Simultaneous drying and densification of silver birch (Betula pendula L.) veneers: analysis of morphology, thickness swelling, and density profile
Source abstract
Abstract
In this study, birch (Betula pendula L.) veneers were simultaneously densified and dried using a contact drying method at pressures of 1.5 and 3 MPa at 130 °C and compared with veneer dried in a laboratory-scale convective type dryer. Compression rate, thickness swelling, and the density profiles of the veneers were investigated. Furthermore, the microstructure of densified veneers was studied by scanning electron microscopy (SEM). A maximum veneer compression rate of 9 % was achieved at a pressure of 3 MPa. Under these conditions, the veneers were, on average, densified from 504 to 574 kg m⁻³(approximately 14 %). After water soaking, full set-recovery—recovery to the initial thickness—occurred. However, the swelling rate was lower for the densified veneer. Density profiles measurements showed that densification occurs throughout the veneers. The SEM images showed that the surface of the densified veneers were smoother, whilst no cracks were detected due to densification. Densification seemed to occur in vessels. Typically, rays were bent when there was a vessel nearby.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Textile materials and evaluations · Cultural Heritage Materials Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Bekhta P, Marutzky R (2007) Reduction of glue consumption in the plywood production by using previously compressed veneer. Holz Roh Werkst 65:87–8810.1007/s00107-006-0142-8 ↗
2. Bekhta P, Hiziroglu S, Shepelyuk O (2009) Properties of plywood manufactured from compressed veneer as building material. Mater Design 30:947–95310.1016/j.matdes.2008.07.001 ↗
3. Bekhta P, Niemz P, Sedliacik J (2012) Effect of pre-pressing of veneer on the glueability and properties of veneer-based products. Eur J Wood Prod 70:99–10610.1007/s00107-010-0486-y ↗
4. Candan Z, Hiziroglu S, McDonald AG (2010) Surface quality of thermally compressed Douglas fir veneer. Mater Design 31:3574–357710.1016/j.matdes.2010.02.003 ↗
5. Cloutier, A, Fang CH, Mariotti N, Koubaa A, Blanchet P (2008) Densification of Wood Veneers Under the Effect of Heat, Steam and Pressure. Proceedings of the 51st International Convention of Society of Wood Science and Technology. Nov 10–12, 2008. Conceptión, Chile
6. Diouf PN, Stevanovic T, Cloutier A, Fang CH, Blanchet P, Koubaa A, Mariotti N (2011) Effects of thermo-hygro-mechanical densification on the surface characteristics of trembling aspen and hybrid poplar wood veneers. Appl Surf Sci 257:3558–356410.1016/j.apsusc.2010.11.074 ↗
7. Dwianto W, Morooka T, Norimoto M, Kitajima T (1999) Stress relaxation of Sugi (Cryptomeria japonica D. Don) wood in radial compression under high temperature steam. Holzforschung 53(5):541–54610.1515/HF.1999.089 ↗
8. Fang CH, Mariotti N, Cloutier A, Koubaa A, Blanchet P (2012) Densification of wood veneers by compression combined with heat and steam. Eur J Wood Prod 70:155–16310.1007/s00107-011-0524-4 ↗
9. Fortino S, Genoese A, Genoese A, Rautkari L (2013) FEM simulation of the hygro-thermal behaviour of wood under surface densification at high temperature. J Mat Sci 48:7603–761210.1007/s10853-013-7577-1 ↗
10. Hill C (2006) Wood Modification. Wiley, Chichester10.1002/0470021748 ↗
11. Hofmann T, Wetzig M, Rétfalvi T, Sieverts T, Bergemann H, Niemz P (2013) Heat-treatment with the vacuum-press dewatering method: chemical properties of the manufactures wood and the condensation water. Eur J Wood Prod 71:121–12710.1007/s00107-012-0657-0 ↗
12. Holmberg H, Lahti P, Paajanen O, Ahtela P (2009) An experimental study on drying times in a contact drying of veneer. Proceedings of 8th World Congress of Chemical Engineering. Montreal, Canada. Aug 23–27, 2009
13. Hukka A, Oksanen O (1999) Convective mass transfer coefficient at wooden surface in jet drying of veneer. Holzforschung 53(2):204–20810.1515/HF.1999.034 ↗
14. Kamke FA, Rathi VM (2011) Apparatus for viscoelastic thermal compression of wood. Eur J Wood Prod 69(3):483–48710.1007/s00107-010-0461-7 ↗
15. Kutnar A, Kamke FA (2012a) Compression of wood under saturated steam, superheated steam, and transient conditions at 150°C, 160°C, and 170°C. Wood Sci Technol 46:73–8810.1007/s00226-010-0380-0 ↗
16. Kutnar A, Kamke FA (2012b) Influence of temperature and steam environment on set recovery of compressive deformation of wood. Wood Sci Technol 46(5):953–96410.1007/s00226-011-0456-5 ↗
17. Kutnar A, Kamke FA, Sernek M (2009) Density profile and morphology of viscoelastic thermal compressed wood. Wood Sci Technol 43:57–6810.1007/s00226-008-0198-1 ↗
18. Lahti P, Paajanen O, Holmberg H, Kairi M (2010) Introducing a new method of veneer drying. Proceedings of the 11th International IUFRO Wood drying conference. Skelleftea, Sweden. Jan 18–22, 2010
19. Laine K, Rautkari L, Hughes M, Kutnar A (2013) Reducing the set-recovery of surface densified solid Scots pine wood by hydrothermal post-treatment. Eur J Wood Prod 71(1):17–2310.1007/s00107-012-0647-2 ↗
20. Lui H, Kamke FA, Kangquan G (2013) Integrated drying and thermo-hydro-mechanical modification of western hemlock veneer. Eur J Wood Prod 71(2):173–18110.1007/s00107-012-0660-5 ↗
21. Navi P, Sandberg D (2012) Thermo-hydro-mechanical processing of wood. Engineering sciences. EPFL Press, Lausanne10.1201/b10143 ↗
22. Paajanen O, Holmberg H, Lahti P, Kairi M (2012) Experiences with new drying method. Int Wood Prod J 3(1):26–3010.1179/2042645312Y.0000000011 ↗
23. Rautkari L, Properzi M, Pichelin F, Hughes M (2009) Surface modification of wood using friction. Wood Sci Technol 43(3–4):291–29910.1007/s00226-008-0227-0 ↗
24. Rautkari L, Properzi M, Pichelin F, Hughes M (2010) Properties and set-recovery of surface densified Norway spruce and European beech. Wood Sci Technol 44:679–69110.1007/s00226-009-0291-0 ↗
25. Rautkari L, Laine K, Laflin N, Hughes M (2011a) Surface modification of Scots pine: the effect of process parameters on the through thickness density profile. J Mater Sci 46:4780–478610.1007/s10853-011-5388-9 ↗
26. Rautkari L, Kamke FA, Hughes M (2011b) Density profile relation to hardness of viscoelastic thermal compressed (VTC) wood composite. Wood Sci Technol 45:693–70510.1007/s00226-010-0400-0 ↗
27. Rautkari L, Kamke FA, Hughes M (2011c) Potential error in density profile measurements for wood composites. Eur J Wood Prod 69:167–16910.1007/s00107-010-0419-9 ↗
28. Rautkari L, Laine K, Kutnar A, Medved S, Hughes M (2013) Hardness and density profile of surface densified and thermally modified Scots pine in relation to degree of densification. J Mater Sci 48:2370–237510.1007/s10853-012-7019-5 ↗
29. Salmén L (1982) Temperature and water induced softening behavior of wood fiber based materials. Dissertation, Royal Institute of technology, KTH, Stockholm