journal article·2016-10Open access

Comparison of the superelasticity of different nickel–titanium orthodontic archwires and the loss of their properties by heat treatment

Humberto Bellini, Javier Moyano, Javier Gil, Andreu Puigdollers

Abstract

The aim of this work is to describe and compare mechanical properties of eight widely used nickel-titanium orthodontic wires under uniform testing conditions and to determine the influence of the heat treatments on the loss of the superelasticity. Ten archwires from two batches from eight different manufacturers were evaluated. A three-point bending test was performed, in accordance with ISO 15841:2006, on 80 round nickel-titanium archwire segments of 0.016 inch. To obtain a load-deflection curve, the centre of each segment was deflected to 3.1 mm and then unloaded until force became zero. On the unloading curve, deflection at the end of the plateau and forces delivered at that point, and at 3, 2, 1 and 0.5 mm of deflection, were recorded. Plateau slopes were calculated from 3 and from 2 mm of deflection. Data obtained were statistically analysed to determine inter-brand, intra-brand and inter-batch differences (P < 0.05). The results show that at 2 mm of deflection, maximum differential force exerted among brands [Nitinol SuperElastic (1.999N)-Sentalloy M (1.001 N)] was 0.998 N (102 gf). The Nitinol SuperElastic plateau slope (0.353 N/mm) was the only one that was statistically different from 2 mm of deflection, as compared with the other brand values (0.129-0.155 N/mm). Damon Optimal Force described the gentlest slope from 3 mm of deflection (0.230 N/mm) and one of the longest plateaus. Titanol and Orthonol showed the most notable intra-brand differences, whereas inter-batch variability was significant for Nitinol (Henry Schein), Euro Ni-Ti and Orthonol. Superelasticity degree and exerted forces differed significantly among brands. Superelasticity of Nitinol SuperElastic was not observed, while Damon Optimal Force and Proclinic Ni-Ti Superelástico (G&H) showed the most superelastic curves. Intra-brand and inter-batch differences were observed in some brands. In all cases, the heat treatment at 600 °C produces precipitation in the matrix. The precipitates are rich in titanium and this fact produce changes in the chemical composition of the matrix and the loss of the superelasticity. At 400 °C these precipitates are not produced and the forces delivered by the wires are very similar with wires untreated.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Shape Memory Alloy Transformations · Orthodontics and Dentofacial Orthopedics · Orthopedic Surgery and Rehabilitation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Juvvadi SR, Kailasam V, Padmanabhan S, Chitharanjan AB. Physical, mechanical, and flexural properties of 3 orthodontic wires: an in-vitro study. Am J Orthod Dentofacial Orthop. 2010;138(5):623–30.10.1016/j.ajodo.2009.01.032 ↗
2. Krishnan V, Kumar KJ. Mechanical properties and surface characteristics of three archwire alloys. Angle Orthod. 2004;74(6):825–31.
3. Kapila S, Sachdeva R. Mechanical properties and clinical applications of orthodontic wires. Am J Orthod Dentofacial Orthop. 1989;96(2):100–9.10.1016/0889-5406(89)90251-5 ↗
4. Bourauel C. Nickel–titanium alloys. Material characteristics, corrosion and biocompatibility. University of Bonn 2007.
5. Kusy RP. A review of contemporary archwires: their properties and characteristics. Angle Orthod. 1997;67(3):197–207.
6. Nakano H, Satoh K, Norris R, Jin T, Kamegai T, Ishikawa F, et al. Mechanical properties of several nickel–titanium alloy wires in three-point bending tests. Am J Orthod Dentofacial Orthop. 1999;115(4):390–5.10.1016/S0889-5406(99)70257-X ↗
7. Proffit W. Mechanical principles in orthodontic force control. In: Contemporary orthodontics. 4th ed. St Louis: Mosby 2006.
8. Miura F, Mogi M, Ohura Y, Hamanaka H. The super-elastic property of the Japanese NiTi alloy wire for use in orthodontics. Am J Orthod Dentofacial Orthop. 1986;90(1):1–10.10.1016/0889-5406(86)90021-1 ↗
9. Andreasen G, Heilman H, Krell D. Stiffness changes in thermodynamic Nitinol with increasing temperature. Angle Orthod. 1985;55(2):120–6.
10. Burstone CJ, Qin B, Morton JY. Chinese NiTi wire—a new orthodontic alloy. Am J Orthod. 1985;87(6):445–52.10.1016/0002-9416(85)90083-1 ↗
11. Wilkinson PD, Dysart PS, Hood JA, Herbison GP. Load-deflection characteristics of superelastic nickel–titanium orthodontic wires. Am J Orthod Dentofacial Orthop. 2002;121(5):483–95.10.1067/mod.2002.121819 ↗
12. Waters NE. Superelastic nickel–titanium wires. Br J Orthod. 1992;19(4):319–22.10.1179/bjo.19.4.319 ↗
13. Bartzela TN, Senn C, Wichelhaus A. Load-deflection characteristics of superelastic nickel–titanium wires. Angle Orthod. 2007;77(6):991–8.10.2319/101206-423.1 ↗
14. Segner D, Ibe D. Properties of superelastic wires and their relevance to orthodontic treatment. Eur J Orthod. 1995;17(5):395–402.10.1093/ejo/17.5.395 ↗
15. Liaw YC, Su YY, Lai YL, Lee SY. Stiffness and frictional resistance of a superelastic nickel–titanium orthodontic wire with low-stress hysteresis. Am J Orthod Dentofacial Orthop. 2007;131(5):578.e12–578.e18.
16. Santoro M, Nicolay OF, Cangialosi TJ. Pseudoelasticity and thermoelasticity of nickel–titanium alloys: a clinically oriented review. Part II: deactivation forces. Am J Orthod Dentofacial Orthop. 2001;119(6):594–603.10.1067/mod.2001.112447 ↗
17. Iijima M, Ohta M, Brantley WA, Naganishi A, Murakami T, Muguruma T, et al. Transformation behavior of nickel–titanium orthodontic wires under tensile load. Dent Mater J. 2011;30(3):398–403.10.4012/dmj.2010-196 ↗
18. Tonner RI, Waters NE. The characteristics of super-elastic Ni–Ti wires in three-point bending. Part II: intra-batch variation. Eur J Orthod. 1994;16(5):421–5.10.1093/ejo/16.5.421 ↗
19. Meling TR, Odegaard J. The effect of short-term temperature changes on superelastic nickel–titanium archwires activated in orthodontic bending. Am J Orthod Dentofacial Orthop. 2001;119(3):263–73.10.1067/mod.2001.112451 ↗
20. Lombardo L, Marafioti M, Stefanoni F, Mollica F, Siciliani G. Load deflection characteristics and force level of nickel–titanium initial archwires. Angle Orthod. 2012;82(3):507–21.10.2319/032511-213.1 ↗
21. Bourauel C, Drescher D, Ebling J, Broome D, Kanarachos A. Superelastic nickel–titanium alloy retraction springs—an experimental investigation of force systems. Eur J Orthod. 1997;19(5):491–500.10.1093/ejo/19.5.491 ↗
22. European Committee for Standardization. European Norm EN ISO 15841:2006. Dentistry. Wires for use in orthodontics. 2006.
23. Kusy RP, Dilley GJ. Elastic modulus of a triple-stranded stainless steel arch wire via three- and four-point bending. J Dent Res. 1984;63(10):1232–40.10.1177/00220345840630101401 ↗
24. Brauchli LM, Keller H, Senn C, Wichelhaus A. Influence of bending mode on the mechanical properties of nickel–titanium archwires and correlation to differential scanning calorimetry measurements. Am J Orthod Dentofacial Orthop. 2011;139(5):e449–54.10.1016/j.ajodo.2009.12.034 ↗
25. Khier SE, Brantley WA, Fournelle RA. Bending properties of superelastic and nonsuperelastic nickel–titanium orthodontic wires. Am J Orthod Dentofacial Orthop. 1991;99(4):310–8.10.1016/0889-5406(91)70013-M ↗
26. Gurgel JA, Kerr S, Powers JM, LeCrone V. Force-deflection properties of superelastic nickel–titanium archwires. Am J Orthod Dentofacial Orthop. 2001;120(4):378–82.10.1067/mod.2001.117200 ↗
27. Elayyan F, Silikas N, Bearn D. Mechanical properties of coated superelastic archwires in conventional and self-ligating orthodontic brackets. Am J Orthod Dentofacial Orthop. 2010;137(2):213–7.10.1016/j.ajodo.2008.01.026 ↗
28. Ramazanzadeh BA, Ahrari F, Sabzevari B, Zebarjad SM, Ahrari A. Effects of a simulated oral environment and sterilization on load-deflection properties of superelastic nickel–titanium-based orthodontic wires. Int J Orthod Milwaukee. 2011;22(1):13–21.
29. Wang HM, Wang BK, Ren CC, Bai YX. Properties of NiTi wires with direct electric resistance heat treatment method in three-point bending tests. Zhonghua Kou Qiang Yi Xue Za Zhi. 2011;46(3):168–71.
30. Iijima M, Muguruma T, Brantley W, Choe HC, Nakagaki S, Alapati SB, et al. Effect of coating on properties of esthetic orthodontic nickel–titanium wires. Angle Orthod. 2012;82(2):319–25.10.2319/021511-112.1 ↗
31. Tonner RI, Waters NE. The characteristics of super-elastic Ni–Ti wires in three-point bending. Part I: the effect of temperature. Eur J Orthod. 1994;16(5):409–19.10.1093/ejo/16.5.409 ↗
32. Quintao CC, Cal-Neto JP, Menezes LM, Elias CN. Force-deflection properties of initial orthodontic archwires. World J Orthod. 2009;10(1):29–32.
33. American National Standard/American Dental Association. Specification No. 32. Orthodontic wires: 2006. Accessed 27 May, 2012.
34. 3M Unitek. Orthodontic Wire Properties—Nitinol Archwires. ISO 15841.
35. Gil FJ, Planell JA. Effect of copper addition on the superelastic behavior of Ni–Ti shape memory alloys for orthodontic applications. J Biomed Mater Res. 1999;48(5):682–8.10.1002/(SICI)1097-4636(1999)48:5<682::AID-JBM12>3.0.CO;2-M ↗
36. Arciniegas M, Gaillard Y, Peña J, Manero JM, Gil FJ. Thermoelastic phase transformation in TiNi alloys under cyclic instrumented indentation. Intermetallics. 2009;17:784–91.10.1016/j.intermet.2009.03.020 ↗
37. Firstov GS, Vitchev RG, Kumar H, Blanpain B, Van Humbeeck J. Surface oxidation of NiTi shape memory alloy. Biomaterials. 2002;23:4863–71.10.1016/S0142-9612(02)00244-2 ↗