Osteoconduction of porous Ti metal enhanced by acid and heat treatments
Source abstract
Abstract
Bone ingrowth into porous Ti metal is important for stable fixation of Ti metal implants to surrounding bone. However, without surface treatment this is limited to only a thin region of the outer surface of the Ti metal. In the present study, a porous Ti metal with a porosity of ~60 % and interpore connections of 70-200 micrometers in diameter was investigated in terms of its chemical and heat treatments, by implanting it into rabbit femur for periods varying from 3 to 12 weeks. The porous Ti metal subjected to heat treatment at 600 °C after H2SO4/HCl mixed acid treatment showed the largest bone ingrowth in comparison with those subjected to no treatment, only acid treatment, and only heat treatment even at an early stage after implantation, and remained as such even 12 weeks after implantation. Their bone ingrowths were well interpreted in terms of apatite-forming abilities of the Ti metals in body environment. Their apatite-forming abilities did not depend upon their surface roughness nor type of crystalline phase, but upon the positive surface charge.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Titanium Alloys Microstructure and Properties · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Kon M, Hirakata LM, Asaoka K. Porous Ti-6Al-4 V alloy fabricated by spark plasma sintering for biomimetic surface modification. J Biomed Mater Res B. 2004;68:88.10.1002/jbm.b.20004 ↗
2. Thelen S, Barthelat F, Brinson LC. Mechanics considerations for microporous titanium as an orthopedic implant material. J Biomed Mater Res A. 2004;69:601.10.1002/jbm.a.20100 ↗
3. Assad M, Jarzem P, Leroux MA, Coillard C, Chernyshov AV, Charette S, Rivard CH. Porous titanium-nickel for intervertebral fusion in a sheep model: part 1. Histomorphometric and radiological analysis. J Biomed Mater Res B. 2003;64:107.10.1002/jbm.b.10530 ↗
4. Wen CE, Yamada Y, Shimojima K, Chino Y, Asahina T, Mabuchi M. Processing and mechanical properties of autogenous titanium implant materials. J Mater Sci Mater Med. 2002;13:397.10.1023/A:1014344819558 ↗
5. Zardiackas LD, Parsell DE, Dillon LD, Mitchell DW, Nunnery LA, Poggie R. Structure, metallurgy, and mechanical properties of a porous tantalum foam. J Biomed Mater Res. 2001;58:180.10.1002/1097-4636(2001)58:2<180::AID-JBM1005>3.0.CO;2-5 ↗
6. Pattanayak DK, Matsushita T, Doi K, Takadama H, Nakamura T, Kokubo T. Effects of oxygen content of porous titanium metal on its apatite-forming ability and compressive strength. Mater Sci Eng C. 2009;29:1974.10.1016/j.msec.2009.03.014 ↗
7. Pattanayak DK, Fukuda A, Matsushita T, Takemoto M, Fujibayashi S, Sasaki K, Nishida N, Nakamura T, Kokubo T. Bioactive Ti metal analogous to human cancellous bone: fabrication by selective laser melting and chemical treatments. Acta Biomater. 2010;7:1398–406. England: 2010 Acta Materialia Inc. published by Elsevier Ltd.10.1016/j.actbio.2010.09.034 ↗
8. Takemoto M, Fujibayashi S, Neo M, So K, Akiyama N, Matsushita T, Kokubo T, Nakamura T. A porous bioactive titanium implant for spinal interbody fusion: an experimental study using a canine model. J Neurosurg Spine. 2007;7:435.10.3171/SPI-07/10/435 ↗
9. Takemoto M, Fujibayashi S, Neo M, Suzuki J, Kokubo T, Nakamura T. Mechanical properties and osteoconductivity of porous bioactive titanium. Biomaterials. 2005;26:6014.10.1016/j.biomaterials.2005.03.019 ↗
10. Aparicio C, Rodriguez D, Gil FJ. Variation of roughness and adhesion strength of deposited apatite layers on titanium dental implants. Mater Sci Eng C. 2011;31:320.10.1016/j.msec.2010.09.018 ↗
11. Takemoto M, Fujibayashi S, Neo M, Suzuki J, Matsushita T, Kokubo T, Nakamura T. Osteoinductive porous titanium implants: effect of sodium removal by dilute HCl treatmen. Biomaterials. 2006;27:2682–91. England.10.1016/j.biomaterials.2005.12.014 ↗
12. Fujibayashi S, Takemoto M, Neo M, Matsushita T, Kokubo T, Doi K, Ito T, Shimizu A, Nakamura T. A novel synthetic material for spinal fusion: a prospective clinical trial of porous bioactive titanium metal for lumbar interbody fusion. Eur Spine J. 2011;20:1486.10.1007/s00586-011-1728-3 ↗
13. Kokubo T, Pattanayak DK, Yamaguchi S, Takadama H, Matsushita T, Kawai T, Takemoto M, Fujibayashi S, Nakamura T. Positively charged bioactive Ti metal prepared by simple chemical and heat treatments. J R Soc Interface. 2010;7(Suppl 5):S503.10.1098/rsif.2010.0129.focus ↗
14. Pattanayak DK, Yamaguchi S, Matsushita T, Nakamura T, Kokubo T. Apatite-forming ability of titanium in terms of pH of the exposed solution. J R Soc Interface. 2012;9:2145.10.1098/rsif.2012.0107 ↗
15. Pattanayak DK, Kawai T, Matsushita T, Takadama H, Nakamura T, Kokubo T. Effect of HCl concentrations on apatite-forming ability of NaOH–HCl- and heat-treated titanium metal. J Mater Sci Mater Med. 2009;20:2401.10.1007/s10856-009-3815-0 ↗
16. Kawai T, Takemoto M, Fujibayashi S, Neo M, Akiyama H, Yamaguchi S, Pattanayak DK, Matsushita T, Nakamura T, Kokubo T. Bone-bonding properties of Ti metal subjected to acid and heat treatments. J Mater Sci Mater Med. 2012;23:2981–92.10.1007/s10856-012-4758-4 ↗
17. Wen CE, Mabuchi M, Yamada Y, Shimojima K, Chino Y, Asahina T. Processing of biocompatible porous Ti and Mg. Scripta Mater. 2001;45:1147.10.1016/S1359-6462(01)01132-0 ↗
18. Otsuki B, Takemoto M, Fujibayashi S, Neo M, Kokubo T, Nakamura T. Pore throat size and connectivity determine bone and tissue ingrowth into porous implants: three-dimensional micro-CT based structural analyses of porous bioactive titanium implants. Biomaterials. 2006;27:5892.10.1016/j.biomaterials.2006.08.013 ↗
19. Kokubo T, Kushitani H, Sakka S, Kitsugi T, Yamamuro T. Solutions able to reproduce in vivo surface-structure changes in bioactive glass–ceramic A-W. J Biomed Mater Res. 1990;24:721.10.1002/jbm.820240607 ↗
20. Kokubo T, Takadama H. How useful is SBF in predicting in vivo bone bioactivity? Biomaterials. 2006;27:2907.10.1016/j.biomaterials.2006.01.017 ↗
21. Fujibayashi S, Neo M, Kim HM, Kokubo T, Nakamura T. A comparative study between in vivo bone ingrowth and in vitro apatite formation on Na2O-CaO-SiO2 glasses. Biomaterials. 2003;24:1349.10.1016/S0142-9612(02)00511-2 ↗
22. Kim HM, Miyaji F, Kokubo T, Nakamura T. Preparation of bioactive Ti and its alloys via simple chemical surface treatment. J Biomed Mater Res. 1996;32:409.10.1002/(SICI)1097-4636(199611)32:3<409::AID-JBM14>3.0.CO;2-B ↗
23. Yan WQ, Nakamura T, Kobayashi M, Kim HM, Miyaji F, Kokubo T. Bonding of chemically treated titanium implants to bone. J Biomed Mater Res. 1997;37:267.10.1002/(SICI)1097-4636(199711)37:2<267::AID-JBM17>3.0.CO;2-B ↗
24. Nishiguchi S, Fujibayashi S, Kim HM, Kokubo T, Nakamura T. Biology of alkali- and heat-treated titanium implants. J Biomed Mater Res A. 2003;67:26.10.1002/jbm.a.10540 ↗
25. Aparicio C, Manero JM, Conde F, Pegueroles M, Planell JA, Vallet-Regi M, Gil FJ. Acceleration of apatite nucleation on microrough bioactive titanium for bone-replacing implants. J Biomed Mater Res A. 2007;82:521.10.1002/jbm.a.31164 ↗
26. Aparicio C, Padros A, Gil FJ. In vivo evaluation of micro-rough and bioactive titanium dental implants using histometry and pull-out tests. J Mech Behav Biomed Mater. 2011;4:1672. Netherlands: 2011 Elsevier Ltd.10.1016/j.jmbbm.2011.05.005 ↗