journal article·2018-01

The influence of biodegradable magnesium implants on the growth plate

Tanja Kraus, Stefan Fischerauer, Stefan Treichler, Elisabeth Martinelli, Johannes Eichler, Anastasia Myrissa, Silvia Zötsch, Peter J. Uggowitzer, Jörg F. Löffler, Annelie M. Weinberg

Acta Biomaterialia· Volume 66
Publisher page

Abstract

Mg-based biodegradable materials are considered promising candidates in the paediatric field due to their favourable mechanical and biological properties and their biodegrading potential that makes a second surgery for implant removal unnecessary. In many cases the surgical fixation technique requires a crossing of the growth plate by the implant in order to achieve an adequate fragment replacement or fracture stabilisation. This study investigates the kinetics of slowly and rapidly degrading Mg alloys in a transphyseal rat model, and also reports on their dynamics in the context of the physis and consecutive bone growth. Twenty-six male Sprague-Dawley rats received either a rapidly degrading (ZX50; n = 13) or a slowly degrading (WZ21; n = 13) Mg alloy, implanted transphyseal into the distal femur. The contralateral leg was drilled in the same manner and served as a direct sham specimen. Degradation behaviour, gas formation, and leg length were measured by continuous in vivo micro CT for up to 52 weeks, and additional high-resolution µCT (HRS) scans and histomorphological analyses of the growth plate were performed. The growth plate was locally destroyed and bone growth was significantly diminished by the fast degradation of ZX50 implants and the accompanying release of large amounts of hydrogen gas. In contrast, WZ21 implants showed homogenous and moderate degradation performance, and the effect on bone growth did not differ significantly from a single drill-hole defect. Statement of significance This study is the first that reports on the effects of degrading magnesium implants on the growth plate in a living animal model. The results show that high evolution of hydrogen gas due to rapid Mg degradation can damage the growth plate substantially. Slow degradation, however, such as seen for WZ21 alloys, does not affect the growth plate more than drilling alone, thus meeting one important prerequisite for deployment in paediatric osteosynthesis.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Magnesium in Health and Disease · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
2. R. Salter Epiphyseal Plate Injuries, New York, 1994.
3. Statistical analysis of the incidence of physeal injuries10.1097/01241398-198709000-00003 ↗
4. Close reduction and intramedullary flexible titanium nails fixation of femoral shaft fractures in children under 5 years of age10.1097/01202412-200607000-00012 ↗
5. Removal of flexible titanium nails in children10.1097/01.bpo.0000218534.51609.aa ↗
6. G. Stroganov, T. Savitsky, M. Mikhailovich, V. Nina, V. Terekhova, et al., Magnesium-based alloys for use in bone surgery, US, 1972.
7. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
8. Bioabsorbable screw fixation for the treatment of ankle fractures10.1007/s00776-006-1077-y ↗
9. Long-term degradation of a poly-lactide co-glycolide/beta-tricalcium phosphate biocomposite interference screw10.1016/j.arthro.2010.11.056 ↗
10. MgZnCa glasses without clinically observable hydrogen evolution for biodegradable implants10.1038/nmat2542 ↗
11. High-strength (HSLA) Mg-Zn-Ca alloys with excellent biodegradation perfomrance10.1007/s11837-014-0875-5 ↗
12. On the in vitro and in vivo degradation performance and biological response of new biodegradable Mg-Y-Zn alloys10.1016/j.actbio.2009.10.008 ↗
13. Biodegradable implants in fracture fixation: early results of treatment of fractures of the ankle10.1016/S0140-6736(85)91847-1 ↗
14. Application of poly-L-lactide screws in flat foot surgery: histological and radiological aspects of bio-absorption of degradable devices
15. Magnesium alloys for temporary implants in osteosynthesis: in vivo studies of their degradation and interaction with bone10.1016/j.actbio.2011.11.008 ↗
16. Synthesis and characterization of Mg-Ca-Sr alloys for biodegradable orthopedic implant applications10.1002/jbm.b.32721 ↗
17. Effects of degradable Mg-Ca alloys on dendritic cell function10.1177/0885328209360424 ↗
18. In vitro degradation behaviour and cytocompatibility of Mg-Zn-Zr alloys10.1007/s10856-010-4111-8 ↗
19. New interests in magnesium
20. Histology and research at the hard tissue-implant interface using Technovit 9100 New embedding technique10.1016/j.actbio.2010.06.022 ↗
21. A. Myrissa, Biocompatibility analysis of different resorbable Magneisum allyos in a rat model (Doctoral thesis), 2016.
22. Disorders of the growth plate10.1097/MED.0b013e328331dca2 ↗
23. Early experience with biodegradable implants in pediatric patients10.1007/s11999-008-0537-4 ↗
24. Transphyseal bioabsorbable screws cause temporary growth retardation in rabbit femur10.1097/01.bpo.0000150845.02162.f7 ↗
25. Posttraumatic growth-plate abnormalities: MR imaging of bony-bridge formation in rabbits10.1148/radiology.175.3.2343128 ↗
26. Epiphyseal disorders10.1056/NEJM198712313172705 ↗
27. The effect of drilling and screw fixation of the growth plate–an experimental study in rabbits10.1002/jor.21463 ↗
28. Influence of trace impurities on the in vitro and in vivo degradation of biodegradable Mg-5Zn-0.3Ca alloys10.1016/j.actbio.2015.05.004 ↗
29. Design strategy for new bioabsorbable Mg-Y-Zn alloys for medical applications10.3139/146.110157 ↗
30. S. Syed Ali, The blood supply of the growth plate and the epiphysis: a comparative scanning electron microscopy and histological experimental study in growing sheep10.1007/s00223-001-2006-x ↗
31. Experimental epiphyseal injuries Grading of traumas and attempts at treating traumatic epiphyseal arrest in animals10.3109/17453676908989497 ↗
32. Long-term in vivo degradation behavior and near-implant distribution of resorbed elements for magnesium alloys WZ21 and ZX5010.1016/j.actbio.2016.06.025 ↗
33. Immunological response to biodegradable magnesium implants10.1007/s11837-014-0874-6 ↗