Nd-induced honeycomb structure of intermetallic phase enhances the corrosion resistance of Mg alloys for bone implants
Source abstract
Abstract
Mg-5.6Zn-0.5Zr alloy (ZK60) tends to degrade too rapid for orthopedic application, in spite of its natural degradation, suitable strength and good biocompatibility. In this study, Nd was alloyed with ZK60 via laser melting method to enhance its corrosion resistance. The microstructure features, mechanical properties and corrosion behaviors of ZK60-xNd (x = 0, 1.8, 3.6, 5.4 wt.%) were investigated. Results showed that laser melted ZK60-xNd were composed of fine ɑ-Mg grains and intermetallic phases along grain boundaries. And the precipitated intermetallic phases experienced successive changes: divorced island-like MgZn phase → honeycomb-like T phase → coarsened and agglomerated W phase with Nd increasing. It was worth noting that ZK60-3.6Nd with honeycomb-like T phase exhibited an optimal corrosion behavior with a corrosion rate of 1.56 mm year-1. The improved corrosion behavior was ascribed to: (I) dense surface film caused by the formation of Nd2O3 hindered the invasion of immersion solution; (II) the three-dimensional honeycomb structure of intermetallic phases formed a tight barrier to restrain the propagation of corrosion. Moreover, ZK60-3.6Nd exhibited good biocompatibility. It was suggested that ZK60-3.6Nd was a preferable candidate for biodegradable bone implant.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Sanchez A, Luthringer B, Feyerabend F, Willumeit R. Mg and Mg alloys: how comparable are in vitro and in vivo corrosion rates? A review. Acta Biomater. 2015;13:16–31.10.1016/j.actbio.2014.11.048 ↗
2. Córdoba L, Montemor M, Coradin T. Silane/TiO 2 coating to control the corrosion rate of magnesium alloys in simulated body fluid. Corros Sci. 2016;104:152–61.10.1016/j.corsci.2015.12.006 ↗
3. Shuai C, Zhou Y, Lin X, Yang Y, Gao C, Shuai X, Wu H, Liu X, Wu P. Preparation and characterization of laser-melted mg–sn–zn alloys for biomedical application. J Mater Sci-Mater Med. 2017;28(1):13.10.1007/s10856-016-5825-z ↗
4. Ang H, Abbott T, Zhu S, Gu C, Easton M. Proof stress measurement of die-cast magnesium alloys. Mater Design. 2016;112:402–9.10.1016/j.matdes.2016.09.088 ↗
5. Rad H, Idris M, Kadir M, Farahany S. Microstructure analysis and corrosion behavior of biodegradable Mg–Ca implant alloys. Mater Design. 2012;33:88–97.10.1016/j.matdes.2011.06.057 ↗
6. Zhang S, Zhang X, Zhao C, Li J, Song Y, Xie C, Tao H, Zhang Y, He Y, Jiang Y. Research on an Mg–Zn alloy as a degradable biomaterial. Acta Biomater. 2010;6(2):626–40.10.1016/j.actbio.2009.06.028 ↗
7. Gu X, Xie X, Li N, Zheng Y, Qin L. In vitro and in vivo studies on a Mg-Sr binary alloy system developed as a new kind of biodegradable metal. Acta Biomater. 2012;8(6):2360–74.10.1016/j.actbio.2012.02.018 ↗
8. Yang Y, Wu P, Wang Q, Wu H, Liu Y, Deng Y, Zhou Y, Shuai C. The enhancement of Mg corrosion resistance by alloying Mn and laser-melting. Materials. 2016;9(4):216.10.3390/ma9040216 ↗
9. Li H, Liu D, Zhao Y, Jin F, Chen M. The influence of Zn content on the corrosion and wear performance of Mg-Zn-Ca alloy in simulated body fluid. J Mater Eng Perform. 2016;25(9):3890–5.10.1007/s11665-016-2207-0 ↗
10. Gu X, Li N, Zheng Y, Ruan L. In vitro degradation performance and biological response of a Mg–Zn–Zr alloy. Mater Sci Eng B-Adv. 2011;176(20):1778–84.10.1016/j.mseb.2011.05.032 ↗
11. Liu C, Jiang J, Wang M, Wang Y, Chu P, Huang W. In In vitro degradation and biocompatibility of WE43, ZK60, and AZ91 biodegradable magnesium alloys, Adv Mater Res, Trans Tech Publ. 2011;287:2008–14.10.4028/www.scientific.net/AMR.287-290.2008 ↗
12. Chen J, Wu P, Wang Q, Yang Y, Peng S, Zhou Y, Shuai C, Deng Y. Influence of alloying treatment and rapid solidification on the degradation behavior and mechanical properties of Mg. Metals. 2016;6(11):259.10.3390/met6110259 ↗
13. Emley E. Principles of Magnesium Technology Pergamon Press. New York, London 1966.
14. Ii R, Bowen P, Hopkins S, Shearier E, Earley E, Gillette A, Aghion E, Bocks M, Drelich J, Goldman J. Corrosion characteristics dictate the long-term inflammatory profile of degradable zinc arterial implants. ACS Biomater Sci Eng. 2016;2(12):2355–64.10.1021/acsbiomaterials.6b00591 ↗
15. Qi Z, Zhang Q, Tan L, Lin X, Yin Y, Wang X, Yang K, Wang Y. Comparison of degradation behavior and the associated bone response of ZK60 and PLLA in vivo. J Biomed Mater Res A. 2014;102(5):1255–63.10.1002/jbm.a.34795 ↗
16. Willbold E, Gu X, Albert D, Kalla K, Bobe K, Brauneis M, Janning C, Nellesen J, Czayka W, Tillmann W. Effect of the addition of low rare earth elements (lanthanum, neodymium, cerium) on the biodegradation and biocompatibility of magnesium. Acta Biomater. 2015;11:554–62.10.1016/j.actbio.2014.09.041 ↗
17. Zucchi F, Grassi V, Frignani A, Monticelli C, Trabanelli G. Electrochemical behaviour of a magnesium alloy containing rare earth elements. J Appl Electrochem. 2006;36(2):195–204.10.1007/s10800-005-9053-3 ↗
18. Zhang X, Yuan G, Mao L, Niu J, Ding W. Biocorrosion properties of as-extruded Mg–Nd–Zn–Zr alloy compared with commercial AZ31 and WE43 alloys. Mater Lett. 2012;66(1):209–11.10.1016/j.matlet.2011.08.079 ↗
19. Du Y, Zheng M, Qiao X, Peng W, Jiang B. Effect of La addition on the microstructure and mechanical properties of Mg–6wt% Zn alloys. Mat Sci Eng A-Struct. 2016;673:47–54.10.1016/j.msea.2016.07.022 ↗
20. Lan A, Huo L. Effect of substitution of minor Nd for Y on mechanical and damping properties of heat-treated Mg–Zn–Y–Zr alloy. Mat Sci Eng A-Struct. 2016;651:646–56.10.1016/j.msea.2015.11.023 ↗
21. Zhao Z, Chen Q, Chao H, Huang S. Microstructural evolution and tensile mechanical properties of thixoforged ZK60-Y magnesium alloys produced by two different routes. Mater Design. 2010;31(4):1906–16.10.1016/j.matdes.2009.10.056 ↗
22. Wang D, Tian Z, Shen L, Liu Z, Huang Y. Influences of laser remelting on microstructure of nanostructured Al2O3–13wt.% TiO2 coatings fabricated by plasma spraying. Appl Surf Sci. 2009;255:4606–10.10.1016/j.apsusc.2008.11.082 ↗
23. Yang Y, Wu P, Lin X, Liu Y, Bian H, Zhou Y, Gao C, Shuai C. System development, formability quality and microstructure evolution of selective laser-melted magnesium. Virtual Phys Prototyp. 2016;11(3):173–81.10.1080/17452759.2016.1210522 ↗
24. Zheng Y, Gu X, Witte F. Biodegradable metals. Mater Sci Eng R. 2014;77(2):1–34.10.1016/j.mser.2014.01.001 ↗
25. Zhou Y, Wu P, Yang Y, Gao D, Feng P, Gao C, Wu H, Liu Y, Bian H, Shuai C. The microstructure, mechanical properties and degradation behavior of laser-melted Mg< img border=. J Alloys Compd. 2016;687:109–14.10.1016/j.jallcom.2016.06.068 ↗
26. Jie Y, Wang J, Wang L, Wu Y, Wang L, Zhang H. Microstructure and mechanical properties of Mg–4.5Zn– x Nd (x = 0, 1 and 2, wt%) alloys. Mater Sci Eng-A Struct. 2008;485(1–2):55–60.
27. Wei L, Dunlop G, Westengen H. The intergranular microstructure of cast Mg-Zn and Mg-Zn-rare earth alloys. Metall Mater Trans. A. 1995;26(8):1947–55.10.1007/BF02670666 ↗
28. Li Q, Wang Q, Li D, Ding W, Li Q, Wang Q, Li D, Ding W. Effect of Nd and Y addition on microstructure and mechanical properties of extruded Mg-Zn-Zr alloy. J Alloys Compd. 2007;427(1–2):115–23.10.1016/j.jallcom.2006.02.054 ↗
29. Fischer J, Prosenc M, Wolff M, Hort N, Willumeit R, Feyerabend F. Interference of magnesium corrosion with tetrazolium-based cytotoxicity assays. Acta Biomater. 2010;6(5):1813–23.10.1016/j.actbio.2009.10.020 ↗
30. Shuai C, Sun H, Wu P, Gao C, Yang Y, Guo W, Yang D, Xu F, Feng P, Peng S. Biosilicate scaffolds for bone regeneration: influence of introducing SrO. RSC Adv. 2017;7:21749–57.10.1039/C7RA01606A ↗
31. Amadeh A, Pahlevani B, Heshmati-Manesh S. Effects of rare earth metal addition on surface morphology and corrosion resistance of hot-dipped zinc coatings. Corros Sci. 2002;44(10):2321–31.10.1016/S0010-938X(02)00043-4 ↗
32. Lothe J, Pound G. Reconsiderations of nucleation theory. J Chem Phys. 1961;36(8):2080–5.10.1063/1.1732832 ↗
33. Strondl A, Fischer R, Frommeyer G, Schneider A. Investigations of MX and γ′/γ″ precipitates in the nickel-based superalloy 718 produced by electron beam melting. Mater Sci Eng-A Struct. 2008;480(1-2):138–47.10.1016/j.msea.2007.07.012 ↗
34. Baril G, Pébère N. The corrosion of pure magnesium in aerated and deaerated sodium sulphate solutions. Corros Sci. 2001;43(3):471–84.10.1016/S0010-938X(00)00095-0 ↗
35. Orlov D, Ralston K, Birbilis N, Estrin Y. Enhanced corrosion resistance of Mg alloy ZK60 after processing by integrated extrusion and equal channel angular pressing. Acta Mater. 2011;59(15):6176–86.10.1016/j.actamat.2011.06.033 ↗
36. Gu X, Zheng Y, Zhong S, Xi T, Wang J, Wang W. Corrosion of, and cellular responses to Mg-Zn-Ca bulk metallic glasses. Biomater. 2010;31(6):1093–103.10.1016/j.biomaterials.2009.11.015 ↗