journal article·2009-02

Effects of preboiling on the acidity and strength properties of heat-treated wood

L. Awoyemi, M. C. Jarvis, A. Hapca

Wood Science and Technology· Volume 43· Issue 1-2
Publisher page

Abstract

Heat treatment is an alternative to the chemical treatment in wood preservation, which has been used to some extent in improving timber quality. However, reduction in strength properties has been one of the major limitations in the use of this technique and therefore investigations on the use of various pre-treatment methods are highly essential. Wood samples from Scots pine were immersed in already boiling water (100°C) for 20 min followed by 2 h of heat treatment at 160 and 200°C. The acidity and strength properties were determined by measurement of pH and static bending test, respectively. There were no significant changes in pH due to preboiling in both heat-treated and untreated wood. Similarly, preboiling did not result in any appreciable differences in strength both before heat treatment and during heat treatment at 160°C. However, for 200°C heat treatment preboiling reduced significantly the degree of strength loss as indicated by 19.4% reduction in modulus of rupture in preboiled wood compared to 26.6% reduction in unpreboiled wood. From the results of this study it is evident that preboiling has a buffering effect on wood during heat treatment and the higher the intensity of heat treatment the higher the significance of the buffering effect of pre-boiling.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Bamboo properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Awoyemi L, Westermark U (2005) Effects of borate impregnation on the response of wood strength to heat treatment. Wood Sci Technol 39:484–49110.1007/s00226-005-0001-5 ↗
2. Ayadi N, Lejeune F, Charrier F, Charrier B, Merlin A (2003) Colour stability of heat-treated wood during artificial weathering. Holz Roh Werkst 61:221–22610.1007/s00107-003-0389-2 ↗
3. Boonstra MJ, Tjeerdsma B (2006) Chemical analysis of heat treated softwoods. Holz Roh Werkst 64:204–21110.1007/s00107-005-0078-4 ↗
4. Boonstra MJ, van Acker J, Kegel E, Stevens M (2006) Optimisation of a two stage heat treatment process: durability aspects. Wood Sci Technol 40:31–57
5. Chafe SC (1993) The effect of boiling on shrinkage, collapse and other wood–water properties in core segments of Eucalyptus regnans F. Muell. Wood Sci Technol 27:205–21710.1007/BF00192817 ↗
6. Geissen A, Du QP (1995) Influence of heat treatment on the accuracy of wood moisture content determination by electrical resistance-type meters. Holz Roh Werkst 53:303–30710.1007/s001070050095 ↗
7. Hakkou M, Petrissans M, Zoulalian A, Gerardin P (2005) Investigation of wood wettability changes during heat treatment on the basis of chemical analysis. Polym Degrad Stab 89:1–510.1016/j.polymdegradstab.2004.10.017 ↗
8. Hanger J, Huber H, Lackner R, Wimmer R, Fellner J (2002) Improving the natural durability of heat-treated spruce, pine and beech. Holzforsch Holzverwert 54:92–93
9. Hodgin DA, Lee AWC (2002) Comparison of strength properties and failure characteristics between fire-retardant-treated and untreated roofing lumber after long-term exposure: A South Carolina case study. For Prod J 52:91–94
10. Kamdem DP, Pizzi A, Triboulot MC (2000) Heat-treated timber: potentially toxic byproducts presence and extent of wood cell wall degradation. Holz Roh Werkst 58:253–25710.1007/s001070050420 ↗
11. Kamdem DP, Pizzi A, Jermannaud A (2002) Durability of heat-treated wood. Holz Roh Werkst 60:1–610.1007/s00107-001-0261-1 ↗
12. Kubojima Y, Okano T, Ohta M (2000) Bending strength and toughness of heattreated wood. J Wood Sci 46:8–1510.1007/BF00779547 ↗
13. Manninen AM, Pasanen P, Holopainen JK (2002) Comparing the VOC emissions between air-dried and heat-treated Scots pine wood. Atmos Environ 36:1763–176810.1016/S1352-2310(02)00152-8 ↗
14. Metsa-Kortelainen S, Antikainen T, Viitanieni P (2006) The water absorption of sapwood and heartwood of Scots pine and Norway spruce heat-treated at 170°C, 190°C, 210°C and 230°C. Holz Roh Werkst 64:192–19710.1007/s00107-005-0063-y ↗
15. Mitsui K (2006) Changes in colour of spruce by repetitive treatment of light irradiation and heat treatment. Holz Roh- Werkst 64:243–24410.1007/s00107-005-0045-0 ↗
16. Nuopponen M, Wikberg H, Vuorinen T, Maunu SL, Jamsa S, Viitaniemi P (2004) Heat-treated softwood exposed to weathering. J Appl Polym Sci 91:2128–213410.1002/app.13351 ↗
17. Obataya E, Tomita B (2002) Hygroscopicity of heat-treated wood. II. Reversible and irreversible reductions in the hygroscopicity of wood due to heating. Mokuzai Gakkaishi 48:288–295
18. Obataya E, Tanaka F, Norimoto M, Tomita B (2000) Hygroscopicity of heat treated wood. I. Effects of after-treatments on the hygroscopicity of heat-treated wood. Mokuzai Gakkaishi 46:77–87
19. Rapp AO, Sailer M (2001) Oil-heat-treatment of wood-process and properties. Drvna Industrija 52:63–70
20. Sailer M, Rapp AO, Leithoff H, Peek RD (2000) Upgrading of wood by application of an oil-heat treatment. Holz Roh Werkst 58:15–2210.1007/s001070050379 ↗
21. Tejada A, Okuyama T, Yamamoto H, Yoshida M (1997) Reduction of growth stresses in log by direct heat treatment: assessment of a commercial scale operation. For Prod J 47:86–93
22. Udaka E, Furuno T (2003) Change in crystalline structure of compressed wood by treatment with a closed heating system. Mokuzai Gakkaishi 49:1–6