journal article·2016-10

Biocompatibility and degradation of LAE442-based magnesium alloys after implantation of up to 3.5 years in a rabbit model

N. Angrisani, J. Reifenrath, F. Zimmermann, R. Eifler, A. Meyer-Lindenberg, K. Vano-Herrera, C. Vogt

Acta Biomaterialia· Volume 44
Publisher page

Abstract

Unlabelled Magnesium as basic implant material has long been the center of orthopedic research. Latest progress is achieved with a European certification and clinical use of a magnesium based compression screw. However, long term studies with implantation duration that exceed one year considerably do not exist. The present examinations analyzed the degradation progress from nine months to 3.5year after implantation of cylindrical pins into the medullary cavity of New Zealand White rabbits. Evaluation included clinical assessment, in vivo μ-computed tomography, analysis of the implants by three-point-bending and examination of the adjacent tissue by means of histology and of inner organs by mass- and optical emission spectrometry using inductively coupled plasma. Clinical acceptance was without objections in all animals. Immoderate reaction of the surrounding bone could be found in neither of the applied techniques. While in vivo μ-computed tomography showed a very slow degradation rate up to 72weeks, three-point-bending revealed a percentage loss of F(max) of 41.1% for implants after 9months implantation and 88.47% for the implant after 3.5years implantation. Although the total amounts of RE detected in the inner organs were very low, the organs of rabbits with LAE442 cylinders showed 10-20-fold increased concentrations of the alloying elements lanthanum, cerium, neodymium and praseodymium compared to animals without any implanted material. Statement of significance This is the first animal study investigating the degradation process of a magnesium alloy in vivo for up to 3.5years. Currently available data from different other in vivo studies cover only implantation durations up to one year. Therefore, the analysis of these long-time effects in the present study is highly significant and of great interest. Comprehensive outcome achieved by different techniques was assessed. The degradation process was slow and homogenous. Maximum applied force (F(max)) reduced by 41.1% for implants after 9months and by 88.47% for the implant after 3.5years implantation. Total amounts of RE detected in the inner organs were very low; the organs of rabbits with LAE442 cylinders showed 10-20-fold increased concentrations.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Orthopaedic implants and arthroplasty · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Reifenrath · Materialwiss. Werkstofftech. · 2010 · 41 · 105410.1002/mawe.201000709 ↗
2. Magnesium alloys for temporary implants in osteosynthesis: in vivo studies of their degradation and interaction with bone10.1016/j.actbio.2011.11.008 ↗
3. Rare Earth metals as alloying components in magnesium implants for orthopaedic applications
4. Biodegradable nasal stents (MgF2-coated Mg-2wt%Nd alloy)-A long-term in vivo study
5. A novel biodegradable frontal sinus stent (MgNd2): a long-term animal study10.1007/s00405-015-3774-7 ↗
6. Recent advances in biodegradable metals for medical sutures: a critical review10.1002/adhm.201500189 ↗
7. Research on the biocompatibility of the new magnesium alloy LANd442 – an in vivo study in the rabbit tibia over 26 weeks10.1002/adem.201180066 ↗
8. Long term in vivo degradation behaviour and biocompatibility of the magnesium alloy ZEK100 for use as biodegradable bone implant10.1016/j.actbio.2012.08.028 ↗
9. In vivo corrosion and corrosion protection of magnesium alloy LAE44210.1016/j.actbio.2009.10.012 ↗
10. Evaluation of the skin sensitizing potential of biodegradable magnesium alloys
11. Degradation behaviour and mechanical properties of magnesium implants in rabbit tibiae10.1007/s10853-009-3936-3 ↗
12. Implant location strongly influences degradation and applicability of magnesium alloys for orthopaedic applications
13. In vivo evaluation of a magnesium-based degradable intramedullary nailing system in a sheep model
14. Neuropathology of aluminum toxicity in rats (glutamate and GABA impairment)10.1016/S1043-6618(02)00336-5 ↗
15. Lithium revisited10.1177/070674370104600402 ↗
16. Grades and Alloys
17. Recent advances on the development of magnesium alloys for biodegradable implants10.1016/j.actbio.2014.07.005 ↗
18. Understanding magnesium corrosion – a framework for improved alloy performance10.1002/adem.200310405 ↗
19. Evaluation of short-term effects of rare earth and other elements used in magnesium alloys on primary cells and cell lines10.1016/j.actbio.2009.09.024 ↗
20. The suppression effect of light rare earth elements on proliferation of two cancer cell lines
21. Effects of rare earth compounds on growth and apoptosis of leukemic cell lines10.1290/1071-2690(2002)038<0373:EORECO>2.0.CO;2 ↗
22. Biocompatibility of rapid-solidified magnesium alloy RS66 as a temporary biodegradable metal10.1016/j.actbio.2013.02.015 ↗
23. Magnesium-based intramedullary nailing system in a sheep model: Biomechanic evaluation and first in vivo results
24. Analysis of metallic traces from the biodegradation of endomedullary AZ31 alloy temporary implants in rat organs after long implantation times10.1088/1748-6041/10/4/045015 ↗
25. In vivo assessment of the host reactions to the biodegradation of the two novel magnesium alloys ZEK100 and AX30 in an animal model10.1186/1475-925X-11-14 ↗
26. Chemical analysis – Methods of standard adition, DIN 32633:2013–05, Beuth Verlag GmbH, Berlin.
27. A method for the study of undecalcified bones and teeth with attached soft tissues: the Säge-Schliff (sawing and grinding) technique10.1111/j.1600-0714.1982.tb00172.x ↗
28. C. Hampp, Degradation und Biokompatibilität der neuen Magnesiumlegierung LANd442 im Vergleich zu LAE442 und der nicht degradablen Titanlegierung Ti6Al4V-Eli nach intramedullärer Implantation in die Kaninchentibia, Dissertation, Klinik für Kleintiere, 2012 ().
29. Chemical analysis – Decision limit, detection limit and determination limit under repeatability conditions – Terms, methods, evaluation, DIN 32645:2008-11, Beuth Verlag GmbH, Berlin.
30. German standard methods for the examination of water, waste water and sludge – General information (group A) – Part 51: Calibration of analytical methods – Linear calibrations (A51), DIN 38402–51:2015–09, Beuth Verlag GmbH, Berlin.
31. Evaluation of the biocompatibility of two magnesium alloys as degradable implant materials in comparison to titanium as non resorbable material in the rabbit10.1016/j.msec.2012.08.046 ↗
32. Influence of heat treatment on the degradation behaviour of degradable magnesium based implants10.1515/bmt-2013-4057 ↗
33. Applicability of Degradable magnesium LAE442 alloy plate-screw-systems in a rabbit model10.1515/bmt-2013-4059 ↗
34. In vivo study of magnesium plate and screw degradation and bone fracture healing10.1016/j.actbio.2015.02.010 ↗
35. Corrosion protection and repassivation after the deformation of magnesium alloys coated with a protective magnesium flouride layer
36. Influence of the grain size on the in vivo degradation behaviour of the magnesium alloy LAE 44210.1177/0954411912471495 ↗
37. In vivo degradation behaviour of the magnesium alloy LANd442 in rabbit tibiae10.3390/ma4122197 ↗
38. In vivo corrosion of two novel magnesium alloys ZEK100 and AX30 and their mechanical suitability as biodegradable implants10.3390/ma4061144 ↗
39. Gasbildung und deren Analysemöglichkeiten im Verlauf der in vivo Degradation von Magnesiumlegierungen
40. Influence of different storage durations on the properties of degradable magnesium based implants
41. The effect of metallic magnesium degradation products on osteoclast-induced osteolysis and attenuation of NF-kappaB and NFATc1 signaling10.1016/j.biomaterials.2014.04.044 ↗
42. Biodegradable magnesium scaffolds: Part II: Peri-implant bone remodeling10.1002/jbm.a.31293 ↗
43. Degrading magnesium screws ZEK100: biomechanical testing, degradation analysis and soft-tissue biocompatibility in a rabbit model10.1088/1748-6041/8/4/045012 ↗
44. In vivo degradation of magnesium plate/screw osteosynthesis implant systems: soft and hard tissue response in a calvarial model in miniature pigs10.1016/j.jcms.2015.12.009 ↗
45. Evaluation of the soft tissue biocompatibility of MgCa0.8 and surgical steel 316L in vivo: a comparative study in rabbits10.1186/1475-925X-9-63 ↗
46. Biodegradable magnesium scaffolds: Part 1: appropriate inflammatory response10.1002/jbm.a.31170 ↗
47. An in vivo study on the metabolism and osteogenic activity of bioabsorbable Mg-1Sr alloy10.1016/j.actbio.2015.11.014 ↗
48. Influence of different surface machining treatments of resorbable magnesium alloy implants on degradation – EDX-analysis and histology results10.1002/mawe.200800378 ↗
49. Comparison of morphological changes in efferent lymph nodes after implantation of resorbable and non-resorbable implants in rabbits10.1186/1475-925X-10-32 ↗
50. Examination of a biodegradable magnesium screw for the reconstruction of the anterior cruciate ligament: a pilot in vivo study in rabbits10.1016/j.msec.2015.11.037 ↗
51. Determination of concentration gradients in bone tissue generated by a biologically degradable magnesium implant10.1039/B813734J ↗
52. Quantitative analysis of elements migration in human teeth with and without filling using LA-ICP-MS10.1016/j.microc.2013.02.006 ↗
53. Biomonitoring of hair samples by laser ablation inductively couples plasma mass spectrometry (LA-ICP-MS)10.1016/j.ijms.2006.09.018 ↗
54. Trace elements in scalp hair of children chronically exposed to volcanic activity (Mt. Etna, Italy)10.1016/j.scitotenv.2013.09.058 ↗
55. Quantitative imaging of metals in tissues10.1007/s10534-008-9200-5 ↗
56. Ecological and biological determinants of trace elements accumulation in liver and kidney of Pontoporia blainvillei10.1016/j.scitotenv.2007.06.045 ↗
57. Assessment of trace elements in human brain using inductively coupled plasma mass spectrometry10.1016/j.jtemb.2013.09.006 ↗
58. Determination of differential heavy metal and trace element accumulation in liver, gills, intestine and muscle of sterlet (Acipenser ruthenus) from the Danube River in Serbia by ICP-OES10.1016/j.microc.2010.11.008 ↗
59. Microwave-assisted digestion of organic samples: how simple can it become?10.1016/j.talanta.2012.06.079 ↗
60. The analytical calibration in (bio)imaging/mapping of the metallic elements in biological samples–definitions, nomenclature and strategies: state of the art10.1016/j.talanta.2014.07.089 ↗
61. Sources of error in external calibration ICP-MS analysis of geological samples and an improved non-linear drift correction procedure10.1016/0584-8547(93)80054-X ↗
62. Age-related effects of major and trace element concentrations in rat liver and their mutual relationships10.1016/j.jtemb.2013.04.006 ↗
63. Investigation of the degradation of biodegradable Mg implant alloys in vitro and in vivo by analytical methods
64. Safety of aluminium from dietary intake. Scientific Opinion of the Panel on Food Additives, Flavourings, Processing Aids and Food Contact Materials (AFC)
65. Anticancer activity of the lanthanum compound [tris(1,10-phenanthroline)lanthanum(III)]trithiocyanate (KP772; FFC24)10.1016/j.bcp.2005.11.009 ↗
66. Cellular response to rare earth mixtures (La and Gd) as components of degradable Mg alloys for medical applications10.1016/j.colsurfb.2014.02.030 ↗
67. Theoretical risk assessment of magnesium alloys as degradable biomedical implants10.1016/j.actbio.2009.11.036 ↗
68. In vitro and in vivo comparison of binary Mg alloys and pure Mg10.1016/j.msec.2015.12.064 ↗
69. Magnesium alloys as implant materials–principles of property design for Mg-RE alloys10.1016/j.actbio.2009.09.010 ↗
70. Preparation and characterization of as-extruded Mg-Sn alloys for orthopedic applications10.1016/j.matdes.2014.12.041 ↗
71. In vitro and in vivo corrosion, cytocompatibility and mechanical properties of biodegradable Mg–Y–Ca–Zr alloys as implant materials10.1016/j.actbio.2013.06.025 ↗
72. The role of surface oxidation on the degradation behavior of biodegradable Mg-RE (Gd, Y, Sc) alloys for resorbable implants10.1016/j.msec.2014.03.055 ↗
73. Magnesium transport in the gastrointestinal tract10.2741/Schweigel ↗