The tensile stress relaxation of Chinese fir wood treated with copper-ethanolamine (Cu-EA) was compared with that of untreated control to investigate the influence of Cu-EA treatment on the dimensional stability of wood in long-term application, and also for a better understanding of copper-wood-water interactions in copper containing water-borne preservative systems. The results showed that temperature and moisture conditions play important roles in the stress relaxation behavior of wood with or without Cu-EA treatment. At 25°C, Cu-EA treatment has little influence on stress relaxation; while at 35°C, Cu-EA treatment can significantly reduce the stress relaxation of wood, suggesting that Cu-EA treatment can increase dimensional stability of wood at high atmospheric temperature in long-term application. The complicated effect of copper retention on stress relaxation further confirms that copper competes for hydroxyl groups as adsorption sites with water molecules, as put forward in the previous report.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Cultural Heritage Materials Analysis · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. American Wood Preservers’s Association Standard (2004) Standard for waterborne preservatives. P5-04. Book of standards. AWPA, Selma, Alabama, pp 203–208
2. American Wood Preserver’s Association Standard (2004) Standard method for analysis of treated wood and treating solutions by atomic absorption spectroscopy. P11-93. Book of standards. AWPA, Selma, Alabama, pp 287–290
3. Cao J, Kamdem DP (2004) Moisture adsorption characteristics of copper–ethanolamine (Cu–EA) treated Southern yellow pine (Pinus spp.). Holzforschung 58(1):32–3810.1515/HF.2004.005 ↗
4. Craciun R, Kamdem D P (1997) XPS and FTIR applied to the study of waterborne copper naphthenate wood preservatives. Holzforschung 51(3):207–21310.1515/hfsg.1997.51.3.207 ↗
5. Dai C (2001) Viscoelasticity of wood composite mats during consolidation. Wood Fiber Sci 33(3):353–363
6. Jiang X, Ruddick JNR (1999) A spectroscopic investigation of copper ethylenediamine fixation in wood. International Research Group Wood Preservation Document no. IRG/WP/99-20160, pp 3–13
7. Lebow ST, Morrell JJ (1995) Interactions of ammoniacal copper zinc arsenate (ACZA) with Douglas-fir. Wood Fiber Sci 27(2):105–118
8. Wolcott MP (1990) Modelling viscoelastic cellular materials for the pressing of wood composites. PhD Dissertation, Department of Wood Science and Forest Products, Virginia Polytechnic Institute and State University
9. Youngs RL (1957) The perpendicular-to-grain mechanical properties of red oak as related to temperature, moisture content, and time. USDA Forest Prod. Lab. Report no. 2079, Madison, WI
10. Zhang J, Kamdem DP (2000) FTIR characterization of copper ethanolamine–wood interaction for wood preservation. Holzforschung 54(2):119–12210.1515/HF.2000.020 ↗