The enhancement of mechanical properties and uniform degradation of electrodeposited Fe-Zn alloys by multilayered design for biodegradable stent applications
Source abstract
Abstract
Pure Fe is a potential biodegradable stent material due to its better biocompatibility and mechanical properties, but its degradation rate needs to be improved. Alloying with Zn to form Fe-Zn alloy is anticipated to meet the degradation rate requirements while retaining the iron's inherent properties. Therefore, Fe-Zn alloys with monolayered and multilayered structures were prepared by electrodeposition. The alloys' composition, microstructure, mechanical properties, in vitro degradation and biocompatibility were assessed. Results showed that the Zn content ranged from 2.1 wt% to 11.6 wt%. After annealing at 450°C, all the alloys consisted of α(Fe) solid solution and Zn-rich B2 ordered coherent phase, except for the alloy with 11.6 wt% Zn content, in which a Fe3Zn10 phase appeared. The layered structure consisted of alternating columnar-grain and nano-grain layers, which compensated for the intrinsic brittleness of electrodeposited metals and improved the galvanic effect of the alloy, thus increasing the strength and plasticity and changing the corrosion from localized to uniform while augmenting the corrosion rate. The yield strength of the multilayered alloy exceeded 350 MPa, its elongation was more than 20%, and its corrosion rate obtained by immersion test in Hank's solution reached 0.367 mm·y-1. Fe-Zn alloys with lower Zn content had good cytocompatibility with the human umbilical vein endothelial cells and good blood compatibility. The above results verified that the multilayered Fe-Zn alloy prepared by electrodeposition presented enhanced mechanical properties, higher degradation rate, uniform degradation mechanism and good biocompatibility. It should be qualified for the application of biodegradable stents. STATEMENT OF SIGNIFICANCE: A potential biodegradable Fe-Zn alloy, which is difficult to be obtained by the metallurgical method, was prepared by electrodeposition to solve the low degradation rate of iron-based biomaterials. A multilayered microstructure design composed of alternating columnar-grain and nano-grain layers was achieved by changing the electrical parameters. The layered design compensated for the intrinsic poor plasticity of electrodeposited metals. It increased the galvanic effect of the alloy, thus augmenting the corrosion rate and changing the corrosion mode of the alloy from localized to uniform corrosion. The yield strength of multilayered alloy exceeded 350 MPa; its elongation was more than 20%. Moreover, the layered alloy had good cytocompatibility and blood compatibility. It indicates that the alloy is qualified for biodegradable stent application.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Electrodeposition and Electroless Coatings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (79)
Show source-provided references
1. Fundamental theory of biodegradable metals-definition, criteria, and design
2. Biodegradable metals10.1016/j.mser.2014.01.001 ↗
3. Metallic implant biomaterials10.1016/j.mser.2014.10.001 ↗
4. Biodegradable Mg and Mg alloys: corrosion and biocompatibility10.1016/j.mseb.2011.05.028 ↗
5. Magnesium-based bioresorbable stent materials: review of reviews10.1007/s40735-019-0216-x ↗
6. Challenges in the use of zinc and its alloys as biodegradable metals: perspective from biomechanical compatibility10.1016/j.actbio.2019.07.038 ↗
7. The influence of alloying and fabrication techniques on the mechanical properties, biodegradability and biocompatibility of zinc: a comprehensive review10.1016/j.actbio.2019.01.035 ↗
8. Long-term safety and absorption assessment of a novel bioresorbable nitrided iron scaffold in porcine coronary artery
9. On the cytocompatibility of biodegradable Fe-based alloys10.1016/j.msec.2012.11.002 ↗
10. Fe-Mn alloys for metallic biodegradable stents: degradation and cell viability studies10.1016/j.actbio.2009.11.025 ↗
11. Biocompatibility of pure iron: in vitro assessment of degradation kinetics and cytotoxicity on endothelial cells10.1016/j.msec.2008.12.019 ↗
12. Long-term in vivo corrosion behavior, biocompatibility and bioresorption mechanism of a bioresorbable nitrided iron scaffold10.1016/j.actbio.2017.03.020 ↗
13. Development of degradable Fe-35Mn alloy for biomedical application10.4028/www.scientific.net/AMR.15-17.107 ↗
14. Design strategy for biodegradable Fe-based alloys for medical applications10.1016/j.actbio.2009.07.039 ↗
15. Effects of alloying elements (Mn, Co, Al, W, Sn, B, C and on biodegradability and in vitro biocompatibility of pure iron10.1016/j.actbio.2010.11.001 ↗
16. in vitro investigation of Fe30Mn6Si shape memory alloy as potential biodegradable metallic material10.1016/j.matlet.2010.10.068 ↗
17. in vitro degradation and biocompatibility of Fe-Pd and Fe-Pt composites fabricated by spark plasma sintering10.1016/j.msec.2013.10.023 ↗
18. A novel high-strength and highly corrosive biodegradable Fe-Pd alloy: structural, mechanical and in vitro corrosion and cytotoxicity study10.1016/j.msec.2017.05.100 ↗
19. in vitro corrosion properties and cytocompatibility of Fe-Ga alloys as potential biodegradable metallic materials10.1016/j.msec.2016.09.086 ↗
20. Improving the radiopacity of Fe-Mn biodegradable metals by magnetron-sputtered W-Fe-Mn-C coatings: application for thinner stents
21. Cancellous bone-like porous Fe@Zn scaffolds with core-shell-structured skeletons for biodegradable bone implants10.1016/j.actbio.2020.11.032 ↗
22. A study of degradation behaviour and biocompatibility of Zn-Fe alloy prepared by electrodeposition10.1016/j.msec.2020.111295 ↗
23. Fe-Zn (iron-zinc)10.1007/s11669-007-9051-8 ↗
24. Enhancing controlled and uniform degradation of Fe by incorporating Mg and Zn aimed for bio-degradable material applications10.1016/j.matchemphys.2022.126171 ↗
25. Preparation of Fe-Zn alloy biomaterials and its effect on anxiety and depression of patients with coronary disease after treatment10.1166/sam.2021.3920 ↗
26. Electroformed pure iron as a new biomaterial for degradable stents: in vitro degradation and preliminary cell viability studies10.1016/j.actbio.2010.01.008 ↗
27. Microstructure and in vitro biodegradable properties of Fe-Zn alloys prepared by electroforming10.4028/www.scientific.net/AMR.1033-1034.1200 ↗
28. Effects of pulse frequency and current density on microstructure and properties of biodegradable Fe-Zn alloy10.1016/j.jmrt.2022.02.096 ↗
29. Design, influence of layer thickness on mechanical properties of multilayered NiFe samples processed by electrodeposition10.1016/j.matdes.2015.10.137 ↗
30. The mechanical behavior of a layered nanostructured Ni with an alternating growth of ultrafine grains and nano-sized grains fabricated by electrodeposition10.1016/j.msea.2017.11.122 ↗
31. 2012
32. 2017 · 2017
33. B.S. Institution, Biological evaluation of medical devices. Part 5. Tests for in vitro cytotoxicity, EN ISO 10993-12, 2012.
34. in vitro corrosion, cytotoxicity and hemocompatibility of bulk nanocrystalline pure iron10.1088/1748-6041/5/6/065015 ↗
35. Biocorrosion properties and blood and cell compatibility of pure iron as a biodegradable biomaterial10.1007/s10856-010-4070-0 ↗
36. Coherent precipitation and strengthening in compositionally complex alloys: a review10.3390/e20110878 ↗
37. Evolution of metallic cardiovascular stent materials: a comparative study among stainless steel, magnesium and zinc10.1016/j.biomaterials.2019.119641 ↗
38. Thermodynamic evaluation of the Fe-Zn system10.1016/S0925-8388(01)01273-7 ↗
39. Potassium salt based alkaline bath for deposition of Zn-Fe alloys10.1016/j.surfcoat.2006.06.027 ↗
40. Coronary stents: a materials perspective10.1016/j.biomaterials.2006.11.042 ↗
41. Non-destructive corrosion study on a magnesium alloy with mechanical properties tailored for biodegradable cardiovascular stent applications10.1016/j.jmst.2020.07.006 ↗
42. Moving research direction in the field of metallic bioresorbable stents-a mini-review
43. Alloying design of biodegradable zinc as promising bone implants for load-bearing applications10.1038/s41467-019-14153-7 ↗
44. Recent advances on the mechanical behavior of zinc based biodegradable metals focusing on the strain softening phenomenon10.1016/j.actbio.2022.08.041 ↗
45. Mechanical behaviour of nanocrystalline electrodeposited Ni above room temperature10.1016/j.scriptamat.2005.03.026 ↗
46. Influence of bath composition on microstructure and properties of electrodeposited Fe-Zn alloy coating
47. Instabilities and ductility of nanocrystalline and ultrafine-grained metals10.1016/S1359-6462(03)00396-8 ↗
48. High tensile ductility in a nanostructured metal
49. Scaling theory of the Hall-Petch relation for multilayers10.1103/PhysRevLett.81.2715 ↗
50. Nucleation and propagation of dislocations in nanocrystalline fcc metals10.1016/j.actamat.2005.12.026 ↗
51. Suppression of nanocrack generation in nanocrystalline materials under superplastic deformation10.1016/j.actamat.2004.11.026 ↗
52. Mechanistic models for the activation volume and rate sensitivity in metals with nanocrystalline grains and nano-scale twins10.1016/j.actamat.2005.03.047 ↗
53. in vitro degradation and biocompatibility evaluation of typical biodegradable metals (Mg/Zn/Fe) for the application of tracheobronchial stenosis
54. Mechanism for corrosion prevention by a mechanical plating of uniform zinc-iron alloy10.1007/s11665-016-2322-y ↗
55. Mechanism of localized corrosion of iron and stainless-steel. 1. Electrochemical studies10.1149/1.2403982 ↗
56. Understanding localized corrosion10.1016/S1369-7021(08)70206-2 ↗
57. Roberge · 2000
58. The mechanism of pitting of high purity iron in NaCl solutions10.1016/0010-938X(84)90133-1 ↗
59. Localised dissolution kinetics, salt films and pitting potentials10.1016/S0010-938X(97)00049-8 ↗
60. Underscale corrosion behavior of carbon steel in a NaCl solution using a new occluded cavity cell for simulation10.1007/s10800-008-9749-2 ↗
61. Are Fe-based stenting materials biocompatible? A critical review of in vitro and in vivo studies10.3390/jfb11010002 ↗
62. Fenton- and fenton-like AOPs for wastewater treatment: from laboratory-to-plant-scale application10.1080/01496390701290151 ↗
63. Oxidation of tartaric acid in presence of iron10.1039/CT8946500899 ↗
64. Is there any difference in the biological impact of soluble and insoluble degradation products of iron-containing biomaterials?10.1016/j.colsurfb.2017.09.032 ↗
65. Cytotoxicity and its test methodology for a bioabsorbable nitrided iron stent10.1002/jbm.b.33246 ↗
66. Hydroxyl radicals and oxidative stress: the dark side of Fe corrosion10.1016/j.colsurfb.2019.110542 ↗
67. Zinc deficiency-induced cell death10.1080/15216540500264554 ↗
68. Advances in metal-induced oxidative stress and human disease10.1016/j.tox.2011.03.001 ↗
69. Chou · 2005
70. Recommendation for modifying current cytotoxicity testing standards for biodegradable magnesium-based materials10.1016/j.actbio.2015.04.011 ↗
71. in vitro cytotoxicity, adhesion, and proliferation of human vascular cells exposed to zinc10.1021/acsbiomaterials.6b00035 ↗
72. ASTM · 2013
73. Biocompatibility and hemocompatibility of surface-modified NiTi alloys10.1002/jbm.a.10549 ↗
74. Nutritional zinc increases platelet reactivity10.1002/ajh.2830380302 ↗
75. Role of zinc in hemostasis: a review10.1007/s12011-007-8038-y ↗
76. Iron, platelet function, and coronary heart disease: a possible link?10.1161/01.CIR.88.2.805 ↗
77. Iron-dependent human platelet activation and hydroxyl radical formation involvement of protein kinase C10.1161/01.CIR.99.24.3118 ↗
78. 20 - Absorbable metals for cardiovascular applications
79. Characterization and in vivo evaluation of a bio-corrodible nitrided iron stent10.1007/s10856-012-4823-z ↗