Improved performance of Bis-GMA dental composites reinforced with surface-modified PAN nanofibers
Source abstract
Abstract
Abstract In the present work, polyacrylonitrile (PAN) nanofibers reinforced dental composites were investigated to achieve the improved interfacial adhesion between the PAN nanofiber and resin matrix using surface modification of nanofibers. PAN nanofibers mat were prepared by electrospinning and then, surface treated with the activated bisphenol A glycidyl methacrylate (Bis-GMA)/triethyleneglycol dimethacrylate (TEGDMA) (50/50 mass ratio) dental resin followed by photo-curing. Also, the treated nanofibers mat was milled into a powder to achieve the uniform distribution of nanofibers in the matrix resin. The reinforced dental composite were prepared by mixing the various mass fraction of the powder (0.5–15 wt%) with the Bis-GMA/TEGDMA dental monomers. The effect of weight ratio of surface-modified nanofibers to blend resin on the chemical structure, morphology, compression and flexural properties, color and polymerization shrinkage of dental composites was evaluated. The results showed that using surface-treated nanofibers with content of 5 wt% enhanced the compression strength, flexural strength, flexural modulus and work of rupture of the resultant dental composite by factors of 23%, 7%, 80%, and 145%, respectively, comparing to the unreinforced neat resin. Also, the polymerization shrinkage reduces by 37%. These significant improved properties of the dental composite could be due to the semi-interpenetration network formation between surface-modified nanofibers and resin matrix and well distribution of nanofibers in the dental resin. Further increasing the nanofiber content led to poor mechanical properties of obtained dental composites. The results also, revealed that the color of resin composite could be whiter using modified PAN nanofibers as the filler.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Bone Tissue Engineering Materials · Electrospun Nanofibers in Biomedical Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Gopikrishna V. Sturdevant’s art and science of operative dentistry. 1th ed. India: Elsevier; 2013.
2. Sachdeva S, Kapoor P, Tamrakar AK, Noor R. Nano-composite dental resins: an overview. Ann Dent Specialty. 2015;3:52–55.
3. Sakaguchi LR, Powers JM. Craig’s restorative dental materials. 13th ed. Elsevier Health Sciences; 2012.
4. Samuel SP, Li S, Mukherjee I, Guo Y, Patel AC, Baran G, et al. Mechanical properties of experimental dental composites containing a combination of mesoporous and nonporous spherical silica as fillers. Dent Mater. 2009;25:296–301.10.1016/j.dental.2008.07.012 ↗
5. Tian M, Gao Y, Liu Y, Liao YL, Hedin NE, Fong H. Fabrication and evaluation of BIS-GMA/TEGDMA dental resins/composites containing nano fibrillar silicate. Dent Mater. 2008;24:235–43.10.1016/j.dental.2007.05.002 ↗
6. Chen CY, Huang CK, Lin SP, Han JL, Hsieh KH, Lin CP. Low-shrinkage visible-light-curable urethane-modified epoxy acrylate/SiO2 composites as dental restorative materials. J Compos Sci Technol. 2008;68:2811–7.10.1016/j.compscitech.2008.06.015 ↗
7. Ilie N, Hilton TJ, Heintze SD, Hickel R, Watts DC, Silikas N, et al. Academy of Dental Materials guidance—resin composites: Part I—Mechanical properties. Dent Mater. 2017;33:880–94.10.1016/j.dental.2017.04.013 ↗
8. Tinschert J, Zwez D, Marx R, Anusavice KJ. Structural reliability of alumina-, feldspar-, leucite-, mica- andzirconia-based ceramics. J Dent. 2000;28:529–35.10.1016/S0300-5712(00)00030-0 ↗
9. Yamaguchi S, Inoue S, Sakai T, Abe T, Kitagawa H, Satoshi I. Multi-scale analysis of the effect of nano-filler particle diameter on the physical properties of CAD/CAM composite resin blocks. Comput Methods Biomech Biomed Eng. 2017;20:714–9.10.1080/10255842.2017.1293664 ↗
10. Randolph LD, Palin WM, Leloup G, Leprince JG. Filler characteristics of modern dental resin composites and their influence on physico-mechanical properties. Dent Mater. 2016;32:1586–99.10.1016/j.dental.2016.09.034 ↗
11. Zandinejad AA, Atai M, Pahlevan A. The effect of ceramic and porous fillers on the mechanical properties of experimental dental composites. Dent Mater. 2006;22:382–7.10.1016/j.dental.2005.04.027 ↗
12. Willems G, Lambrechts P, Braem M, Celis JP, Vanherle G. A classification of dental composites according to their morphological and mechanical characteristics. Dent Mater. 1992;8:310–9.10.1016/0109-5641(92)90106-M ↗
13. Lassilaa L, Garoushia S, Vallittua PK, Sailynoja E. Mechanical properties of fiber-reinforced restorat composite with two distinguished fiber length distribution. J Mech Behav Biomed Mater. 2016;60:331–8.10.1016/j.jmbbm.2016.01.036 ↗
14. Debnath S, Wunder SL, McCool JI, Baran GR. Silane treatment effects on glass/ resin interfacial shear strengths. Dent Mater. 2003;19:441–8.10.1016/S0109-5641(02)00089-1 ↗
15. Garoushi S, Vallittu PK, Lassila LVJ. Short glass fiber reinforced restorative composite resin with semi-inter penetrating polymer network matrix. Dent Mater. 2007;23:1356–62.10.1016/j.dental.2006.11.017 ↗
16. Lung CYK, Matinlinna JP. Aspects of silane coupling agents and surface conditioning in dentistry: an overview. Dent Mater. 2012;28:467–77.10.1016/j.dental.2012.02.009 ↗
17. Li X, Liu W, Sun L, Aifantis KE, Yu B, Fan Y, et al. Resin composites reinforced by nanoscaled fibers or tubes for dental regeneration. Biomed Res Int. 2014;2014; https://doi.org/10.1155/2014/542958.10.1155/2014/542958 ↗
18. Lin S, Cai Q, Ji J, Sui G, Yu Y, Yang X, et al. Electrospun nanofiber reinforced and toughened composites through in situ nano-interface formation. Compos Sci Technol. 2008;68:3322–32.10.1016/j.compscitech.2008.08.033 ↗
19. Liu F, Wang R, Cheng Y, Jiang X, Zhang Q, Zhu M. Polymer grafted hydroxyapatite whisker as a filler for dental composite resin with enhanced physical and mechanical properties. Mater Sci Eng. 2013;33:4994–5000.10.1016/j.msec.2013.08.029 ↗
20. Liu F, Jiang X, Zhang Q, Zhu M. Strong and bioactive dental resin composite containing poly(Bis-GMA) grafted hydroxyapatite whiskers and silica nanoparticles. Compos Sci Technol. 2014;101:86–93.10.1016/j.compscitech.2014.07.001 ↗
21. Foroutan F, Javadpour J, khavandi A, Atai M, Rezaie HR. Mechanical properties of dental composite materials reinforced with micro and nano-size Al2O3 filler particles. Mater Sci Eng. 2011;8:25–33.
22. Bahramian N, Atai M, Naimi-Jamal MR. Ultra-high-molecular-weight polyethylene fiber reinforced dental composites: Effect of fiber surface treatment on mechanical properties of the composites. Dent Mater. 2015;31:1022–9.10.1016/j.dental.2015.05.011 ↗
23. Yi M, Sun H, Zhang H, Deng X, Cai Q, Yang X. Flexible fiber-reinforced composites with improved interfacial adhesion by mussel-inspired polydopamine and poly(methyl methacrylate) coating. Mater Sci Eng. 2016;58:742–9.10.1016/j.msec.2015.09.026 ↗
24. Fong H. Electrospun nylon 6 nanofiber reinforced BIS GMA/TEGDMA dental restorative composite resins. Polym. 2004;45:2427–32.10.1016/j.polymer.2004.01.067 ↗
25. Gao Y, Sagi S, Zhang L, Liao Y, Cowles DM, Sun Y, et al. Electrospun nano-scaled glass fiber reinforcement of Bis-GMA/TEGDMA dental composites. J Appl Polym Sci. 2008;110:2063–70.10.1002/app.28695 ↗
26. Sun W, Cai Q, Li P, Deng X, Wei Y, Xu M, et al. Post-draw PAN–PMMA nanofiber reinforced and toughened Bis-GMA dental restorative composite. Dent Mater. 2010;26:873–80.10.1016/j.dental.2010.03.022 ↗
27. Tian M, Gao Y, Liu Y, Liao Y, Xu R, Hedin NE, et al. Bis-GMA/TEGDMA dental composites reinforced with electro spun nylon 6 nanocomposite nanofibers containing highly aligned fibrillar silicate single crystals. Polym. 2007;48:2720–8.10.1016/j.polymer.2007.03.032 ↗
28. Vidotti HA, Manso AP, Leung V, Valle ALD, Ko F, Carvalho RM. Flexural properties of experimental nanofiber reinforced composite are affected by resin composition and nanofiber/resin ratio. Dent Mater. 2015;31:1132–41.10.1016/j.dental.2015.06.018 ↗
29. Aghazadeh Mohandesi J, Rafiee MA, Barzegarani V, SHafiei F. Compressive fatigue behavior of dental restorative composites. Dent Mater. 2007;26:827–37.10.4012/dmj.26.827 ↗
30. Cheng L, Zhou X, Zhong H, Deng X, Cai Q, Yang X. NaF-loaded core–shell PAN–PMMA nanofibers as reinforcements for Bis-GMA/TEGDMA restorative resins. Mater Sci Eng. 2014;34:262–9.10.1016/j.msec.2013.09.020 ↗
31. Visvanathan A, Ilie N, Hickel R, Kunzelmann K. The influence of curing times and light curing methods on the polymerization shrinkage stress of a shrinkage-optimized composite with hybrid-type prepolymer fillers. Dent Mater. 2007;23:777–84.10.1016/j.dental.2006.06.019 ↗
32. Kleverlaan CJ, Feilzer AJ. Polymerization shrinkage and contraction stress of dental resin composites. Dent Mater. 2005;21:1150–7.10.1016/j.dental.2005.02.004 ↗