Characterization of copper corrosion products originated in simulated uterine fluids and on packaged intrauterine devices
Source abstract
Abstract
This paper studies the characterization of corrosion products originated after 1 and 12 weeks' immersion of copper specimens in simulated uterine fluids at pH 6.3 and 8.0 and at 37 degrees C temperature. The experimental techniques used were X-ray photo-electron spectroscopy, scanning electron microscopy, and energy dispersive X-ray. The compounds found were calcite (CaCO3), calcium phosphate, cuprite (Cu2O) and copper hydroxide (Cu(OH)2). The morphology of corrosion products was a non-uniform, layer showing some paths through which copper ions can be released. In parallel, corrosion products formed on packaged, unused copper-containing intrauterine devices (IUD) were analyzed. Cuprite (Cu2O) and chalcocite (Cu2S) were the main species identified.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Pregnancy and Medication Impact · Reproductive System and Pregnancy
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. G. OSTER and M. P. SALGO, New Engl. J. Med. 28 (1975) 432.10.1056/NEJM197508282930906 ↗
2. G. K. OSTER, Fertil Steril. 23 (1972) 18.10.1016/S0015-0282(16)38703-9 ↗
3. W. A. A. VAN OS, C. C. A. DE NOOYER and P. E. R. RHEMREV, in ``Medicated Intrauterine Devices Physiological and Clinical Aspects'' (Martinus Nijhoff, London, 1980) p. 111.10.1007/978-94-009-8872-9_10 ↗
4. K. HAGENFELDT, Contraception 6 (1972) 37.10.1016/S0010-7824(72)80004-0 ↗
5. H. TIMONEN, Contraception 14 (1976) 25.10.1016/S0010-7824(76)80005-4 ↗
6. A. KOSONEN, Fertil. Steril. 30 (1978) 59.10.1016/S0015-0282(16)43397-2 ↗
7. H. H. EL-BADRAWI and E. S. E. HAFEZ, in ``Medicated Intrauterine Devices Physiological and Clinical Aspects'' (Martinus Nijhoff, London, 1980) p. 60.10.1007/978-94-009-8872-9_7 ↗
8. A. KOSONEN, in ``Medicated Intrauterine Devices Physiological and Clinical Aspects'' (Martinus Nijhoff, London, 1980) p. 22.10.1007/978-94-009-8872-9_3 ↗
9. M. THIERY, F. SCHMIDT and H. J. TATUM. Contraception 26 (1982) 295.10.1016/0010-7824(82)90077-4 ↗
10. R. W. JONES, N. M. GREGSON and M. ELSTEIN, Brit. Med. J. 2 (1973) 520.10.1136/bmj.2.5865.520 ↗
11. A. SEDLIS, E. KANDEMIR and M. L. STONE, Obstet. Gynecol. 30 (1967) 114.
12. H. LEIDHEISER JR., in ``The Corrosion of Copper, Tin, and Their Alloys'' (Wiley, New York, 1971) p. 14 and p. 60.
13. J. M. BASTIDAS, A. LOPEZ-DELGADO, F. A. LOPEZ and M. P. ALONSO, J. Mater. Sci. 32 (1997) 129.10.1023/A:1018535401657 ↗
14. J. M. BASTIDAS and J. SIMANCAS. Biomaterials 18 (1997) 247.10.1016/S0142-9612(96)00136-6 ↗
15. C. ZHANG, N. XU and B. YANG, Corros. Sci. 38 (1996) 635.10.1016/0010-938X(95)00154-C ↗
16. B. I. RICKETT and J. H. PAYER, J. Electrochem. Soc. 142 (1995) 3713.10.1149/1.2048403 ↗
17. S. K. CHAWLA, N. SANKARRAMAN and J. H. PAYER, J. Electron Spectroc. 61 (1992) 1.10.1016/0368-2048(92)80047-C ↗
18. A. LOPEZ-DELGADO, E. CANO, J. M. BASTIDAS and F. A. LOPEZ, J. Electrochem. Soc. 145 (1998) 4140.10.1149/1.1838928 ↗
19. D. W. RICE, R. J. CAPPELL, W. KINSOLVING and J. J. LASKOWSKI, J. Electrochem. Soc. 127 (1980) 891.10.1149/1.2129780 ↗
20. S. P. SHARMA, J. Electrochem. Soc. 127 (1980) 21.10.1149/1.2129622 ↗
21. A. MOREAU, Electrochim. Acta 26 (1981) 1609.10.1016/0013-4686(81)85134-1 ↗
22. S. FELIU JR., J. L. G. FIERRO and C. MAFFIOTTE, Prog. Org. Coat. 30 (1997) 247.10.1016/S0300-9440(96)00690-X ↗