Abstract

A combination of bulk and surface modification of wood could lead to a product that shows the advantages of both treatments. This study evaluates the penetration of melamine resin into acetylated and silylated cell walls and possible side effects of melamine impregnation on this bulk treatment in order to clarify the feasibility of a combination of the chosen bulk modification (acetylation or silylation) and surface treatments (hardening by melamine modification). UV microscopy confirmed that melamine resin penetrates into wood cell walls even after acetylation and silylation treatment. Energy dispersive X-ray analysis showed that the melamine treatment did not lead to substantial washing out of silyl groups with the silylation reagent used. The possibility of a combination of the selected bulk and surface modification methods is given.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Natural Fiber Reinforced Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Birkofer L, Stuhl O (1989) General synthetic pathways to organosilicon compounds. In: Patai S, Rappoport Z (eds) The chemistry of organic silicon compounds. Part 1. Wiley, Chichester, pp 655–76210.1002/0470025107.ch10 ↗
2. Boonstra MG, Pizzi A, Tekely P, Pendlebury J (1996) Chemical modification of Norway spruce and Scots pine. A 13C NMR CP-MAS study of the reactivity and reactions of polymeric wood components with acetic anhydride. Holzforschung 50:215–22010.1515/hfsg.1996.50.3.215 ↗
3. Bower RK, Wellons JD (1974) Sorption of styrene and acrylonitrile by wood aerogels. Wood Sci 7:123–129
4. Brebner KI, Schneider MH (1985) Wood-polymer combinations: Bonding of alkoxysilane coupling agents to wood. Wood Sci Technol 19:75–8110.1007/BF00354755 ↗
5. Burger C, Kreuzer F-H (1996) Polysiloxanes and polymers containing siloxane groups. In: Kricheldorf HR (ed) Silicon in polymer synthesis. Springer, Berlin Heidelberg New York, pp 113–22210.1007/978-3-642-79175-8_3 ↗
6. Denes AR, Tshabalala MA, Rowell R, Denes F, Young A (1999) Hexamethyldisiloxane-plasma coating of wood surfaces for creating water repellent characteristics. Holzforschung 53:318–32610.1515/HF.1999.052 ↗
7. Gindl W, Gupta HS (2002) Cell-wall hardness and Young’s modulus of melamine-modified spruce wood by nano-indentation. Comp Part A Appl Sci Manuf 33:1141–114510.1016/S1359-835X(02)00080-5 ↗
8. Gindl W, Dessipri E, Wimmer R (2002) Using UV-microscopy to study diffusion of melamine-urea-formaldehyde resin in cell walls of spruce wood. Holzforschung 56:103–10710.1515/HF.2002.017 ↗
9. Gindl W, Müller U, Teischinger A (2003a) Transverse compression strength and fracture of spruce wood modified by melamine-formaldehyde impregnation of cell walls. Wood Fiber Sci 35:239–246
10. Gindl W, Zargar-Yaghubi F, Wimmer R (2003b) Impregnation of softwood cell walls with melamine-formaldehyde resin. Bioresour Technol 87:325–33010.1016/S0960-8524(02)00233-X ↗
11. Gindl W, Hansmann C, Gierlinger N, Schwanninger M, Hinterstoisser B, Jeronimidis G (2004) Using a water-soluble melamine-formaldehyde resin to improve the hardness of Norway spruce wood. J Appl Polym Sci 93:1900–190710.1002/app.20653 ↗
12. Hagstrand PO (1999) Mechanical analyses of melamine–formaldehyde composites. PhD thesis, Chalmer University of Technology10.3139/217.1548 ↗
13. Hansmann C, Schwanninger M, Stefke B, Hinterstoisser B, Gindl W (2004) UV-microscopic analysis of acetylated spruce and birch cell walls. Holzforschung 58:483–48810.1515/HF.2004.073 ↗
14. Hua L, Flodin P, Rönnhult T (1987b) Cellulose fiber–polyester composites with reduced water sensitivity (2)—surface analysis. Polym Comp 8:203–20710.1002/pc.750080309 ↗
15. Hua L, Zadorecki P, Flodin P (1987a) Cellulose fiber-polyester composites with reduced water sensitivity (1)—chemical treatment and mechanical properties. Polym Comp 8:199–20210.1002/pc.750080308 ↗
16. Inoue M, Ogata S, Nishikawa M, Otsuka Y, Kawai S, Norimoto M (1993) Dimensional stability, mechanical properties and color changes of a low molecular weight melamine-formaldehyde resin impregnated wood. Mokuzai Gakkaishi 39:181–189
17. Kricheldorf HR (1996) Appendix B: Silylation and silylating agents. In: Kricheldorf HR (ed) Silicon in polymer synthesis. Springer, Berlin Heidelberg New York, pp 469–49110.1007/978-3-642-79175-8 ↗
18. Lukowsky D (1999) Holzschutz mit Melaminharzen. PhD Thesis, University of Hamburg
19. Mai C, Militz H (2004) Modification of wood with silicon compounds. Treatment systems based on organic silicon compounds—a review. Wood Sci Technol 37:453–46110.1007/s00226-004-0225-9 ↗
20. Matsuda H (1996) Chemical modification of solid wood. In: Hon DNS (ed) Chemical modification of lignocellulosic materials. Marcel Decker Inc, New York, pp 159–183
21. Matuana LM, Balatinecz JJ, Park CB, Sodhi RNS (1999) X-ray photoelectron spectroscopy study of silane-treated newsprint-fibers. Wood Sci Technol 33:259–27010.1007/s002260050114 ↗
22. Miroy F, Eymard P, Pizzi A (1995) Wood hardening by methoxyl melamine. Holz Roh Werkstoff 53:26710.1007/s001070050089 ↗
23. Rapp AO (1999) Physikalische und biologische Vergütung von Vollholz durch Imprägnierung mit wasserverdünnbaren Harzen. PhD Thesis, University of Hamburg
24. Rapp AO, Bestgen H, Adam W, Peek RD (1999) Electron loss spectroscopy (EELS) for quantification of cell-wall penetration of a melamine resin. Holzforschung 53:111–11710.1515/HF.1999.018 ↗
25. Rijckaert V, van Acker J, Stevens M (1998) Decay resistance of high performance biocomposites based on chemically modified fibres. The International research Group on Wood Preservation, Document no.: IRG/WP 98–40120
26. Rowell R (1983) Chemical modification of wood. For Prod Abstr 6:363–382
27. Schneider MH, Brebner KI (1985) Wood.polymer combinations: the chemical modification of wood by alkoxysilane coupling agents. Wood Sci Technol 19:67–7310.1007/BF00354754 ↗
28. Sèbe G, Brook MA (2001) Hydrophobization of wood surfaces: covalent grafting of silicone polymers. Wood Sci Technol 35:269–28210.1007/s002260100091 ↗
29. Sèbe G, de Jéso B (2000) The dimensional stabilisation of Maritime pine sapwood (Pinus pinaster) by chemical reaction with organosilicon compounds. Holzforschung 54:474–48010.1515/HF.2000.080 ↗
30. Spurr AR (1969) A low viscosity embedding medium for electron microscopy. Ultrastruct Res 26:31–4310.1016/S0022-5320(69)90033-1 ↗
31. Stamm AJ, Baechler RH (1960) Decay resistance and dimensional stability of five modified woods. For Prod J 10:22–26
32. Troughton GE (1969) Accelerated aging of glue-wood bonds. Wood Sci 1:172–176
33. Troughton GE, Chow SZ (1968) Evidence for covalent bonding between melamine formaldehyde glue and wood. Part I—bond degradation. J Inst Wood Sci 21:29–33
34. Wise LE, Jahn EC (1952) Wood chemistry, vol 2. Reinhold Publishing Corp, New York
35. Zollfrank C (2001) Silylation of solid beech wood. Wood Sci Technol 35:183–18910.1007/s002260000071 ↗
36. Zollfrank C, Wegener G (2002) FTIR microscopy and ultrastructural investigation of silylated solid wood. Holzforschung 56:39–4210.1515/HF.2002.007 ↗