The effect of abrading and cutting instruments on machinability of dental ceramics
Source abstract
Abstract
The aim was to investigate the effect of machining instruments on machinability of dental ceramics. Four dental ceramics, including two zirconia ceramics were machined by three types (SiC, diamond vitrified, and diamond sintered) of wheels with a hand-piece engine and two types (diamond and carbide) of burs with a high-speed air turbine. The machining conditions used were abrading speeds of 10,000 and 15,000 r.p.m. with abrading force of 100 gf for the hand-piece engine, and a pressure of 200 kPa and a cutting force of 80 gf for the air-turbine hand-piece. The machinability efficiency was evaluated by volume losses after machining the ceramics. A high-abrading speed had high-abrading efficiency (high-volume loss) compared to low-abrading speed in all abrading instruments used. The diamond vitrified wheels demonstrated higher volume loss for two zirconia ceramics than those of SiC and diamond sintered wheels. When the high-speed air-turbine instruments were used, the diamond points showed higher volume losses compared to the carbide burs for one ceramic and two zirconia ceramics with high-mechanical properties. The results of this study indicated that the machinability of dental ceramics depends on the mechanical and physical properties of dental ceramics and machining instruments. The abrading wheels show autogenous action of abrasive grains, in which ground abrasive grains drop out from the binder during abrasion, then the binder follow to wear out, subsequently new abrasive grains come out onto the instrument surface (autogenous action) and increase the grinding amount (volume loss) of grinding materials.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Denry I, Holloway JA. Ceramics for dental applications: a review. Materials. 2010;3:351–68.10.3390/ma3010351 ↗
2. Sailer I, Philippa, Zembic A, Pjetursson BE, Hämmerle CH, Zwahlen M. A systematic review of the performance of ceramic and metal implant abutments supporting fixed implant reconstructions. Clin Oral Implants Res. 2009;20:4–31. Suppl 410.1111/j.1600-0501.2009.01787.x ↗
3. Albakry M, Guazzato M, Swain MV. Biaxial flexural strength, elastic moduli, and x-ray diffraction characterization of three pressable all-ceramic materials. J Prosthet Dent. 2003;89:374–80.10.1067/mpr.2003.42 ↗
4. Conrad HJ, Seong WJ, Pesun IJ. Current ceramic materials and systems with clinical recommendations: a systematic review. J Prosthet Dent. 2007;98:389–404.10.1016/S0022-3913(07)60124-3 ↗
5. Kontonasaki E, Kantiranis N, Papadopoulou L, Chatzistavrou X, Kavouras P, Zorba T, Sivropoulou A, Chrissafis K, Paraskevopoulos KM, Koidis PT. Microstructural characterization and comarative evaluation of physical, mechanical and biological properties of three ceramics for metal-ceramic restrations. Dent Mater. 2008;24:1362–73.10.1016/j.dental.2008.03.002 ↗
6. Gonzaga CC, Cesar PF, Miranda WG Jr, Yoshimura HN. Slow crack growth and reliability of dental ceramics. Dent Mater. 2011;27:394–406.10.1016/j.dental.2010.10.025 ↗
7. International Organization for Standardization. ISO 6872: Dental ceramic. Geneva, Switzerland; 2008.
8. International Organization for Standardization. ISO 9693: Metal-ceramic dental restorative systems. Geneva, Switzerland; 1999.
9. Denry IL, Holloway JA. Elastic constants, Vickers hardness, and fracture toughness of fluorrichterite-based glass-ceramics. Dent Mater. 2004;20:213–9.10.1016/S0109-5641(03)00094-0 ↗
10. Kern M, Sasse M, Wolfart S. Ten-year outcome of three-unit fixed dental prostheses made from monolithic lithium disilicate ceramic. J Am Assoc. 2012;143:234–40.
11. Kosmac T, OBlak C, Jevnikar P, Funduk N, Marion L. Strength and reliability of surface treated Y-TZP dental ceramics. J Biomed Mater Res. 2000;53:304–13.10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
12. Sax C, Hämmerle CH, Sailer I. 10-year clinical outcomes of fixed dental prostheses with zirconia frameworks. Int J Comput Dent. 2011;14:183–202.
13. Choi JE, Waddell JN, Torr B, Swain MV. Pressed ceramics onto zirconia. Part 1: comparison of crystalline phases present, adhesion to a zirconia system and flexural strength. Dent Mater. 2011;27:1204–12.10.1016/j.dental.2011.08.006 ↗
14. White SN, Miklus VG, McLaren EA, Lang LA, Caputo AA. Flexural strength of a layered zironia and porcelain dental all-ceramic system. J Prosthet Dent. 2005;94:125–31.10.1016/j.prosdent.2005.05.007 ↗
15. Fischer J, Stawarczyk B, Hämmerle CH. Flexural strength of veneering ceramics for zirconia. J Dent. 2008;24:471–5.
16. Albashaireh ZS, Ghazal M, Kern M. Two-body wear of different ceramic materials opposed to zirconia ceramic. J Prosthet Dent. 2010;104:105–13.10.1016/S0022-3913(10)60102-3 ↗
17. Jung YS, Lee JW, Choi YJ, Ahn JS, Shin SW, Huh JB. A study on the in-vitro wear of the natural tooth structure by opposing zirconia or dental porcelain. J Adv Prosthodont. 2010;2:111–5.10.4047/jap.2010.2.3.111 ↗
18. Taira M, Wakasa K, Yamaki M, Matsui A. Dental cutting behaviour of mica-based and apatite-based machinable glass-ceramics. J Oral Rehabil. 1990;17:461–72.10.1111/j.1365-2842.1990.tb01417.x ↗
19. Schmidt C, Weigl P. Machinability of IPS Empress 2 framework ceramic. J Biomed Mater Res. 2000;53:348–52.10.1002/1097-4636(2000)53:4<348::AID-JBM8>3.0.CO;2-0 ↗
20. Song XF, Ren HT, Yin L. Machinability of lithium disilicate glass ceramic in in vitro dental diamond bur adjusting process. J Mech Behav Biomed Mater. 2016;53:78–92.10.1016/j.jmbbm.2015.08.003 ↗
21. Ohkubo C, Watanabe I, Ford JP, Nakajima H, Hosoi T, Okabe T. The machinability of cast titanium and Ti-6Al-4V. Biomaterials. 2000;21:421–8.10.1016/S0142-9612(99)00206-9 ↗
22. Watanabe I, Ohkubo C, Ford JP, Atsuta M, Okabe T. Cutting efficiency of air-turbine burs on cast titanium and dental casting alloys. Dent Mater. 2000;16:420425.10.1016/S0109-5641(00)00038-5 ↗
23. Ohkubo C, Hosoi T, Ford JP, Watanabe I. Effect of surface reaction layer on grindability of cast titanium alloys. Dent Mater. 2006;22:268–74.10.1016/j.dental.2005.04.020 ↗
24. Ban S. Properties of zirconia for realization of all-ceramic restoration. Shikwa Gakuho. 2007;107:670–84.
25. Tang X, Nakamura T, Usami H, Wakabayashi K, Yatani H. Effects of multiple firings on the mechanical properties and microstructure of veneering ceramics for zirconia frameworks. J Dent. 2012;40:372–80.10.1016/j.jdent.2012.01.014 ↗
26. Anusavice KJ. Phillip’s Science of Dental Materials. 12th ed St. Louis: Elsevier; 2013. P. 239.