finishes for textiles: improving comfort, performance and protection. Woodhead Publishing Series in Textiles. Elsevier. https://doi.org/10.1016/C2013-0-16373-810.1016/C2013-0-16373-8 ↗
42. Ringman R, Pilgård A, Brischke C, Richter K (2014) Mode of action of brown rot decay resistance in modified wood: a review. Holzforschung 68:239–24610.1515/hf-2013-0057 ↗
43. Ritschkoff AC, Rättö M, Nurmi A, Kokko H, Rapp A, Militz H (1999) Effect of some resin treatments on fungal degradation reactions. The International Research Group on Wood Protection, Stockholm, IRG/WP/99-10318
44. Rowell RM (2014) Acetylation of wood – A review. Int J Lignocellul Prod 1:1–27
45. Rowell RM (2012) Chemical modification of wood to produce stable and durable composites. Cell Chem Technol 46:443–448
46. Rowell RM, Dickerson JP (2014) Acetylation of wood. In: Deterioration and protection of sustainable biomaterials. American Chemical Society, pp 301–32710.1021/bk-2014-1158.ch018 ↗
47. Rowell RM, Ibach RE, McSweeny J, Nilsson T (2009) Understanding decay resistance, dimensional stability and strength changes in heat-treated and acetylated wood. Wood Mater Sci Eng 4:14–2210.1080/17480270903261339 ↗
48. Sandberg D, Kutnar A, Mantanis G (2017) Wood modification technologies-a review. Iforest 10:895–90810.3832/ifor2380-010 ↗
49. Schaffert S (2006) Steuerung und Optimierung von Holzvernetzungsprozessen [Control and optimization of wood crosslinking processes]. Ph.D. thesis. Goettingen, Germany, University of Goettingen.
50. Schindler WD, Hauser PJ (2004) Chemical finishing of textiles. Woodhead Publishing Ltd, Cambridge10.1533/9781845690373 ↗
51. Stamm AJ, Seborg RM (1936) Minimizing wood shrinkage and swelling. J Ind Eng Chem 28:1164–116910.1021/ie50322a009 ↗
52. Thybring EE, Piqueras S, Tarmian A, Burgert I (2020) Water accessibility to hydroxyls confined in solid wood cell walls. Cellulose 27:5617–562710.1007/s10570-020-03182-x ↗
53. Tomasino C (1992) Chemistry and technology of fabric preparation and finishing. North Carolina State University, Raleigh
54. Vanneste M (2014) Easy care finishes for textiles, Chapter 7. In: Paul R (ed) Functional Finishes for Textiles: Improving Comfort, Performance and Protection, Woodhead Publishing Series in Textiles Number 156. Elsevier, London, pp 227–256
55. Verma P, Junga U, Militz H, Mai C (2009) Protection mechanisms of DMDHEU treated wood against white and brown rot fungi. Holzforschung 63:371–37810.1515/HF.2009.051 ↗
56. Wepner F (2006) Entwicklung eines Modifizierungsverfahrens für Buchenfurniere (Fagus sylvatica L.) auf Basis von zyklischen N-Methylol-Verbindungen [Development of a wood modification process for beech veneers (Fagus sylvatica L.) on the basis of cyclic N-methylol compounds]. Ph.D. thesis. Goettingen, Germany, University of Goettingen.
57. Xie Y, Krause A, Mai C, Militz H, Richter K, Urban K, Evans PD (2005) Weathering of wood modified with the N-methylol compound 1,3-dimethylol-4,5-dihydroxyethyleneurea. Polym Degrad Stab 89:189–19910.1016/j.polymdegradstab.2004.08.017 ↗
58. Xie Y, Krause A, Militz H, Mai C (2008) Weathering of uncoated and coated wood treated with methylated 1,3-dimethylol-4,5-dihydroxyethyleneurea (mDMDHEU). Holz Roh Werkst 66:455–46410.1007/s00107-008-0270-4 ↗
59. Ziifle HM, Benerito RR, Gonzales EJ, Berni RJ (1968) Kinetics of the reactions of ethyleneurea derivatives with cotton cellulose: Part III: The cellulose-dimethyldihydroxyethyleneurea reaction. Text Res J 38:925–93010.1177/004051756803800907 ↗