journal article·2019-03

Performance assessment of Pr1−xSrxCo0.8Cu0.2O3−δ perovskite oxides as cathode material for solid oxide fuel cells with Ce0.8Sm0.2O1.9 electrolyte

Sanlong Wang, Xiangwei Meng, Jinghai Yang, Lili Yang, Lizhong Wang, Mingxing Song, Yiming Zhou, Shiquan Lü

Publisher page

Abstract

In this paper, Pr1−xSrxCo0.8Cu0.2O3−δ (x = 0.2, 0.3, 0.4, 0.5, 0.6) cathode material is investigated for intermediate-temperature solid oxide fuel cells (IT-SOFCs). Pr1−xSrxCo0.8Cu0.2O3−δ oxides are prepared by the EDTA-citrate complexing method. XRD results show that there is a structural change from orthorhombic (x = 0.2 and 0.3) to cubic (x = 0.4, 0.5 and 0.6) in Pr1−xSrxCo0.8Cu0.2O3−δ system. The electrical conductivities of all the samples are all higher than 523 S cm−1 between 500 and 800 °C. The semiconductor-to-metal conductivity transition takes place at around x = 0.4. In order to further reduce thermal expansion coefficients (TECs) and improve electrochemical performance of the Pr1−xSrxCo0.8Cu0.2O3−δ cathode, we fabricate Pr0.5Sr0.5Co0.8Cu0.2O3−δ–x wt% Ce0.8Sm0.2O1.9 (PSCC–xSDC, x = 20–60) composite cathodes. In PSCC–xSDC electrode, the TEC and polarization resistance (Rp) both decrease with the addition of SDC. The PSCC–50SDC composite cathode has the lowest Rp. The lowest Rp 0.029 Ω cm2 is obtained at 800 °C for PSCC–50SDC electrode. Subsequently, we fabricate SDC (300 µm thick) electrolyte-supported fuel cell with PSCC–50SDC cathodes. The maximum power densities is 428 mW cm−2 at 800 °C. The present results demonstrate that PSCC–50SDC composite is a promising candidate cathode for IT-SOFCs.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Magnetic and transport properties of perovskites and related materials · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. N.Q. Minh, Solid oxide fuel cell technology-features and applications. Solid State Ionics. 174, 271–277 (2004)10.1016/j.ssi.2004.07.042 ↗
2. D.J.L. Brett, A. Atkinson, N.P. Brandon, S.J. Skinner, Intermediate temperature solid oxide fuel cells. Chem. Soc. Rev. 37, 1568–1578 (2008)10.1039/b612060c ↗
3. N.P. Brandon, S. Skinner, B.C.H. Steele, Recent advances in materials for fuel cells. Annu. Rev. Mater. Res. 33, 183–213 (2003)10.1146/annurev.matsci.33.022802.094122 ↗
4. R. Li, G. Chen, K. Wu, Y.H. Cheng, La0.8Sr1.2CoO4 + δ-CGO composite as cathode on La0.9Sr0.1Ga0.8Mg0.2O3–δ electrolyte for intermediate temperature solid oxide fuel cells. J. Power Sourc. 232, 332–337 (2013)10.1016/j.jpowsour.2012.11.110 ↗
5. R. Li, D. Wang, L. Ge, S. He, H. Chen, L. Guo, Effect of Bi2O3 on the electrochemical performance of LaBaCo2O5 + δ cathode for intermediate-temperature solid oxide fuel cells. Ceram. Int. 40, 2599–2603 (2014)10.1016/j.ceramint.2013.10.074 ↗
6. E. Koep, D.S. Mebane, R. Das, C. Compson, M. Liu, Electrochem. Solid-State Lett. 8, A592–A595 (2005)10.1149/1.2050607 ↗
7. M.J. Jørgensen, S. Primdahl, C. Bagger, M. Mogensen, Effect of sintering temperature on microstructure and performance of LSM–YSZ composite cathodes. Solid State Ionics 139, 1–11 (2001)10.1016/S0167-2738(00)00818-3 ↗
8. S.B. Adler, J.A. Lane, B.C.H. Steele, Electrode kinetics of porous mixed-conducting oxygen electrodes. J. Electrochem. Soc. 143, 3554–3564 (1996)10.1149/1.1837252 ↗
9. H. Fukunaga, M. Koyama, N. Takahashi, C. Wen, K. Yamada Reaction model of dense Sm0.5Sr0.5CoO3 as SOFC cathode. Solid State Ionics 132, 279–285 (2000)10.1016/S0167-2738(00)00642-1 ↗
10. Z.P. Shao, S.M. Haile, A high-performance cathode for the next generation of solid oxide fuel cells. Nature 431, 170–173 (2004)10.1038/nature02863 ↗
11. K. Yasumoto, Y. Inagaki, M. Shiono, M. Dokiya, An (La,Sr)(Co,Cu)O3–δ cathode for reduced temperature SOFCs. Solid State Ionics 148, 545–549 (2002)10.1016/S0167-2738(02)00115-7 ↗
12. T. Ishihara, T. Kudo, H. Matsuda, Y. Takita, Doped PrMnO3 perovskite oxide as a new cathode of solid oxide fuel cells for low temperature operation. J. Electrochem. Soc. 142, 1519–1524 (1995)10.1149/1.2048606 ↗
13. L. Cong, T. He, Y. Ji, P. Guan, Y. Huang, W. Su, Synthesis and characterization of IT-electrolyte with perovskite structure La0.8Sr0.2Ga0.85Mg0.15O3–δ by glycine–nitrate combustion method. J. Alloys Compd. 348, 325–331 (2003)10.1016/S0925-8388(02)00859-9 ↗
14. H.C. Yu, K.Z. Fung, Electrode properties of La1–xSrxCuO2.5–δ as new cathode materials for intermediate-temperature SOFCs. J. Power Sources 133, 162–168 (2004)10.1016/j.jpowsour.2004.02.002 ↗
15. K. Vidal, L.M. Rodríguez-Martínez, L. Ortega-San-Martín, E. Díez-Linaza, M.L. Nó, T. Rojo, A. Laresgoiti, M.I. Arriortua, Isolating the effect of doping in the structure and conductivity of (Ln1–xMx)FeO3–δ perovskites. Solid State Ionics 178, 1310–1316 (2007)10.1016/j.ssi.2007.06.015 ↗
16. L.W. Tai, M.M. Nasrallah, H.U. Anderson, D.M. Sparlin, S.R. Sehlin, Structure and electrical properties of La1–xSrxCo1–yFeyO3. Part 2. The system La1–xSrxCo0.2Fe0.8–O3. Solid State Ionics 76, 273–283 (1995)10.1016/0167-2738(94)00245-N ↗
17. F.J. Jin, Y. Shen, R. Wang, T.M. He, Double-perovskite PrBaCo2/3Fe2/3Cu2/3O5 + δ as cathode material for intermediate temperature solid-oxide fuel cells. J. Power Sourc. 234, 244–251 (2013)10.1016/j.jpowsour.2013.01.172 ↗
18. G.Z. Xing, J.B. Yi, J.G. Tao, T. Liu, L.M. Wong, Z. Zhang, G.P. Li, S.J. Wang, J. Ding, T.C. Sum, C.H.A. Huan, T. Wu, Comparative study of room-temperature ferromagnetism in Cu-Doped ZnO nanowires enhanced by structural inhomogeneity. Adv. Mater. 20, 3521–3527 (2008)10.1002/adma.200703149 ↗
19. G.Z. Xing, J.B. Yi, D.D. Wang, L. Liao, T. Yu, Z.X. Shen, C.H.A. Huan, T.C. Sum, J. Ding, T. Wu, Strong correlation between ferromagnetism and oxygen deficiency in Cr-doped In2O3–δ nanostructures. Physical Review B 79, 174406 (2009)10.1103/PhysRevB.79.174406 ↗
20. H.W. Brinks, H. Fjellvåg, A. Kjekshus, B.C. Hauback, Structure and magnetism of Pr1–xSrxFeO3–δ. J. Solid State Chem. 150, 149–233 (2000)10.1006/jssc.1999.8551 ↗
21. J. Piao, K. Sun, N. Zhang, X. Chen, S. Xu, D. Zhou, Preparation and characterization of Pr1–xSrxFeO3 cathode material for intermediate temperature solid oxide fuel cells. J. Power Sourc. 172, 633–640 (2007)10.1016/j.jpowsour.2007.05.023 ↗
22. E. Boehm, J.M. Bassat, M.C. Steil, P. Dordor, F. Mauvy, J.C. Grenier, Oxygen transport properties of La2Ni1–xCuxO4+δ mixed conducting oxides. Solid State Sci. 5, 973–981 (2003)10.1016/S1293-2558(03)00091-8 ↗
23. H. Lv, Y. Wu, B. Huang, B. Zhao, K. Hu, Structure and electrochemical properties of Sm0.5Sr0.5Co1–xFexO3–δ cathodes for solid oxide fuel cells. Solid State Ionics 177, 901–906 (2006)10.1016/j.ssi.2006.01.038 ↗
24. H. Takahashi, F. Munakata, M. Yamanaka, Ab initio study of the electronic structures in LaCoO3–SrCoO3 systems. Phys. Rev. B 57, 15211 (1998)10.1103/PhysRevB.57.15211 ↗
25. K.T. Lee, A. Manthiram, LaSr3Fe3–yCoyO10–δ (0 ≤ y ≤ 1.5) intergrowth oxide cathodes for intermediate temperature solid oxide fuel cells. Chem. Mater. 18, 1621–1626 (2006)10.1021/cm052645+ ↗
26. M. Karmele Vidal, L. Rodríguez-Martínez, L. Ortega-San-Martín, E. Díez-Linaza, M. Luisa Nó, T. Rojo, A. Laresgoiti, M. Isabel Arriortua, Isolating the effect of doping in the structure and conductivity of (Ln1–xMx)FeO3–δ perovskites. Solid State Ionics 178, 1310–1316 (2007)10.1016/j.ssi.2007.06.015 ↗
27. T.Z. Jiang, Z.H. Wang, B.Y. Ren, J.S. Qiao, W. Sun, K.N. Sun, Compositionally continuously graded cathode layers of (Ba0.5Sr0.5)(Fe0.91Al0.09)O3–δ–Gd0.1Ce0.9O2 by wet powder spraying technique for solid oxide fuel cells. J. Power Sources 247, 858–864 (2014)10.1016/j.jpowsour.2013.09.034 ↗
28. G.Z. Xing, Y. Wang, J.I. Wong, Y.M. Shi, Z.X. Huang, S. Li, H.Y. Yang, Hybrid CuO/SnO2 nanocomposites: towards cost-effective and high performance binder free lithium ion batteries anode materials. Appl. Phys. Lett. 105, 143905 (2014)10.1063/1.4896256 ↗
29. S.B. Adler, Limitations of charge-transfer models for mixed-conducting oxygen electrodes. Solid State Ionics 135, 603–612 (2000)10.1016/S0167-2738(00)00423-9 ↗
30. S.Y. Li, Z. Lü, B. Wei, X.Q. Huang, J.P. Miao, Z.G. Liu Performances of Ba0.5Sr0.5Co0.6Fe0.4O3–δ–Ce0.8Sm0.2O1.9 composite cathode materials for IT-SOFC. J. Alloys Compd. 448, 116–121 (2008)10.1016/j.jallcom.2006.10.032 ↗
31. S. Lü, G. Long, Y. Ji, X. Meng, C. Sun, Characterization of SmBaCoFeO5 + δ-Ce0.9Gd0.1O1.95 composite cathodes for intermediate-temperature solid oxide fuel cells. Int. J. Hydrogen Energy 35, 7930–7935 (2010)10.1016/j.ijhydene.2010.05.058 ↗
32. Y. Ji, H. Wang, H. Zhang, Gd0.8Sr0.2CoO3 – δ–Sm0.1Ce0.9O1.95 composite cathode for intermediate temperature solid oxide fuel cells. Mater. Res. Bull. 85, 30–34 (2017)10.1016/j.materresbull.2016.09.001 ↗
33. B. Wei, Z. Lü, X. Huang, M. Liu, N. Li, W. Su, J. Power Sourc. 176, 1–8 (2008)10.1016/j.jpowsour.2007.09.120 ↗
34. K.T. Lee, A. Manthiram, Effect of cation doping on the physical properties and electrochemical performance of Nd0.6Sr0.4Co0.8M0.2O3–δ(M = Ti, Cr, Mn, Fe, Co, and Cu) cathodes. Solid State Ionics 178, 995–1000 (2007)10.1016/j.ssi.2007.04.010 ↗
35. Ho-ChiehY.Kuan-Zong Fung, Electrode properties of La1–xSrxCuO2.5–δ as new cathode materials for intermediate-temperature SOFCs. J. Power Sourc. 133, 162–168 (2004)10.1016/j.jpowsour.2004.02.002 ↗
36. M.M. Li, J.G. Cheng, Y. Gan, S.S. Li, B.B. He, W.Z. Sun, Effects of strontium doping on the structure, oxygen nonstoichiometry and electrochemical performance of Pr2–xSrxNi0.6Cu0.4O4 + δ (0.1 ≤ x ≤ 0.5) cathode materials. J. Power Sourc. 275, 151–158 (2015)10.1016/j.jpowsour.2014.10.191 ↗