Abstract

In this paper, the reaction-bonded SiC materials with super lithium-ion corrosion resistance and ultra-high mechanical properties were prepared by surface treatment. The surface treatment of reaction-bonded SiC was carried out by nitriding treatment to reduce the content of free Si. The mechanical properties of the reaction-bonded SiC treated at different nitriding temperatures were analyzed. The corrosion reaction of lithium-ion cathode material on reaction-bonded SiC was studied. The results show that when the nitriding temperature is 1350 °C, the mechanical properties reach the maximum and the corresponding corrosion resistance is greatly improved. The bending strength increases from (265.3 ± 8.7) to (425.4 ± 8.3) MPa, and the fracture toughness increases from (3.7 ± 0.3) MPa m1/2 to (4.5 ± 0.2) MPa m1/2. In general, the corrosion resistance and mechanical properties of surface-treated SiC materials are significantly improved compared with that of original SiC materials, indicating that surface-treated SiC has a broader application prospect in the synthesis of lithium-ion cathode materials.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advancements in Battery Materials · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. X. Duan, H. Zheng, Y. Chen et al., Study on the corrosion resistance of cordierite-mullite and SiC refractories to Li-ion ternary cathode materials. Ceram. Int. 46(3), 2829–2835 (2020)10.1016/j.ceramint.2019.09.275 ↗
2. L. Liu, X. Feng, C. Rahe et al., Internal short circuit evaluation and corresponding failure mode analysis for lithium-ion batteries. J. Energy Chem. 61, 269–280 (2021)10.1016/j.jechem.2021.03.025 ↗
3. J.M. Lim, T. Hwang, D. Kim et al., Intrinsic origins of crack generation in Ni-rich LiNi0.8Co0.1Mn0.1O2 layered oxide cathode material. Sci. Rep. 7(1), 1–10 (2017)10.1038/s41598-016-0028-x ↗
4. W. Liu, P. Oh, X. Liu et al., Nickel-rich layered lithium transition‐metal oxide for high‐energy lithium‐ion batteries. Angew. Chem. Int. Ed. 54(15), 4440–4457 (2015)10.1002/anie.201409262 ↗
5. X. Zhang, X. Sun, X. Li et al., Recent progress in rate and cycling performance modifications of vanadium oxides cathode for lithium-ion batteries. J. Energy Chem. 59, 343–363 (2021)10.1016/j.jechem.2020.11.022 ↗
6. B. Huang, X. Li, Z. Wang et al., A comprehensive study on electrochemical performance of Mn-surface-modified LiNi0.8Co0.15Al0. 05O2 synthesized by an in-situ oxidizing-coating method. J. Power Sources 252(252), 200–207 (2014)10.1016/j.jpowsour.2013.11.092 ↗
7. E. Panjaitan, A. Manaf, B. Soegijono et al., Effect of additional poly vinyledene fluoride (PVDF) on LiCoO2 cathodes. Proc. Chem. 4, 60–64 (2012)10.1016/j.proche.2012.06.009 ↗
8. H. Liang, Z. Wang, H. Guo et al., Improvement in the electrochemical performance of LiNi0.8Co0.1Mn0.1O2 cathode material by Li2ZrO3 coating. Appl. Surf. Sci. 423(30), 1045–1053 (2017)10.1016/j.apsusc.2017.06.283 ↗
9. M. Chen, E. Zhao, D. Chen et al., Decreasing Li/Ni disorder and improving the electrochemical performances of Ni-rich LiNi0.8Co0.1Mn0.1O2 by Ca doping. Inorg. Chem. 56(14), 8355–8362 (2017)10.1021/acs.inorgchem.7b01035 ↗
10. T. Ohji, High-temperature reliability of advanced ceramics. J. Energy Res. Technol. 123(1), 64–69 (2001)10.1115/1.1347990 ↗
11. A.P. Garshin, V.I. Kulik, A.S. Nilov, Analysis of the status and prospects for the commercial use of fiber-reinforced silicon-carbide ceramics. Refract. Ind. Ceram 53(1), 62–70 (2012)10.1007/s11148-012-9463-9 ↗
12. X. He, Y. Zhou, D. Jia et al., Effect of sintering additives on microstructures and mechanical properties of short-carbon-fiber-reinforced SiC composites prepared by precursor pyrolysis–hot pressing. Ceram. Int. 32(8), 929–934 (2006)10.1016/j.ceramint.2005.07.007 ↗
13. J.S. Lee, T. Yano, Fabrication of short-fiber-reinforced SiC composites by polycarbosilane infiltration. J. Eur. Ceram. Soc. 24(1), 25–31 (2004)10.1016/S0955-2219(03)00125-0 ↗
14. K. Park, T. Vasilos, Interface and thermal shock resistance of SiC fiber/SiC composites. Scripta Mater. 39, 11 (1998)10.1016/S1359-6462(98)00356-X ↗
15. M.A. Mulla, V.D. Krstic, Mechanical properties of β-SiC pressureless sintered with Al2O3 additions. Acta Metall. Mater. 42(1), 303–308 (1994)10.1016/0956-7151(94)90072-8 ↗
16. S.N. Perevislov, M.A. Markov, A.V. Krasikov et al., Effect of SiC dispersed composition on physical and mechanical properties of reaction-sintered silicon carbide. Refract. Ind. Ceram 61(2), 211–215 (2020)10.1007/s11148-020-00458-4 ↗
17. Z. Ren, W. Zhou, Y. Qing et al., Effect of different kinds of SiC fibers on microwave absorption and mechanical properties of SiCf/SiC composites. J. Mater. Sci.: Mater. Electron. 32(21), 25668–25678 (2021)
18. L. Cheng, K. Ma, X. Yue et al., Role of Ti in direct active bonding of SiC substrate using Sn-Ag-Ti alloy filler. J. Mater. Sci.: Mater. Electron. 33(6), 3331–3347 (2022)
19. S. Suyama, T. Kameda, Y. Itoh, Development of high-strength reaction-sintered silicon carbide. Diam. Relat. Mater. 12(3–7), 1201–1204 (2003)10.1016/S0925-9635(03)00066-9 ↗
20. S. Duan, D. Zhu, W. Zhou, et al. Mechanical and microwave absorption properties of Ti-filled SiCf/SiC composites via precursor infiltration and pyrolysis. J. Mater. Sci.: Mater. Electron. 31, 2634–2642 (2020)
21. S. Ge, X. Yao, Y. Liu et al., Effect of sintering temperature on the properties of highly electrical resistive SiC ceramics as a function of Y2O3-Er2O3 additions. Materials 13(21), 4768 (2020)10.3390/ma13214768 ↗
22. Y. Zhang, L. Shuang, J. Han et al., Fabrication and characterization of random chopped fiber reinforced reaction bonded silicon carbide composite. Ceram. Int. 38(2), 1261–1266 (2012)10.1016/j.ceramint.2011.08.058 ↗
23. J. Li, X. Ren, Y. Zhang et al., Silicon carbide hot-pressing sintered by magnesium additive: microstructure and sintering mechanism. J. Mater. Res. Technol. 9(1), 520–529 (2020)10.1016/j.jmrt.2019.10.081 ↗
24. N.F. Gadzyra, N.K. Davidchuk, G.G. Gnesin, Structurization of composite ceramics based on stoichiometric silicon carbide during free sintering and hot pressing. Powder Metall. Met. Ceram. 48(5–6), 311–315 (2009)10.1007/s11106-009-9129-4 ↗
25. K. Itatani, T. Tanaka, I.J. Davies et al., Some properties of silicon carbide composites fabricated with chopped Si-Al-C fibers. Int. J. Mater. Prod. Technol. 16(1–3), 239–247 (2001)10.1504/IJMPT.2001.005436 ↗
26. S.K. Lee, Y.C. Kim, C.H. Kim, Microstructural development and mechanical properties of pressure-less sintered SiC with plate-like grains using Al2O3-Y2O3 additives. J. Mater. Sci. 29(20), 5321–5326 (1994)10.1007/BF01171542 ↗
27. T. Zhang, Z. Zhang, J. Zhang et al., Preparation of SiC ceramics by aqueous gelcasting and pressureless sintering. Mater. Sci. Eng. A 443(1–2), 257–261 (2007)10.1016/j.msea.2006.08.047 ↗
28. C. Li, S. Li, D. An et al., Microstructure and mechanical properties of spark plasma sintered SiC ceramics aided by B4C. Ceram. Int. 46(8), 10142–10146 (2020)10.1016/j.ceramint.2020.01.005 ↗
29. D.P. Shornikov, A.V. Tenishev, V.N. Kazakova et al. Fabrication of a high-density compacted material from a coarse-grained silicon carbide powder by magnetic pulsed pressing combined with spark plasma sintering. Russian Metallurgy (Metally), 2019, 2019(10): 1102–110610.1134/S0036029519100252 ↗
30. M. Lodhe, N. Chawake, D. Yadav et al., On the correlation between β→α transformation and densification mechanisms in SiC during spark plasma sintering. Scripta Mater. 115(1), 137–140 (2016)10.1016/j.scriptamat.2016.01.002 ↗
31. S. Suyama, Y. Itoh, Strengthening mechanism of high-strength reaction-sintered silicon carbide. Key Eng. Mater. 484, 89–97 (2011)10.4028/www.scientific.net/KEM.484.89 ↗
32. J. Lee, D. Kim, D. Shin et al., A new process for minimizing residual silicon and carbon of reaction-bonded silicon carbide via chemical vapor deposition. J. Eur. Ceram. Soc. 41(7), 4000–4005 (2021)10.1016/j.jeurceramsoc.2021.02.009 ↗
33. V.G. Kulich, A.L. Maystrenko, V.N. Tkach et al., Saturation of capillary pores in silicon carbide briquettes with liquid–phase carbon-containing solutions before the reaction-sintering. J. Super-hard Mater. 38(6), 402–411 (2016)10.3103/S1063457616060046 ↗
34. Y. Xuanye, Y. Hongge, C. Jihua et al., Solid-state synthesis of ultrafine-LiCoO2 by enhanced thermal decomposition of carbonate precursors followed by double-calcining. Solid State Ionics 289, 159–167 (2016)10.1016/j.ssi.2016.03.005 ↗
35. C. Lagergren, Synthesis and performance of LiCoO2 cathodes for the molten carbonate fuel cell. J. Electrochem. Soc. 141(11), 2959–2966 (1994)10.1149/1.2059265 ↗
36. L. Giorgi, M. Carewska, M. Patriarca et al., Development and characterization of novel cathode materials for molten carbonate fuel cell. J. Power Sources 49(1–3), 227–243 (1994)10.1016/0378-7753(93)01814-X ↗
37. X. Yang, H. Yan, J. Chen et al., Solid-state synthesis of ultrafine-LiCoO2 by enhanced thermal decomposition of carbonate precursors followed by double-calcining. Solid State Ionics 289, 159–167 (2016)10.1016/j.ssi.2016.03.005 ↗
38. G. Yao, Y. Li, P. Jiang et al., Formation mechanisms of Si3N4 and Si2N2O in silicon powder nitridation. Solid State Sci. 66, 50–56 (2017)10.1016/j.solidstatesciences.2017.03.002 ↗
39. H.T. Lin, S. Waters, K. Breder, High-temperature creep response of a commercial grade siliconized silicon carbide. J. Mater. Sci. 34(18), 4393–4398 (1999)10.1023/A:1004616617093 ↗
40. J. Binner, Y. Zhang, Characterization of silicon carbide and silicon powders by XPS and zeta potential measurement. J. Mater. Sci. Lett. 20(2), 123–126 (2001)10.1023/A:1006734100499 ↗
41. E. Ravizza, S. Spadoni, R. Piagge et al., XPS composition study of stacked Si oxide/Si nitride/Si oxide nano-layers. Surf. Interface Anal. 44(8), 1209–1213 (2012)10.1002/sia.4943 ↗
42. J.P. Iii, G. Subhash, A. Trachet et al., The rate-dependent response of pressureless-sintered and reaction-bonded silicon carbide-based ceramics. Int. J. Appl. Ceram. Technol. 12, E207–E216 (2015)10.1111/ijac.12332 ↗
43. S.K. Lee, W. Ishida, S.Y. Lee et al., Crack-healing behavior and resultant strength properties of silicon carbide ceramic. J. Eur. Ceram. Soc. 25(5), 569–576 (2005)10.1016/j.jeurceramsoc.2004.01.021 ↗
44. K. Ando, M.C. Chu, K. Tsuji et al., Crack healing behaviour and high-temperature strength of mullite/SiC composite ceramics. J. Eur. Ceram. Soc. 22(8), 1313–1319 (2002)10.1016/S0955-2219(01)00431-9 ↗
45. K.W. Nam, M.K. Kim, S.W. Park et al., Crack-healing behavior and bending strength of Si3N4/SiC composite ceramics by SiO2 colloidal. Mater. Sci. Eng. A 471(1–2), 102–105 (2007)10.1016/j.msea.2007.03.005 ↗