Synthesized silicon-substituted hydroxyapatite coating on titanium substrate by electrochemical deposition
Source abstract
Abstract
Silicon-substituted hydroxyapaptite (Si-HA) coatings were prepared on titanium substrates by electrolytic deposition technique in electrolytes containing Ca(2+), PO(4)(3-) and SiO(3)(2-) ions with various SiO(3)(2-)/(PO(4)(3-) + SiO(3)(2-)) molar ratios (η(si)). The deposition was all conducted at a constant voltage of 3.0 V, with titanium substrate as cathode and platinum as anode, for 1 h at 85°C. The coatings thus prepared were characterized with inductively coupled plasma (ICP), X-ray diffraction (XRD), fourier transform infrared spectroscopy (FTIR), field-emission-type scanning electron microscope (FSEM). The results show that the silicon amount in the coatings increases linearly to about 0.48 wt% at first with increasing η(si) between 0 and 0.03, then increases slowly to about 0.55 wt% between 0.03 and 0.10 and finally maintains almost at a level around 0.55 wt% between 0.10 and 0.30. The tree-like Si-HA crystals are observed in the coatings prepared in the electrolyte of η(si) = 0.20. And the presence of silicon in electrolytes decreases the thickness of the coatings, with effect being more significant as η(si) increased. Additionally, the substitution of Si causes some OH(-) loss and changes the lattice parameters of hydroxyapatite (HA).
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Titanium Alloys Microstructure and Properties · Surface Treatment and Coatings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Suchanek W, Yoshimura M. Processing and properties of hydroxyapatite-based biomaterials for use as hard tissue replacement implants. J Mater Res. 1998;13:94–117.10.1557/JMR.1998.0015 ↗
2. Höland W, Vogel W, Naumann K, Gummel J. Interface reactions between machinable bioactive glass-ceramics and bone. J Biomed Mater Res. 1985;19:303–12.10.1002/jbm.820190311 ↗
3. Elliot J. Structure and chemistry of the apatites and other calcium orthophosphates. Amsterdam: Elsevier; 1994.
4. Carlisle EM. Silicon: a possible factor in bone calcification. Science. 1970;167:279–80.10.1126/science.167.3916.279 ↗
5. Gibson I, Hing JA, Best S, Bonfield W. Enhanced in vitro cell activity and surface apatite layer formation on novel silicon-substituted hydroxyapatites. Bioceramics. 1999;12:191–4.10.1142/9789814291064_0046 ↗
6. Patel N, Best S, Bonfield W, Gibson I, Hing K, Damien E, Revell P. A comparitive study on the in vivo behavior of hydroxyapatite and silicon substituted hydroxyapatite granules. J Mater Sci Mater Med. 2002;13:1199–206.10.1023/A:1021114710076 ↗
7. Tang Q, Brooks R, Rushton N, Best M. Production and characterization of HA and SiHA coatings. J Mater Sci Mater Med. 2010;21:173–81.10.1007/s10856-009-3841-y ↗
8. Zhang E, Zou C. Porous titanium and silicon-substituted hydroxyapatite biomodification prepared by a biomimetic process: characterization and in vivo evaluation. Acta Biomater. 2009;5:1732–41.10.1016/j.actbio.2009.01.014 ↗
9. Thian E, Huang J, Vickers M, Best S, Barber Z, Bonfield W. Silicon-substituted hydroxyapatite (Si-HA): a novel calcium phosphate coating for biomedical applications. J Mater Sci. 2006;41:709–17.10.1007/s10853-006-6489-8 ↗
10. Hijon N, Cabanas M, Pena J, Vallet-Regi M. Dip coated silicon-substituted hydroxyapatite films. Acta Biomater. 2006;2:567–74.10.1016/j.actbio.2006.05.004 ↗
11. Yang Y, Paital SR, Dahotre NB. Effects of SiO2 substitution on wettability of laser deposited Ca-P biocoating on Ti-6Al-4V. J Mater Sci Mater Med. 2010;21:2511–21.10.1007/s10856-010-4105-6 ↗
12. Ban S, Maruno S. Effect of temperature on electrochemical deposition of calcium phosphate coatings in a simulated body fluid. Biomaterials. 1995;16:977–81.10.1016/0142-9612(95)94904-Y ↗
13. Ye W, Wang XX. Ribbon-like and rod-like hydroxyapatite crystals deposited on titanium surface with electrochemical method. Mater Lett. 2007;61:4060–5.
14. Ma M, Ye W, Wang XX. Effect of supersaturation on the morphology of hydroxyapatite crystals deposited by electrochemical deposition on titanium. Mater Lett. 2008;62:3875–7.10.1016/j.matlet.2008.05.009 ↗
15. Jiao MJ, Wang XX. Electrolytic deposition of magnesium-substituted hydroxyapatite crystals on titanium substrate. Mater Lett. 2009;63:2286–9.10.1016/j.matlet.2009.07.048 ↗
16. Kay MI, Young RA, Posner AS. A crystal structure of hydroxyapatite. Nature. 1964;204:1050–2.10.1038/2041050a0 ↗
17. Vallet-Regí M, Arcos D. Silicon substituted hydroxyapatite. A method to upgrade calcium phosphate based implants. J Mater Chem. 2005;15:1509–16.10.1039/B414143A ↗
18. Rößler S, Sewing A, Stölzel M, Scharnweber M, Dard M, Worch H. Electrochemically assisted deposition of thin calcium phosphate coatings at near-physiological pH and temperature. J Biomed Mater Res. 2002;64:655–63.
19. Andersson J, Areva S, Spliethoff B, Lindén M. Sol–gel synthesis of a multifunctional, hierarchically porous silica/apatite composite. Biomaterials. 2005;26:6827–35.10.1016/j.biomaterials.2005.05.002 ↗
20. Leventouri T, Bunaciu C, Perdikatsis V. Neutron powder diffraction studies of silicon-substituted hydroxyapatite. Biomaterials. 2004;24:4205–21.10.1016/S0142-9612(03)00333-8 ↗
21. Gibson I, Best S, Bonfield W. Chemical characterization of silicon-substituted hydroxyapatite. J Biomed Mater Res. 1999;44:422–8.10.1002/(SICI)1097-4636(19990315)44:4<422::AID-JBM8>3.0.CO;2-# ↗
22. Tang X, Xiao X, Liu R. Structural characterization of silicon-substituted hydroxyapatite synthesized by hydrothermal method. Mater Lett. 2005;59:3841–6.10.1016/j.matlet.2005.06.060 ↗
23. Zhang E, Zou C, Zeng S. Preparation and characterization of silicon-substituted hydroxyapatite coating by a biomimetic process on titanium substrate. Surf Coat Technol. 2009;23:1075–80.10.1016/j.surfcoat.2008.09.038 ↗
24. Lin DY, Wang XX. Electrodeposition of hydroxyapatite coating on CoNiCrMo substrate in dilute solution. Surf Coat Technol. 2010;204:3205–13.10.1016/j.surfcoat.2010.03.020 ↗
25. Porter AE, Patel N, Skeeper JN, Best SM, Bonfield W. Comparison of in vivo dissolution processes in hydroxyapatite and silicon-substituted hydroxyapatite ceramics. Biomaterials. 2003;24:4609–20.10.1016/S0142-9612(03)00355-7 ↗
26. Thian E, Huang J, Best S, Barber Z, Brooks R, Rushton N, Bonfield W. The response of osteoblasts to nanocrystalline silicon-substituted hydroxyapatite thin films. Biomaterials. 2005;27:2692–8.10.1016/j.biomaterials.2005.12.019 ↗
27. Thian E, Huang J, Best S, Barber Z, Bonfield W. Silicon-substituted hydroxyapatite: the next generation of bioactive coatings. Mater Sci Eng C. 2007;27:251–6.10.1016/j.msec.2006.05.016 ↗
28. Chen X, Wu T, Wang Q, Shen JW. Shield effect of silicate on adsorption of proteins onto silicon-doped hydroxyapatite (100) surface. Biomaterials. 2008;29:2423–32.10.1016/j.biomaterials.2008.02.002 ↗
29. Thian ES, Ahmad Z, Huang J, Edirisinghe MJ, Jayasinghe SN, Ireland DC, Brooks RA, Rushton N, Bonfield W, Best SM. The role of surface wettability and surface charge of electrosprayed nanoapatites on the behavior of osteoblasts. Acta Biomater. 2010;6:750–5.10.1016/j.actbio.2009.08.012 ↗