Abstract
Aluminum is widely used as a heavy current with thick wire and is also used for aerospace and automotive in recent years. In addition, Al wires usually apply to semiconductor with bonding wire process. In this study, the wire material contained Al-7 wt% Zn-0.3 wt% Si, called ZS703, with drawing and heat treatment to obtain 12 mil (300 μm) and 4 mil (100 μm) Al alloy fine wires. These wires form an isometric crystal structure, which resulted in hardness decrease with annealing heat treatment. After heat treatment, the grain size and elongation increased obviously. Regardless of the diameter of Al wires, the electrical measurements (I–V curve) indicated abnormal increase in resistance (platform zone of I–V curve) at a certain current. This result caused incandescence (the void effect and joule heat). After platform zone of I–V curve, the resistance of all Al wires increased and the fuse current decreased because of decreasing of electrical effective cross-sectional area. After chlorination, the mechanical properties of the wires did not change obviously for both of the 4 mil Al wires (ZS703 and ZS703H), but elongation decreased significantly. Especially for ZS703H wire, the wires were brittle due to poor resistance to chlorine. In electrical analysis, the thin film formation of Al(OH)3 was found that increased the cross-sectional area of effective conduction. As a result, the resistance of the Al wires decreased before incandescence phenomenon, and the fusing current decreases because of melt-void effect of current.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Electronic Packaging and Soldering Technologies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. T.Y. Hung, S.Y. Chiang, C.J. Huang, C.C. Lee, K.N. Chiang, Thermal-mechanical behavior of the bonding wire for a power module subjected to the power cycling test. Microelectron. Reliab. 51, 1819–1823 (2011)10.1016/j.microrel.2011.06.048 ↗
2. P. Sun, C. Gong, X. Du, Y. Peng, B. Wang, L. Zhou, Condition monitoring IGBT module bond wires fatigue using short-circuit current identification. IEEE Trans. Power Electron. 32, 3777–3786 (2017)10.1109/TPEL.2016.2585669 ↗
3. Y. Huang, Y. Jia, Y. Luo, F. Xiao, B. Liu, Lifting-off of Al bonding wires in IGBT modules under power cycling: failure mechanism and lifetime model. IEEE J. Emerg. Selected Topics Power Electr. 1, 11 (2019). https://doi.org/10.1109/JESTPE.2019.292424110.1109/JESTPE.2019.2924241 ↗
4. H. Tsai, J. Lee, C. Tsai, H. Wang, C. Chang and T. Chuang, An innovative annealing-twinned Ag–Au–Pd bonding wire for IC and LED packaging. in 2012 7th International Microsystems, Packaging, Assembly and Circuits Technology Conference (IMPACT), (Taipei, 2012), pp. 243–246.10.1109/IMPACT.2012.6420241 ↗
5. M.H. Lue, C.T. Huang, S.T. Huang, K.C. Hsieh, Bromine-and chlorine-induced degradation of gold-aluminum bonds. J. Electron. Mater. 33, 1111–1117 (2004)10.1007/s11664-004-0112-z ↗
6. Y. T. Chiu, T. H. Chiang, P. F. Yang and C. P. Hung, The corrosion behavior of Ag alloy wire bond on Al pad in molding compounds of various chlorine contents under biased-HAST. in 2016 International Conference on Electronics Packaging (ICEP), (Sapporo, 2016), pp. 497–501.10.1109/ICEP.2016.7486877 ↗
7. S.K. Prasad, Advanced wirebond interconnection technology (Springer Science & Business Media, New York, 2004)
8. M.S. Broll, U. Geissler, J. Höfer, S. Schmitz, O. Wittler, K.D. Lang, Microstructural evolution of ultrasonic-bonded aluminum wires. Microelectron. Reliab. 55, 961–968 (2015)10.1016/j.microrel.2015.03.002 ↗
9. G. Khatibi, B. Weiss, J. Bernardi, S. Schwarz, Microstructural investigation of interfacial features in Al wire bonds. J. Electron. Mater. 41, 3436–3446 (2012)10.1007/s11664-012-2215-2 ↗
10. S. Park, S. Nagao, T. Sugahara, K. Suganuma, Mechanical stabilities of ultrasonic Al ribbon bonding on electroless nickel immersion gold finished Cu substrates. Jpn. J. Appl. Phys. 53, 1–6 (2014)
11. K. M. Chu, Electronic flame-off mechanism and wire bonding reliability of fine Zn-coated Al-Si wires. Master Thesis, Department of Materials Science and Engineering, National Cheng Kung University, Tainan, Taiwan, 2016.
12. F.Y. Hung, T.S. Lui, K.M. Chu, Y.W. Tseng, Aluminum wires have the free air balls (FABs): electronic flame-off, fracture strength, electrical properties, and bonding characteristics of nano Zn film Al–Si bonding wires. Metals 7, 1–12 (2017)10.3390/met7050152 ↗
13. S.A. Jasim, Improving of some mechanical properties, microstructure and electrical conductivity of pure aluminum by adding zinc. J. Univ. Babylon 25, 119–128 (2017)
14. R.S. Rana, R. Purohit, S. Das, Reviews on the influences of alloying elements on the microstructure and mechanical properties of aluminum alloys and aluminum alloy composites. Int. J. Sci. Res. Publ. 2, 1–7 (2012)
15. G. Karunesh, Y.J. Manjunath, Determination of mechanical properties of aluminum alloy (7075) reinforced with aluminum oxide (Al2O3). Int. J. Eng. Res. 5, 1141–1146 (2016)
16. B. Zaid, D. Saidi, A. Benzaid, S. Hadji, Effects of pH and chloride concentration on pitting corrosion of AA6061 aluminum alloy. Corros. Sci. 50, 1841–1847 (2008)10.1016/j.corsci.2008.03.006 ↗
17. Y.H. Wu, F.Y. Hung, T.S. Lui, K.J. Chen, Study of wire bonding reliability of Ag–Pd–Au alloy wire with flash-gold after chlorination and sulfidation. Microelectron. Reliab. 99, 186–196 (2019)10.1016/j.microrel.2019.05.014 ↗
18. L. Merkle, T. Kaden, M. Sonner, A. Gademann, J. Turki, Mechanical fatigue properties of heavy aluminium wire bonds for power applications. in 2008 2nd Electronics System-Integration Technology Conference, (Greenwich, 2008), pp. 1363–1368.10.1109/ESTC.2008.4684554 ↗
19. J.P. Hou, R. Li, Q. Wang, H.Y. Yu, Z.J. Zhang, Q.Y. Chen, H. Ma, X.M. Wu, X.W. Li, Z.F. Zhang, Three principles for preparing Al wire with high strength and high electrical conductivity. J. Mater. Sci. Technol. 35, 742–751 (2019)10.1016/j.jmst.2018.11.013 ↗
20. K.P. Yau, D.G. Schulze, C.T. Johnston, S.L. Hem, Aluminum hydroxide adjuvant produced under constant reactant concentration. J. Pharm. Sci. 95, 1822–1833 (2006)10.1002/jps.20692 ↗