journal article·2013-09

Comparison of a SiO2–CaO–ZnO–SrO glass polyalkenoate cement to commercial dental materials: ion release, biocompatibility and antibacterial properties

A. W. Wren, A. Coughlan, M. M. Hall, M. J. German, M. R. Towler

Publisher page

Abstract

Ion Release and biocompatibility of a CaO-SrO-ZnO-SiO₂ (BT 101) based glass polyalkenoate cement (GPC) was compared against commercial GPCs, Fuji IX and Ketac Molar. The radiopacity (R) was similar for each material, 2.0-2.8. Ion release was evaluated on each material over 1, 7, 30 and 90 days. BT 101 release included Ca (23 mg/L), Sr (23 mg/L) Zn (13 mg/L), Si (203 mg/L). Fuji IX release includes Ca (0.7 mg/L), Al (3 mg/L) Si (26 mg/L), Na (60 mg/L) and P (0.5 mg/L) while Ketac Molar release includes Ca (1 mg/L), Al (0.6 mg/L) Si (23 mg/L), Na (76 mg/L) and P (0.7 mg/L). Simulated body fluid trials revealed CaP surface precipitation on BT 101. No evidence of precipitation was found on Fuji IX or Ketac Molar. Cytotoxicity testing found similar cell viability values for each material (~60 %, P = 1.000). Antibacterial testing determined a reduced CFU count with BT 101 (2.5 × 10³) when compared to the control bacteria (2.4 × 10⁴), Fuji IX (1.5 × 10⁴) and Ketac Molar (1.2 × 10⁴).
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Endodontics and Root Canal Treatments · Dental materials and restorations · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Nicholson, J.W., and A.D. Wilson. 1993. Acid-Base cements–Their biomedical and industrial applications. In Chemistry of Solid State Materials, Vol 3. Cambridge: Cambridge University press
2. Xie D, Brantley WA, Culbertson BM, Wang G. Mechanical properties and microstructures of glass ionomer cements. Dent Mater. 2000;16:129–38.10.1016/S0109-5641(99)00093-7 ↗
3. Hatton PV, Hurrell-Gillingham K, Reaney IM, Miller CA, Crawford A. Devitrification of ionomer glass and its effect on the in vitro biocompatability of glass ionomer cements. Biomaterials. 2003;24:3153–60.10.1016/S0142-9612(02)00510-0 ↗
4. DeBarra E, Hill R. Influence of alkali metal ions on the fracture properties of glass polyalkenoate (ionomer) cements. Biomaterials. 1998;19:495–502.10.1016/S0142-9612(97)00129-4 ↗
5. Fennell B, Hill RG. The influence of poly(acrylic) acid molar mass and concentration on the properties of polyalkenoate cements. J Mater Sci. 2001;36:5193–202.10.1023/A:1012445928805 ↗
6. Cho S, Cheng AC. A review of glass ionomer restorations in the primary dentition. Journal/Canadian Dental Association. 1999;65:491–5.
7. DeBruyne MAA, DeMoor RJG. The use of glass ionomer cements in both conventional and surgical endodontics. Int Endod J. 2004;37:91–104.10.1111/j.0143-2885.2004.00769.x ↗
8. Weber A, May A, von Ilberg C. Bone replacement by ionomer cement in osteoplastic frontal sinus operations. Eur Arch Otorhinolaryngol. 1997;254(1):S162–4.10.1007/BF02439751 ↗
9. Akinmade AO, Nicholson JW. Glass ionomer cements as adhesives. Journal of Material Science. 1993;4(2):95–101.
10. Tyas MJ, Burrow MF. Adhesive restorative materials: A review. Aust Dent J. 2004;49(3):112–21.10.1111/j.1834-7819.2004.tb00059.x ↗
11. Smith DC. Development of glass-ionomer cement systems. Biomaterials. 1998;19(6):467–78.10.1016/S0142-9612(97)00126-9 ↗
12. Hill RG, Griffin S. Glass composition influence on glass polyalkenoate cement mechanical properties. J Non-Cryst Solids. 1996;196:255–9.10.1016/0022-3093(95)00596-X ↗
13. Nicholson JW. Adhesive dental materials-A review. Int J Adhes Adhes. 1998;18(4):229–36.10.1016/S0143-7496(98)00027-X ↗
14. Zimehl R, Hannig M. Non metallic restorative materials based on glass ionomer cements - recent trends and developments. Colloids Surf A. 2000;163(1):55–62.10.1016/S0927-7757(99)00430-6 ↗
15. Firling CE, Hill TA, Severson AR. Aluminium toxicity perturbs long bone calcification in the embryonic chick. Arch Toxicol. 1999;73:359–66.10.1007/s002040050674 ↗
16. Carter DH, Sloan P, Brook IM, Hatton PV. Role of exchanged ions in the integration of ionomeric (glass polyalkenoate) bone substitutes. Biomaterials. 1997;18:459–66.10.1016/S0142-9612(96)00150-0 ↗
17. Kaplan AE, Williams J, Billington RW, Braden M, Pearson GJ. Effects of variation in particle size on biaxial flexural strength of two conventional glass–ionomer cements. J Oral Rehabil. 2004;31:373–8.10.1046/j.1365-2842.2003.01234.x ↗
18. Marie PJ. Strontium ranelate; a novel mode of action optimizing bone formation and resorption. Osteoporos Int. 2005;16:S7–10.10.1007/s00198-004-1753-8 ↗
19. Marie PJ. Strontium ranelate: New insights into its dual mode of action. Bone. 2007;40:S6–8.10.1016/j.bone.2007.02.003 ↗
20. Yamaguchi M, Ma ZJ. Stimulatory effect of zinc on Deoxyribonucleic acid synthesis in bone growth of newborn rats: enhancement with zinc and insulin like growth factor-I. Calcif Tissue Int. 2001;69:158–63.10.1007/s00223-001-2010-1 ↗
21. Griffin SG, Hill RG. Influence of glass composition on the properties of glass polyalkenoate cements Part I: influence of aluminium to silicon ratio. Biomaterials. 1999;20(17):1579–86.10.1016/S0142-9612(99)00058-7 ↗
22. Wren AW, Coughlan A, Laffir FR, Towler MR. Comparison of a SiO2-CaO-ZnO-SrO glass polyalkenoate cement to commercial dental materials: glass structure and physical properties. J Mater Sci. 2012;. doi: 10.1007/s10856-012-4813-1 .
23. Kokubo T, Takadama H. How useful is SBF in predicting in vivo bone bioactivity. Biomaterials. 2006;27:2907–15.10.1016/j.biomaterials.2006.01.017 ↗
24. Lewis G, Towler MR, Boyd D, German MJ, Wren AW, Clarkin OM, Yates A. Evaluation of two novel aluminum-free, zinc-based glass polyalkenoate cements as alternatives to PMMA bone cement for use in vertebroplasty and balloon kyphoplasty. J Mater Sci. 2012;21:59–66.
25. Czarnecka B, Limanowska-Shaw H, Nicholson JW. Buffering and ion-release by a glass-ionomer cement under near-neutral and acidic conditions. Biomaterials. 2002;23:2783–8.10.1016/S0142-9612(02)00014-5 ↗
26. Boyd D, Towler MR, Wren AW, Clarkin OM, Tanner DA. TEM analysis of apatite surface layers observed on zinc based glass polyalkenoate cements. J Mater Sci. 2008;43:1170–3.10.1007/s10853-007-2362-7 ↗
27. Bigi A, Foresti E, Gandolfi M, Gazzano M, Roveri N. Inhibiting effect of zinc on hydroxylapatite crystallization. J Inorg Biochem. 1995;58:49–58.10.1016/0162-0134(94)00036-A ↗
28. Kanzaki N, Treboux G, Onuma K, Ito A, Tsutsumi S. Inhibitory effect of magnesium and zinc crystallization kinetics of Hydroxyapatite (0001) face. J Phys Chem. 2000;104:4189–94.10.1021/jp9939726 ↗
29. Kokubo T. Solutions able to reproduce in vivo surface-structure changes in bioactive glass ceramic in A-W. J Biomed Mater Res. 1990;24(B):721–34.10.1002/jbm.820240607 ↗