Silver coated bioactive glass particles for wound healing applications
Source abstract
Abstract
Bioactive glass particles (0.42SiO(2)-0.15CaO-0.23Na(2)O-0.20ZnO) of varying size (<90 μm and 425-850 μm) were synthesized and coated with silver (Ag) to produce Ag coated particles (PAg). These were compared against the uncoated analogous particles (Pcon.). Surface area analysis determined that Ag coating of the glass particles resulted in increased the surface area from 2.90 to 9.12 m(2)/g (90 μm) and 1.09-7.71 m(2)/g (425-850 μm). Scanning electron microscopy determined that the Ag coating remained at the surface and there was little diffusion through the bulk. Antibacterial (Escherichia coli--13 mm and Staphylococcus epidermidis--12 mm) and antifungal testing (Candida albicans--7.7 mm) determined that small Ag-coated glass particles exhibited the largest inhibition zones compared to uncoated particles. pH analysis determined an overall higher pH consider in the smaller particles, where after 24 h the large uncoated and Ag coated particles were 8.27 and 8.74 respectively, while the smaller uncoated and Ag coated particles attained pH values of 9.63 and 9.35 respectively.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Dental materials and restorations · Laser-Ablation Synthesis of Nanoparticles
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Hench LL. The story of bioglass. J Mater Sci Mater Med. 2006;17:967–78.10.1007/s10856-006-0432-z ↗
2. Hench LL, Peitl O, Zanotto ED. Highly bioactive P2O5–Na2O–CaO–SiO2 glass ceramics. J Non Crys Solids. 2001;292:115–26.10.1016/S0022-3093(01)00822-5 ↗
3. Verne E, Di Nunzio S, Bosetti M, Appendino P, Vitale Brovarone C, Maina G, Cannas M. Surface characterization of silver-doped bioactive glass. Biomaterials. 2005;26:5111–9.10.1016/j.biomaterials.2005.01.038 ↗
4. Wren AW, Laffir FR, Kidari A, Towler MR. The structural role of titanium in Ca–Sr–Zn–Si/Ti glasses for medical applications. J Non Crys Solids. 2010;357(3):1021–6.10.1016/j.jnoncrysol.2010.11.039 ↗
5. Serra J, Gonzalez P, Liste S, Chiussi S, Leon B, Perez-amor M, Ylanen HO, Hupa M. Influence of the non-bridging oxygen groups on the bioactivity of silicate glasses. J Mater Sci Mater Med. 2002;13:1221–5.10.1023/A:1021174912802 ↗
6. Kokubo T, Takadama H. How useful is SBF in predicting in vivo bone bioactivity. Biomaterials. 2006;27:2907–15.10.1016/j.biomaterials.2006.01.017 ↗
7. Rico H, Villa LF. Zinc, a new coherent therapy for osteoporosis. Calcif Tissue Int. 2000;67:422–3.10.1007/s002230001138 ↗
8. Balamurugan A, Balossier G, Kannan S, Michel J, Rebelo AHS, Ferreira JMF. Development and in vitro characterization of sol–gel derived CaO–P2O5–SiO2–ZnO bioglass. Acta Biomater. 2007;3:255–62.10.1016/j.actbio.2006.09.005 ↗
9. Piscanec S, Ciacchi LC, Vesselli E, Comelli G, Sbaizero O, Meriani S, De Vita A. Bioactivity of TiN-coated titanium implants. Acta Mater. 2004;52:1237–45.10.1016/j.actamat.2003.11.020 ↗
10. Ochoa I, Sanz-Herrera JA, García-Aznar JM, Doblaré M, Yunos DM, Boccaccini AR. Permeability evaluation of 45S5 bioglass®-based scaffolds for bone tissue engineering. J Biomech. 2009;42(3):257–60.10.1016/j.jbiomech.2008.10.030 ↗
11. Chen QZ, Thompson ID, Boccaccini AR. 45S5 Bioglass®-derived glass-ceramic scaffolds for bone tissue engineering. Biomaterials. 2006;27(11):2414–25.10.1016/j.biomaterials.2005.11.025 ↗
12. Peter M, Binulal NS, Nair SV, Selvamurugan N, Tamura H, Jayakumar R. Novel biodegradable chitosan-gelatin/nano-bioactive glass ceramic composite scaffolds for alveolar bone tissue engineering. Chem Eng J. 2010;158(2):353–61.10.1016/j.cej.2010.02.003 ↗
13. Jones JR, Ehrenfried LM, Hench LL. Optimising bioactive glass scaffolds for bone tissue engineering. Biomaterials. 2006;27(7):964–73.10.1016/j.biomaterials.2005.07.017 ↗
14. Wren AW, Akgun B, Adams B, Coughlan A, Mellott NP, Towler MR. Characterization and antibacterial efficacy of silver-coated Ca–Na–Zn–Si/Ti glasses. J Biomater Appl. 2011;7(3):1–4.
15. Kawashita M, Tsuneyama S, Miyaji F, Kokubo T, Kozuka H, Yamamoto K. Antibacterial silver-containing silica glass prepared by solgel method. Biomaterials. 2000;21:393–8.10.1016/S0142-9612(99)00201-X ↗
16. Newby PJ, El-Gendy R, Kirkham J, Yang XB, Thompson ID, Boccaccini AR. Ag-doped 45S5 Bioglass (R)-based bone scaffolds by molten salt ion exchange: processing and characterisation. J Mater Sci Mater Med. 2011;22(3):557–69.10.1007/s10856-011-4240-8 ↗
17. Lee S-B, Otgonbayar U, Lee J-H, Kim K-M, Kim K-N. Silver ion-exchanged sodium titanate and resulting effect on antibacterial efficacy. Surf Coat Technol. 2010;205(1):S172–6.10.1016/j.surfcoat.2010.07.049 ↗
18. Husheng J, Wensheng H, Liqiao W, Bingshe X, Xuguang L. The structures and antibacterial properties of nano-SiO2 supported silver/zinc–silver materials. Dent Mater. 2008;24:244–9.10.1016/j.dental.2007.04.015 ↗
19. Axford JS. Joint and bone infections. Medicine. 2006;34(10):405.10.1053/j.mpmed.2006.07.009 ↗
20. Arias F, Mata-Essayag S, Landaeta ME, de Hartung Capriles C, Perez C, Nunez MJ, Carvajal A, Silva M. Candida albicans osteomyelitis: case report and literature review. Int J Infect Dis. 2004;8:307–14.10.1016/j.ijid.2003.12.006 ↗
21. Pastor L, García-Domenech R, Gálvez J, Wolski S, García MD. New antifungals selected by molecular topology. Bioorg Med Chem Lett. 1998;8(18):2577–82.10.1016/S0960-894X(98)00460-0 ↗
22. Jiang B, Bussey H, Roemer T. Novel strategies in antifungal lead discovery. Cur Opin Microbiol. 2002;5(5):466–71.10.1016/S1369-5274(02)00361-2 ↗
23. Lou N, Lixin M, Lizhong J, Zhan J, Wu Z, Wu D. Directly ultraviolet photochemical deposition of silver nanoparticles on silica spheres: preparation and characterization. Mater Lett. 2009;63:154–6.10.1016/j.matlet.2008.09.033 ↗
24. Akgun BA, Durucan C, Mellott NP. Effect of silver incorporation on crystallization and microstructural properties of sol–gel derived titania thin films on glass. J Sol Gel Sci Technol. 2011;58:277–89.10.1007/s10971-010-2388-1 ↗
25. Qin Z, Zhang J, Hub Y, Chi Q, Mortensen NP, Quc D, Molin S, Ulstrup J. Organic compounds inhibiting S. epidermidis adhesion and biofilm formation. Ultramicroscopy. 2009;109:881–8.10.1016/j.ultramic.2009.03.040 ↗
26. Pallavicini P, Taglietti A, Dacarro G, Diaz-Fernandez YA, Galli M, Grisoli P, Patrini M, De Magistris GS, Zanoni R. Self-assembled monolayers of silver nanoparticles firmly grafted on glass surfaces: low Ag + release for an efficient antibacterial activity. J Colloid Interface Sci. 2010;350:110–6.10.1016/j.jcis.2010.06.019 ↗
27. Balamurugan A, Balossier G, Laurent-Maquin D, Pina S, Rebelo AHS, Faure J, Ferreira JMF. An in vitro biological and anti-bacterial study on a sol–gel derived silver-incorporated bioglass system. Dent Mater. 2008;24:1343–51.10.1016/j.dental.2008.02.015 ↗
28. Yang X, Yang W, Wang Q, Li H, Wang k, Yang L, Liu W. Atomic force microscopy investigation of the characteristic effects of silver ions on Escherichia coli and Staphylococcus epidermidis. Talanta. 2010;81:1508–12.10.1016/j.talanta.2010.02.061 ↗