Microstructure of Cu–Ni–Si alloys, especially morphology, amount and size of Ni–Si intermetallics, was controlled by heat and thermal–mechanical treatment, and then its influence on electrical breakdown behavior was investigated systematically. Results show that first breakdown is prior to occur on the Ni3Si phase at the grain boundary and δ-Ni2Si in the inner of Cu matrix in Cu–Ni–Si alloys. The decrease of Ni3Si size by using thermal–mechanical treatment can significant enhance the breakdown behavior of Cu–Ni–Si alloys since it can change the total area of preferred phase within the action area of cathode spot. As a result, the chopping current and erosion depth decrease but arc life, breakdown field and erosion area increase with the decrease of Ni3Si size, while the precipitation δ-Ni2Si phase has limited effect on breakdown properties. On the whole, Cu–Ni–Si alloy by solution, hot forging and aging treatments in sequence has the best breakdown properties due to the uniform dispersion of Ni3Si phase.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electromagnetic Effects on Materials · Semiconductor materials and interfaces · Electrodeposition and Electroless Coatings

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. S. Gorsse, B. Ouvrard, M. Gouné, A. Poulon-Quintin, J. Alloys Compd 633, 42 (2015)10.1016/j.jallcom.2015.01.234 ↗
2. C. Watanabe, R. Monzen, K. Tazaki, J. Mater. Sci. Mater. Electron. 43(3), 813 (2008)
3. S. Xu, H. Fu, Y. Wang, J. Xie, Mater. Sci. Eng. A 726, 208 (2018)10.1016/j.msea.2018.04.077 ↗
4. D. Li, Q. Wang, B. Jiang, X. Li, W. Zhou, C. Dong, H. Wang, Q. Chen, Prog. Nat. Sci. Mater. Int. 27, 467 (2017)10.1016/j.pnsc.2017.06.006 ↗
5. W. Wang, H. Kang, Z. Chen, Z. Chen, C. Zou, R. Li, G. Yin, T. Wang, Mater. Sci. Eng. A 673, 378 (2016)10.1016/j.msea.2016.07.021 ↗
6. X. Xiao, Z. Yi, T. Chen, R. Liu, H. Wang, J. Alloys Compd 660, 178 (2016)10.1016/j.jallcom.2015.11.103 ↗
7. J. Chalon, J.D. Guérin, L. Dubar, A. Dubois, E.S. Puchi-Cabrera, Mater. Sci. Eng. A 667, 77 (2016)10.1016/j.msea.2016.04.061 ↗
8. M.G. Corson, Trans. AIME 77, 435 (1927)
9. X.J. Liu, S.L. Xiang, S.Y. Yang, R.P. Shi, C.P. Wang, J. Alloys Compd 578, 439 (2013)10.1016/j.jallcom.2013.06.072 ↗
10. C. Watanabe, R. Monzen, J. Mater. Sci. Mater. Electron. 46(12), 4327 (2011)
11. S. Suzuki, N. Shibutani, K. Mimura, M. Isshiki, Y. Waseda, J. Alloys Compd 417, 116 (2006)10.1016/j.jallcom.2005.09.037 ↗
12. D.M. Zhao, Q.M. Dong, P. Liu, B.X. Kang, J.L. Huang, Z.H. Jin, Mater. Chem. Phys. 79, 81 (2003)10.1016/S0254-0584(02)00451-0 ↗
13. M. Gholami, J. Vesely, I. Altenberger, H.A. Kuhn, M. Janecek, M. Wollmann, L. Wagner, J. Alloys Compd 696, 201 (2017)10.1016/j.jallcom.2016.11.233 ↗
14. R. Monzen, C. Watanabe, Mater. Sci. Eng. A 483–484, 117 (2008)10.1016/j.msea.2006.12.163 ↗
15. H. Xie, L. Jia, Z. Lu, Mater. Charact. 60, 114 (2009)10.1016/j.matchar.2008.07.008 ↗
16. L. Jia, H. Xie, Z.L. Lu, X. Wang, S.M. Wang, Mater. Sci. Technol. 28, 243 (2012)10.1179/1743284711Y.0000000054 ↗
17. Y. Yamamoto, H. Sasaki, M. Odasin, J. Jpn. Copp. Brass Res. Assoc. 38, 204 (1999). (in Japanese)
18. H.J. Ryu, H.K. Baik, S.H. Hong, J. Mater. Sci. 35, 3641 (2000)10.1023/A:1004830000742 ↗
19. L. Jia, H. Xie, Z.L. Lu, X. Wang, Y.L. Zhao, Mater. Sci. Forum 695, 344 (2011)10.4028/www.scientific.net/MSF.695.344 ↗
20. J.L. Zhang, Z.L. Lu, Y.T. Zhao, L. Jia, H. Xie, S.P. Tao, Mater. Res. Express 4, 096511 (2017)10.1088/2053-1591/aa87f9 ↗
21. H. Azzeddine, B. Mehdi, L. Hennet, D. Thiaudière, B. Alili, M. Kawasaki, D. Bradai, T.G. Langdon, Mater. Sci. Eng. A 597, 288 (2014)10.1016/j.msea.2013.12.092 ↗
22. Q. Lei, Z. Li, M.P. Wang, L. Zhang, S. Gong, Z. Xiao, Z.Y. Pan, J. Alloys Compd 509, 3617 (2011)10.1016/j.jallcom.2010.12.115 ↗
23. Q. Lei, Z. Xiao, W. Hu, B. Derby, Z. Li, Mater. Sci. Eng. A 697, 37 (2017)10.1016/j.msea.2017.05.001 ↗
24. D.M. Zhao, Q.M. Dong, P. Liu, B.X. Kang, J.L. Huang, Z.H. Jin, Mater. Sci. Eng. A 361, 93 (2003)10.1016/S0921-5093(03)00496-9 ↗
25. Y.A. Wang, J.X. Li, Y. Yan, L.J. Qiao, Tribol. Int. 50, 26 (2012)10.1016/j.triboint.2011.12.022 ↗
26. X. Wang, S. Liang, P. Yang, Z. Fan, Vacuum 83, 1475 (2009)10.1016/j.vacuum.2009.06.049 ↗
27. H.Y. Li, X. Zhou, X.Q. Lu, Y.P. Wang, Trans. Nonferr. Met. Soc. China (Engl. Ed.) 27, 102 (2017)10.1016/S1003-6326(17)60011-6 ↗
28. H.X. Yang, S. Liang, X. Wang, P. Xiao, Z. Fan, Int J Refract Met Hard Mater 28, 305 (2010)10.1016/j.ijrmhm.2009.11.009 ↗
29. H.I. Choi, K.Y. Lee, S.I. Kwun, J. Mater. Sci. Lett. 16, 1600 (1997)10.1023/A:1018580721028 ↗
30. W.C. Cao, S.H. Liang, X. Zhang, X.H. Wang, X.H. Yang, Vacuum 85, 943 (2011)10.1016/j.vacuum.2011.02.001 ↗
31. J.A. Kittl, M.A. Pawlak, A. Lauwers, C. Demeurisse, K. Opsomer, K.G. Anil, C. Vrancken, M.J.H. van Dal, A. Veloso, S. Kubicek, P. Absil, K. Maex, S. Biesemans, IEEE Electron Device Lett. 27, 34 (2006)10.1109/LED.2005.861404 ↗
32. E.Z. Luo, Y.P. Liu, W.D. Liu, L.J. Chen, M.S. Zheng, Acta Electron. Sin. 24, 5 (1996). (in Chinese)