On the surface elemental composition of non-corroded and corroded dental ceramic materials in vitro

P. Milleding, S. Karlsson, L. Nyborg

Publisher page

Abstract

Dental ceramics are traditionally looked upon as inert materials. As many are glass phased, it may be hypothesized that they will be subjected to glass corrosion in aqueous environments. The aim of the study was therefore to analyze the surface elemental composition of glass-phased and all-crystalline ceramics, before and after low- and high-intensity, in vitro corrosion (milli-Q-water at 37+/-2 degrees C for 18 h and 4% acetic acid at 80+/-2 degrees C for 18 h, respectively). The analysis of the surface elemental composition was performed using ESCA. The hypothesis was confirmed. After high-intensity corrosion, the complete wash out of alkali ions, alkaline-earth ions and elemental alumina was found, leaving behind a surface totally dominated by silica. The all-crystalline ceramics, densely sintered alumina and yttria-partially stabilized tetragonal zirconia, displayed only minor surface changes, even after high-intensity corrosion. In comparison to the corrosion testing in acid, the corrosion process in milli-Q-water did not produce different results in principle, except for the lower magnitude of the depletion of alkali ions and the virtually unchanged level of elemental alumina. Unexpectedly, no substantial difference in surface degradation was found between the glass ceramic and the ordinary porcelain-fused-to-metal ceramic or between ceramics of higher sintering temperature and those of low or ultra-low sintering temperature. The composition and microstructure alone did not appear to provide a full explanation for the inter-individual differences in surface corrosion when exposed to comparable environmental conditions.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Radiography and Imaging

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. W. D. Kingery, in “Introduction to Ceramics” (John Wiley & Sons Inc., New York, 1965).
2. M. M. Barreiro, O. Riesgo and E. E. Vicente, Dent. Mater. 5 (1989) 51.10.1016/0109-5641(89)90094-8 ↗
3. W. Baumann, “Med Diss. Verblendmetallkeramik für Titan ‐Haftefestigkeit und Aufbrenntemperatur” (Aachen, Germany, 1992).
4. M. Schmid, J. Fischer, M. Salk and J. Strub, Schweiz Monatsschr. Zahnmed. 102 (1992) 1046.
5. R. Schäfer and H. F. Kappert, Zahnärztl Z. 48 (1993) 626.
6. J. Tinschert, R. Marx and R. Gussone, Dtsch. Zahnärztl Z. 50 (1995) 31.
7. K. J. Anusavice, Adv. Dent. Res. 6 (1992) 82.10.1177/08959374920060012201 ↗
8. W. Hohmann, in “Dentalkeramik auf der Basis hydrothermaler Gläser” (Quintessenz Verlag GmbH, Berlin, 1993).
9. K. J. Anusavice, K.-J. Söderholm and D. G. Grossman, MRS Bull. (1993) 64.10.1557/S0883769400038069 ↗
10. R. Carlsson, Durability of Building Mater. 5 (1988) 421.
11. A. Paul and M. S. Zaman, J. Mater. Sci. 13 (1978) 1399.
12. P. Milleding, A. Wennerberg, S. Alaeddin, S. Karlsson and E. Simon, Biomaterials 20 (1999) 733.10.1016/S0142-9612(98)00223-3 ↗
13. B. Kasemo and J. Lausmaa, Int. J. Oral. Maxillofac. Impl. 3 (1988) 247.
14. R. L. Williams and D. F. William, Biomaterials 9 (1988) 206.10.1016/0142-9612(88)90085-3 ↗
15. L. Räisänen, M. Könönen, J. Juhanoja, P. Varpavaara, J. Hautaniemi, J. Kivilahti and M. Hormia, J. Biomed. Mater. Res. 49 (2000) 79.10.1002/(SICI)1097-4636(200001)49:1<79::AID-JBM10>3.0.CO;2-N ↗
16. P. Thomsen, C. Larsson, L. E. Ericsson, L. Sennerby, J. Lausmaa and B. Kasemo, J. Mater. Sci. Mater. Med. 8 (1997) 653.10.1023/A:1018579605426 ↗
17. I. Abrahamsson, T. Berglundh, P.-O. Glantz and J. Lindhe, J. Clin. Periodontol. 25 (1998) 721.10.1111/j.1600-051X.1998.tb02513.x ↗
18. A. Krajewski, R. Malavolti and A. Piancastelli, Biomaterials 17 (1996) 53.10.1016/0142-9612(96)80755-1 ↗
19. Y. Takami, S. Yamane, K. Makinouchi, G. Otsuka, J. Glueck and R. Benkowski, J. Biomed. Mater. Res. 40 (1998) 24.10.1002/(SICI)1097-4636(199804)40:1<24::AID-JBM3>3.0.CO;2-T ↗
20. ISO 6872, “International Standards for Dental Ceramics” (Geneva, Switzerland, 1995).
21. W. G. DeRijk, K. A. Jennings, D. L. Menis, in “Proceedings Biomedical Engineering Conference”, edited by B. W. Sauer (Biomedical engineering ‐recent development. New York, Pergamon, 1985) p. 152.
22. ESCA HANDBOOK, Perkin Elmer.
23. B. Kasemo and J. Gold, Adv. Dent. Res. 13 (1999) 8.10.1177/08959374990130011901 ↗
24. J. Lausmaa, B. Kasemo, U. Rolander, L. M. Bjursten, L. E. Ericsson, L. Rosander and P. Thomsen, in “Surface Characterization of Biomaterials” edited by B. D. Ratner (Elsevier Science, The Netherlands, 1988) p. 161.
25. J. F. Schairer and N. L. Bowen, Am. J. Sci. 253 (1955) 681.10.2475/ajs.253.12.681 ↗
26. E. M. Levin, C. R. Robbins and H. F. Murdie, in “Phase Diagrams for Ceramists, vol. 1” (The American Ceramic Society, Columbus, OH, 1964).
27. L. Holland, in “The Properties of Glass Surfaces” (Chapman and Hall, London, 1964).
28. W. J. McCracken, in “Corrosion of Glass, Ceramics and Superconductors” (Noyes Publication, New Jersey, USA, 1992) p. 432.
29. R. G. Newton, Glass Technol. 26 (1985) 21.
30. W. B. White, in “Corrosion of Glass, Ceramics and Superconductors” (Noyes Publication, New Jersey, USA, 1992) p. 2.
31. L. L. Hench, in “Proceedings XI Int. Congr. Glass, Prague, July 1977” (Survey Papers, vol. II, 1977) p. 343.10.1016/0022-3093(77)90098-9 ↗
32. L. L. Hench and D. E. Clark, J. Non-Cryst. Solids 28 (1978) 83.10.1016/0022-3093(78)90077-7 ↗
33. G. A. Parks, Chem. Rev. 65 (1965) 171.10.1021/cr60234a002 ↗
34. D. J. O'Connor, P. G. Johansen and A. S. Buchanan, Trans. Farad. Soc. 52 (1956) 229.10.1039/tf9565200229 ↗
35. K. Oda and T. Yoshio, J. Amer. Ceram. Soc. 80 (1997) 3233.10.1111/j.1151-2916.1997.tb03258.x ↗
36. R. Carlsson and S. Karlsson, SKBF Technical Report 80-15, Swedish Corrosion Institute (1980).
37. McD. Robinson, J. A. Pask and D. W. Fuerstenau, J. Amer. Ceram. Soc. 10 (1964) 516.10.1111/j.1151-2916.1964.tb13801.x ↗
38. R. A. Eppler, in “Corrosion of Glass, Ceramics and Superconductors” (Noyes Publication, New Jersey, USA, 1992) p. 372.
39. C. Piconi and G. Maccauro, Biomaterials 20 (1999) 1.10.1016/S0142-9612(98)00010-6 ↗
40. M. Röhle, N. Claussen and A. H. Heuer, in “Proceedings of the Second International Conference on the Science and Technology of Zirconia, Stuttgart, June 1983” (Advances in Ceramics, vol. 12, The American Ceramic Society, USA, 1984) p. 352.
41. K. O. Axelsson, in “Dissertation: Influence of Reactive Gases on the Chemical Composition and Structure of ZrO2” (Chalmers University of Technology, Göteborg, Sweden, 1985) p. 52.
42. F. F. Lange, G. L. Dunlop and B. I. Davis, J. Amer. Ceram. Soc. 69 (1986) 237.10.1111/j.1151-2916.1986.tb07415.x ↗
43. J. Li, Y. Liu, L. Hermansson and R. Söremark, Clin. Mater. 12 (1993) 197.10.1016/0267-6605(93)90073-G ↗
44. J. Chevalier, J. M. Drouin and B. Calès, in “Proceedings of the 10th International Symposium on Ceramics in Medicine, Paris, October 1997” (Prozyr Bioceramic Expertise Publications, 1998) p. 9.
45. T. T. Lepistö and T. A. Mäntylä, Ceram. Eng. Sci. Proc. 10 (1986) 658.10.1002/9780470310557.ch13 ↗
46. M. Yoshimura, T. Noma, K. Kawabata and S. Somiya, J. Mater. Sci. Lett. 6 (1987) 465.10.1007/BF01756800 ↗
47. S. Mattsson and A. J. Pugh, Soil Sci. 38 (1934) 229.
48. R. Moreno, J. S. Moya and J. Requena, Bol. Soc. Esp. Ceram. Vidr. 26 (1987) 335.
49. A. Paul, J. Mater. Sci. 12 (1977) 2246.10.1007/BF00552247 ↗
50. B. Calès, in “Proceedings of the 6th Biomaterial Symposium, Göttingen, 1994” (Prozyr Bioceramic Expertise Publications, 1998) p. 2.
51. T. T. Lepistö and T. A. Mäntylä, in “Corrosion of Glass, Ceramics and Superconductors” (Noyes Publication, New Jersey, USA, 1992) p. 492.