Optimization of processing variables during heat treatment of oak (Quercus mongolica) wood
Source abstract
Abstract
The properties of oak heat treated at temperatures of 160–220 °C, oxygen concentrations of 2–10 %, steam pressures of 0.1–0.4 MPa and treatment time of 2–4 h were investigated. Although modulus of elasticity (MOE), modulus of rupture (MOR) and equilibrium moisture content (EMC) of the heat-treated wood (HTW) were reduced, the value of [Formula: see text] was increased, and the dimensional stability [anti-swelling efficiency in radial (ASE-R), anti-humidity efficiency (AHE)] was improved considerably. Six regression equations (temperature, oxygen concentration, steam pressure and time as functions of MOE, MOR, ASE-R, AHE, EMC and [Formula: see text]) were developed for the estimation and a nonlinear programming model was derived with operation research theory to obtain the most desirable HTW properties under some production constraints.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Wood and Agarwood Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Akyildiz MH, Ates S (2008) Effect of heat treatment on equilibrium moisture content of some wood species in Turkey. Res J Agric Biol Sci 4(6):660–665
2. Bekhta P, Niemz P (2003) Effect of high temperature on the change in color, dimensional stability and mechanical properties of spruce wood. Holzforschung 57:539–54610.1515/HF.2003.080 ↗
3. Borrega M, Karenlampi PP (2008a) Mechanical behavior of heat treated spruce (Picea abies) wood at constant moisture content and ambient humidity. Holz Roh- Werkst 66:63–6910.1007/s00107-007-0207-3 ↗
4. Borrega M, Karenlampi PP (2008b) Effect of relative humidity on thermal degradation of Norway spruce (Picea abies) wood. J Wood Sci 54(4):323–32810.1007/s10086-008-0953-9 ↗
5. Bourgois J, Janin G, Guyonnet R (1991) La mesure de couleur: une me’ thode d’e’ tude et d’optimisation des transformations chimiques du bois thermolyse. Holzforschung 45:377–38210.1515/hfsg.1991.45.5.377 ↗
6. Brischke C, Welzbacher CR, Brandt K, Rapp AO (2007) Quality control of thermally modified timber: interrelationship between heat treatment intensities and CIE L*a*b* color data on homogenized wood samples. Holzforschung 61:19–2210.1515/HF.2007.004 ↗
7. Brito JO, Silva FG, Leão MM, Almeida G (2008) Chemical composition changes in eucalyptus and pinus woods submitted to heat treatment. Bioresour Technol 99:8545–854810.1016/j.biortech.2008.03.069 ↗
8. Burmester A (1973) Effect of heat-pressure-treatment of semi-dry wood on its dimensional stability. Holz Roh- Werkst 31:237–24310.1007/BF02607268 ↗
9. Cai JB, Cai LP (2012) Effects of thermal modification on mechanical and swelling properties and color change of lumber killed by mountain pine beetle. BioRes 7(3):3488–349910.15376/biores.7.3.3488-3499 ↗
10. Cao YJ, Lu JX, Huang RF, Zhao YK, Wu YZ (2011) Evaluation of decay resistance for steam-heat-treated wood. BioRes 6(4):4696–470410.15376/biores.6.4.4696-4704 ↗
11. Cao YJ, Jiang JH, Lu JX, Huang RF, Jiang JL, Wu YM (2012a) Color change of Chinese fir through steam-heat treatment. BioRes 7(3):2809–281910.15376/biores.7.3.2809-2819 ↗
12. Cao YJ, Lu JX, Huang RF, Jiang JL (2012b) Increased dimensional stability of Chinese fir through steam-heat treatment. Eur J Wood Prod 70(4):441–44410.1007/s00107-011-0570-y ↗
13. Cao YJ, Lu JX, Huang RF, Zhao X, Jiang JL (2012c) Effect of steam-heat treatment on mechanical properties of Chinese fir. BioRes 7(1):1123–113310.15376/biores.7.1.1123-1133 ↗
14. Chen JY (2008) Research on techniques and properties of Mongolian scotch pine after thermal treatment with pressure. Nanjing Forestry University, Nanjing
15. Chinese standards LY/T 1700 (2007) Wood based flooring for ground with heating system, Beijing, China
16. Chinese standards GB/T 1936.2-09 (2009) Method for determination of the modulus of elasticity in static bending of wood, Beijing, China
17. Chinese standards GB/T1936.1-09 (2009) Method of testing in bending strength of wood, Beijing, China
18. Ding T, Gu LB, Li T (2011) Influence of steam pressure on physical and mechanical properties of heat-treated Mongolian pine lumber. Eur J Wood Prod 69:121–12610.1007/s00107-009-0406-1 ↗
19. Giebeler E (1983) Dimensional stabilization of wood by moisture heat pressure treatment. Holz Roh Werkst 41:87–9410.1007/BF02608498 ↗
20. González-Peña MM, Hale MDC (2009) Color in thermally modified wood of beech, Norway spruce and Scots pine. Part2: property predictions from color changes. Holzforschung 63:394–40110.1515/HF.2009.077 ↗
21. Gündüz G, Korkut S, Korkut DS (2008) The effects of heat treatment on physical and technological properties and surface roughness of Camiyani Black Pine (Pinus nigra Arn. subsp. pallasiana var. pallasiana) wood. Bioresour Technol 99:2275–228010.1016/j.biortech.2007.05.015 ↗
22. Johansson D, Morén T (2006) The potential of color measurement for strength prediction of thermally treated wood. Holz Roh- Werkst 64:104–11010.1007/s00107-005-0082-8 ↗
23. Korkut DS, Korkut S, Bekar I, Budakçı M, Dilik T, Çakıcıer N (2008a) The effects of heat treatment on the physical properties and surface roughness of Turkish Hazel (Corylus colurna L.) Wood. Int J Mol Sci 9:1772–178310.3390/ijms9091772 ↗
24. Korkut S, Akgül M, Dündar T (2008b) The effects of heat treatment on some technological properties of Scots pine (Pinus sylvestirs L.) wood. Bioresour Technol 99:1861–186810.1016/j.biortech.2007.03.038 ↗
25. Korkut S, Kök MS, Korkut DS, Gürleyen T (2008c) The effects of heat treatment on technological properties in Red-bud maple (Acer trautvetteri Medw.) wood. Bioresour Technol 99:1538–154310.1016/j.biortech.2007.04.021 ↗
26. Kubojima Y, Okano T, Ohta M (2000) Bending strength and toughness of heat-treated wood. J Wood Sci 46:8–1510.1007/BF00779547 ↗
27. Millett MA, Gerhards GC (1972) Accelerated aging: residual weight and flexural properties of wood heated in atmospheric at 115 °C to 170 °C. Wood Sci 4(4):193–201
28. Shi JL, Kocaefe D, Zhang J (2007) Mechanical behavior of Québec wood species heat-treated using Thermo Wood process. Holz Roh- Werkst 65:255–25910.1007/s00107-007-0173-9 ↗
29. Wang JY, Cooper PA (2005) Effect of oil type, temperature and time on moisture properties of hot oil-treated wood. Holz Roh- Werkst 63:417–42210.1007/s00107-005-0033-4 ↗
30. Zivkovic V, Prsa I, Turkulin H, Sinkovic T, Jirous-Rajkovic V (2008) Dimensional stability of heat treated wood floorings. Drvna Industrija 59(2):69–73