journal article·2015-09

Upconversion luminescent materials of Y–Gd oxysulfide binary system codoped with Yb and Er

Pengde Han, Xiaoping Jiang, Sen Cheng, Wei Jin, Fangli Yu, Rongfeng Guan, Qitu Zhang

Publisher page

Abstract

(Y1−xGdx)2O2S:0.08Yb/0.02Er powders doped with different concentrations of Gd3+ (x = 0, 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9 and 1.0) were prepared by flux method. The effects of Gd3+ doping amount on the phase composition, the crystal structure, the luminescent intensity, the emission color, phonon energy and forbidden bandwidth of Y2O2S:Yb/Er were investigated by XRD, UPL, CIE, RAMAN and R%, respectively. (Y1−xGdx)2O2S:Yb/Er powders doped with different concentrations of Gd3+ were all pure oxysulfide phase. Upconversion luminescent intensity of (Y0.9Gd0.1)2O2S:Yb/Er was the maximum. Green and red emission intensity of Y2O2S:Yb/Er was increased by three times with doping 10 mol% Gd3+ ions. The emission color was basically yellow. Gd3+ ions optimized the crystal structure of Y2O2S, changed the crystal field of Er3+ and Yb3+ ions, and improved the upconversion luminescent properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Luminescence Properties of Advanced Materials · Solid State Laser Technologies · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. V. Pankratov, A.I. Popov, L. Shirmane et al., J. Appl. Phys. 110, 53522–53528 (2011)10.1063/1.3634112 ↗
2. V. Pankratov, A.I. Popov, A. Kotlov et al., Opt. Mater. 33, 1102–1105 (2011)10.1016/j.optmat.2010.12.019 ↗
3. L. Yang, J.X. Wang, X. Dong, J. Mater. Sci. 48, 644–650 (2013)10.1007/s10853-012-6768-5 ↗
4. J. Thirumalai, R. Chandramohan, S. Valanarasu et al., Micro Nano Lett. 6, 614–618 (2011)10.1049/mnl.2011.0252 ↗
5. C. Waite, R. Mann, A.L. Diaz, J. Solid State Chem. 198, 357–363 (2013)10.1016/j.jssc.2012.10.023 ↗
6. X.L. Liu, P.X. Zhu, Y.F. Gao et al., J. Mater. Chem. 1, 477–483 (2013)
7. Y.F. Ma, J.W. Zhang, H. Li et al., Laser Phys. Lett. 9, 561–563 (2012)10.7452/lapl.201210041 ↗
8. H. Yang, X.P. Qin, J. Zhang et al., J. Alloys Compd. 509, 5274–5279 (2011)10.1016/j.jallcom.2010.11.030 ↗
9. M. Sugiyama, Y. Fujimoto, T. Yanagida et al., J. Cryst. Growth 362, 178–181 (2013)10.1016/j.jcrysgro.2011.10.030 ↗
10. N. Wagner, B. Herden, T. Dierkes et al., J. Eur. Ceram. Soc. 32, 3085–3089 (2012)10.1016/j.jeurceramsoc.2012.03.015 ↗
11. D.L. Gao, X.Y. Zhang, H.R. Zheng et al., J. Alloys Compd. 554, 395–399 (2013)10.1016/j.jallcom.2012.12.010 ↗
12. J.B. Zhao, Z.D. Lu, Y.D. Yin et al., Nanoscale 5, 944–952 (2013)10.1039/C2NR32482B ↗
13. J.H. Lee, T.S. Lee, J.Y. Ryu et al., J. Nucl. Med. 54, 96–103 (2013)10.2967/jnumed.112.108043 ↗
14. D. Wang, L. Ren, X. Zhou et al., Nanotechnology 23, 225705 (2012)10.1088/0957-4484/23/22/225705 ↗
15. Z.Q. Li, X.D. Li, Q.Q. Liu et al., Nanotechnology 23, 025402 (2012)10.1088/0957-4484/23/2/025402 ↗
16. F. Wang, Y. Han, C.S. Lim et al., Nature 463, 1061–1065 (2010)10.1038/nature08777 ↗
17. S.J. Duclosa, C.D. Greskovicha, R.J. Lyonsab et al., Nucl. Instrum. Methods A 505, 68–71 (2003)10.1016/S0168-9002(03)01022-2 ↗
18. M. Tamatani, N. Tsuda, K. Nomoto et al., J. Lumin. 12–13, 935–940 (1976)10.1016/0022-2313(76)90201-5 ↗
19. M. Leskelä, L. Niínistö, H. Dexpert et al., Mater. Res. Bull. 14, 455–461 (1979)10.1016/0025-5408(79)90185-5 ↗
20. G.A. Kumar, M. Pokhrel, A. Martinez et al., J. Alloys Compd. 513, 559–565 (2012)10.1016/j.jallcom.2011.11.006 ↗
21. G.A. Kumar, M. Pokhrel, D.K. Sardar, Mater. Lett. 68, 395–398 (2012)10.1016/j.matlet.2011.10.087 ↗
22. M. Mikami, A. Oshiyama, Phys. Rev. B 57, 8939–8944 (1998)10.1103/PhysRevB.57.8939 ↗
23. A.M. Pires, O.A. Serra, M.R. Davolos, J. Alloys Compd. 374, 181–184 (2004)10.1016/j.jallcom.2003.11.088 ↗
24. M. Mikami, A. Oshiyama, J. Lumin. 87–89, 1206–1209 (2000)10.1016/S0022-2313(99)00512-8 ↗