journal article·2021-12Open access

Investigation on tribological behaviors of biodegradable pure Zn and Zn-X (Li, Cu, Ge) binary alloys

Huafang Li, Jinyan Huang, Peng Zhang, Qi Zhang

Abstract

Abstract As a potential biodegradable implant material, zinc (Zn) alloys have attracted increasing attention due to their good biocompatibility and moderate degradation rate. Zn and its alloys are expected to become candidate materials for medical devices. The metals implanted in the human body will inevitably undergo friction in the human body before it is completely degraded. Friction and wear are essential factors which may cause medical devices’ service failure. However, there are still few studies on the friction and wear properties of biodegradable Zn-based alloys in the human body, and most studies just focus on the mechanical properties, degradation properties and biocompatibility of the alloys. Thus, it is crucial to study the friction and wear properties of Zn and its alloys. In the present work, we investigated the tribological properties of biodegradable pure Zn and Zn-X (Li, Cu, Ge) alloys. Our study found that under simulated body fluid and dry friction conditions, the addition of alloying elements Li and Cu can improve the friction properties of Zn. Among the four metals, Zn-0.5Li alloy has the lowest friction coefficient and the best wear resistance. Hank’s solution has lubricating and corrosive effects. That is to say, when the alloy is rubbed in Hank’s solution, it can not only be protected by the lubrication of the solution, but also tribocorrosion will occur as well.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Orthopaedic implants and arthroplasty · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Zheng YF, Gu XN, Witte F. Biodegradable metals. Mater Sci Eng R Rep. 2014;77:1–34.10.1016/j.mser.2014.01.001 ↗
2. Zhu Z-Y, Meng L, Chen L. Strain-induced martensitic transformation in biomedical Co–Cr–W–Ni alloys. Rare Met. 2020;39:241–9.10.1007/s12598-019-01364-6 ↗
3. Chen Q, Thouas GA. Metallic implant biomaterials. Mater Sci Eng R Rep. 2015;87:1–57.10.1016/j.mser.2014.10.001 ↗
4. Chen Y, Xu Z, Smith C, Sankar J. Recent advances on the development of magnesium alloys for biodegradable implants. Acta Biomater. 2014;10:4561–73.10.1016/j.actbio.2014.07.005 ↗
5. Su Y, Yang H, Gao J, Qin Y-X, Zheng Y, Zhu D. Interfacial Zinc Phosphate is the key to controlling biocompatibility of metallic Zinc implants. Adv Sci. 2019;6:1900112.10.1002/advs.201900112 ↗
6. Heublein B, Rohde R, Kaese V, Niemeyer M, Hartung W, Haverich A. Biocorrosion of magnesium alloys: a new principle in cardiovascular implant technology? Heart. 2003;89:651–6.10.1136/heart.89.6.651 ↗
7. Zhao N, Zhu D. Application of Mg—Based alloys for cardiovascular stents. Int J Biomed Eng Technol. 2013;12:382–98.10.1504/IJBET.2013.057677 ↗
8. Zhao N, Zhu D. Endothelial responses of magnesium and other alloying elements in magnesium-based stent materials. Metallomics. 2015;7:118–28.10.1039/C4MT00244J ↗
9. Ma J, Zhao N, Betts L, Zhu D. Bio-Adaption between magnesium alloy stent and the blood vessel: a review. J Mater Sci Technol. 2016;32:815–26.10.1016/j.jmst.2015.12.018 ↗
10. Zhu D, Cockerill I, Su Y, Zhang Z, Fu J, Lee KW. et al. Mechanical strength, biodegradation, and in vitro and in vivo biocompatibility of Zn biomaterials. ACS Appl Mater Interfaces. 2019;11:6809–19.10.1021/acsami.8b20634 ↗
11. Bowen P, Drelich J, Goldman J. Zinc exhibits ideal physiological corrosion behavior for bioabsorbable stents. Adv Mater. 2013;25:2577–82.10.1002/adma.201300226 ↗
12. Liu X, Sun J, Yang Y, Pu Z, Zheng Y. In vitro investigation of ultra-pure Zn and its mini-tube as potential bioabsorbable stent material. Mater Lett. 2015;161:53–6.10.1016/j.matlet.2015.06.107 ↗
13. Werkhoven RJ, Sillekens WH, van Lieshout JBJM. Processing aspects of magnesium alloy stent tube, In: WH Sillekens, SR Agnew, NR Neelameggham, SN Mathaudhu (Eds.), Magnesium Technology 2011, Springer International Publishing, Cham, 2016, pp. 419–24.10.1002/9781118062029.ch79 ↗
14. Zhao S, Seitz J-M, Eifler R, Maier HJ, Guillory RJ, Earley EJ. et al. Zn-Li alloy after extrusion and drawing: structural, mechanical characterization, and biodegradation in abdominal aorta of rat. Mater Sci Eng C. 2017;76:301–12.10.1016/j.msec.2017.02.167 ↗
15. Vojtěch D, Kubásek J, Šerák J, Novák P. Mechanical and corrosion properties of newly developed biodegradable Zn-based alloys for bone fixation. Acta Biomater. 2011;7:3515–22.10.1016/j.actbio.2011.05.008 ↗
16. Li H, Yang H, Zheng Y, Zhou F, Qiu K, Wang X. Design and characterizations of novel biodegradable ternary Zn-based alloys with IIA nutrient alloying elements Mg, Ca and Sr. Mater Des. 2015;83:95–102.10.1016/j.matdes.2015.05.089 ↗
17. Tong X, Zhang D, Zhang X, Su Y, Shi Z, Wang K. et al. Microstructure, mechanical properties, biocompatibility, and in vitro corrosion and degradation behavior of a new Zn–5Ge alloy for biodegradable implant materials. Acta Biomater. 2018;82:197–204.10.1016/j.actbio.2018.10.015 ↗
18. Niu J, Tang Z, Huang H, Pei J, Zhang H, Yuan G. et al. Research on a Zn-Cu alloy as a biodegradable material for potential vascular stents application. Mater Sci Eng C. 2016;69:407–13.10.1016/j.msec.2016.06.082 ↗
19. Liu D-B, Wu B, Wang X, Chen M-F. Corrosion and wear behavior of an Mg–2Zn–0.2Mn alloy in simulated body fluid. Rare Met. 2015;34:553–9.10.1007/s12598-013-0052-y ↗
20. Li H-F, Huang J-Y, Lin G-C, Wang P-Y. Recent advances in tribological and wear properties of biomedical metallic materials. Rare Met. 2021;40:3091–106.10.1007/s12598-021-01796-z ↗
21. Kunčická L, Kocich R, Lowe TC. Advances in metals and alloys for joint replacement. Prog Mater Sci. 2017;88:232–80.10.1016/j.pmatsci.2017.04.002 ↗
22. Hussein MA, Mohammed AS, Al-Aqeeli N. Wear characteristics of metallic biomaterials: a review. Materials. 2015;8:2749–68.10.3390/ma8052749 ↗
23. Xu W, Chen M, Lu X, Zhang D-W, Singh H-P, Jian-shu Y. et al. Effects of Mo content on corrosion and tribocorrosion behaviours of Ti-Mo orthopaedic alloys fabricated by powder metallurgy. Corros Sci. 2020;168:10855710.1016/j.corsci.2020.108557 ↗
24. Holt G, Murnaghan C, Reilly J, Meek D. The biology of aseptic osteolysis. Clin Orthop Relat Res. 2007;460:240–52.10.1097/BLO.0b013e31804b4147 ↗
25. Masui T, Sakano S, Hasegawa Y, Warashina H, Ishiguro N. Expression of inflammatory cytokines, RANKL and OPG induced by titanium, cobalt-chromium and polyethylene particles. Biomaterials. 2005;26:1695–702.10.1016/j.biomaterials.2004.05.017 ↗
26. Guo L, Qin L, Kong F, Yi H, Tang B. Improving tribological properties of Ti-5Zr-3Sn-5Mo-15Nb alloy by double glow plasma surface alloying. Appl Surf Sci. 2016;388:203–11.10.1016/j.apsusc.2016.01.201 ↗
27. Wang ZG, Li Y, Huang WJ, Chen XL, He HR. Micro-abrasion-corrosion behaviour of a biomedical Ti-25Nb-3Mo-3Zr-2Sn alloy in simulated physiological fluid. J Mech Behav Biomed Mater. 2016;63:361–74.10.1016/j.jmbbm.2016.07.010 ↗
28. Xu W, Yu A, Lu X, Tamaddon M, Ng L, Hayat MD. et al. Synergistic interactions between wear and corrosion of Ti-16Mo orthopedic alloy. J Mater Res Technol. 2020;9:9996–10003.10.1016/j.jmrt.2020.06.095 ↗
29. Yang X, Hutchinson CR. Corrosion-wear of beta-Ti alloy TMZF (Ti-12Mo-6Zr-2Fe) in simulated body fluid. Acta Biomater. 2016;42:429–39.10.1016/j.actbio.2016.07.008 ↗
30. Wang ZG, Zhou YT, Wang HN, Li Y, Huang WJ. Tribocorrosion behavior of Ti-30Zr alloy for dental implants. Mater Lett. 2018;218:190–2.10.1016/j.matlet.2018.02.008 ↗
31. Yoneyama C, Cao S, Igual Munoz A, Mischler S. Influence of Bovine Serum Albumin (BSA) on the tribocorrosion behaviour of a low carbon CoCrMo alloy in simulated body fluids. Lubricants. 2020;8:61.10.3390/lubricants8050061 ↗
32. Luo W, Kuai J. Friction and wear properties of artificial joints of CoCrMo alloy. IOP Conf Ser: Mater Sci Eng. 2018;439:042072.10.1088/1757-899X/439/4/042072 ↗
33. Fellah M, Labaïz M, Assala O, Iost A, Dekhil L. Tribological behaviour of AISI 316L stainless steel for biomedical applications. Tribol Mater Surf Interfaces. 2013;7:135–49.10.1179/1751584X13Y.0000000032 ↗
34. Wu S, Liu X, Yeung KWK, Xu ZS, Chung CY, Chu PK. Wear properties of porous NiTi orthopedic shape memory alloy. J Mater Eng Perform. 2012;21:2622–7.10.1007/s11665-012-0392-z ↗
35. ISO 8407:2021, Corrosion of metals and alloys-removal of corrosions products from corrosion test specimens, International Organization of Standardization, Geneva, Switzerland, 2021.
36. Olesinski RW, Abbaschian GJ. The Ge-Zn (Germanium-Zinc) system. Bull Alloy Phase Diagr. 1985;6:540–3.10.1007/BF02887154 ↗
37. Pelton AD. The Li-Zn (Lithium-Zinc) System. J Phase Equilibria. 1991;12:42–5.10.1007/BF02663672 ↗
38. Ma D, Li Y, Ng SC, Jones H. Unidirectional solidification of Zn-rich Zn–Cu peritectic alloys—I. Microstructure selection. Acta Mater. 2000;48:419–31.10.1016/S1359-6454(99)00365-1 ↗