Microstructure and electrical properties of ZnO–Pr6O11–Bi2O3-based varistor ceramics with sintering changes
Source abstract
Abstract
The effect of sintering temperature on microstructure, electrical properties, and dielectric characteristics of the ZnO–Pr6O11–Bi2O3-based varistor ceramics was systematically investigated. When the sintering temperature increased, the average grain sizes increased from 1.7 to 4.9 μm, and the densities of the sintered pellets increased from 5.45 to 5.83 g/cm3 until the sintering temperature is 1200 °C. When the sintering temperature increased from 1100 to 1150 °C, the breakdown field decreased sharply from 24.6 to 5.1 kV/cm, and the non–ohmic coefficient decreased sharply from 75.0 to 8.6. When the sintering temperature exceeded 1150 °C, the breakdown field decreased to 3.1 kV/cm at 1250 °C, and the non-ohmic coefficient was roughly 10, and then almost not affected by the sintering temperature. The dielectric constant increased from 115.7 to 896.9 with the increase of sintering temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · High voltage insulation and dielectric phenomena · Transition Metal Oxide Nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. L.M. Levinson, H.R. Philipp, Am. Ceram. Soc. Bull. 65, 639 (1986)
2. T.K. Gupta, J. Am. Ceram. Soc. 73, 1817 (1990)10.1111/j.1151-2916.1990.tb05232.x ↗
3. K. Mukae, Am. Ceram. Bull. 66, 1329 (1987)
4. K. Mukae, K. Tsuda, S. Shiga, IEEE Trans. Power Deliv. 3, 591 (1988)10.1109/61.4296 ↗
5. K. Mukae, K. Tsuda, Jpn. J. Ceram. Soc. 100, 1048 (1992)10.2109/jcersj.100.1048 ↗
6. C.-W. Nahm, Mater. Lett. 47, 182 (2001)10.1016/S0167-577X(00)00262-7 ↗
7. H. Heng, X. Fu, Z. Fu, C. Wang, L. Qi, H. Miao, J. Alloys Compd. 497, 304 (2010)10.1016/j.jallcom.2010.03.047 ↗
8. Z. Peng, X. Fu, Y. Zang, Z. Fu, C. Wang, L. Qi, H. Miao, J. Alloys Compd. 508, 494 (2010)10.1016/j.jallcom.2010.08.100 ↗
9. C.-W. Nahm, J. Rare Earth 30, 1028 (2012)10.1016/S1002-0721(12)60174-4 ↗
10. C.-W. Nahm, J. Am. Ceram. Soc. 96, 2732 (2013)10.1111/jace.12548 ↗
11. C.-W. Nahm, Ceram. Int. 40, 2477 (2014)10.1016/j.ceramint.2013.07.007 ↗
12. C.-W. Nahm, Ceram. Int. 40, 12561 (2014)10.1016/j.ceramint.2014.03.164 ↗
13. C.-W. Nahm, Microelectron. Reliab. 55, 565 (2015)10.1016/j.microrel.2015.01.012 ↗
14. J.C. Wurst, J.A. Nelson, J. Am. Ceram. Soc. 55, 109 (1972)10.1111/j.1151-2916.1972.tb11224.x ↗