Effect of thermal treatments on tensile strength of commercially cast pure titanium and Ti-6Al-4V alloys
Source abstract
Abstract
Heating titanium structures is assumed to relieve tensions induced by the casting process as well as possibly optimizing some mechanical properties. The aim of this investigation was to evaluate the effect of thermal treatments on tensile strength of commercially pure titanium (CP Ti) and Ti-6Al-4V alloy. Thirty dumbbell rods, with diameters of 3.0 mm at the central segment and lengths of 42 mm, were cast for each metal using the Rematitan System. CP Ti and Ti-6Al-4V specimens were randomly divided into three groups of ten: a control group that received no thermal treatment and two test groups. One (T1) was heated at 750 degrees C for 2 h and the other (T2) was annealed at 955 degrees C for 1 h and aged at 620 degrees C for 2 h. Tensile strength was measured with a universal testing machine (MTS model 810). Tensile strength means and standard deviations were statistically compared using a Kruskal-Wallis test at a alpha=0.05 significance level. No statistically significant differences in tensile strength were observed among CP Ti groups. For the Ti-6Al-4V alloy, the control and T1 groups revealed statistically higher tensile strengths when compared to the T2 group, with no significant difference between the control and T1 groups.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. M. J. DONACHIE, JR., in “Titanium. A Technical Guide” (ASM International, Hhio, 1988) p. 21, 57, 105.
2. K. S. JANG, S. J. YOUN and Y. S. KIM, J. Prosthet. Dent. 86(2001) 93.10.1067/mpr.2001.116168 ↗
3. C. OHKUBO, I. WATANABE, J. P. FORD, H. NAKAJIMA, T. HOSOI and T. OKABE, Biomaterials 21 (2000) 421.10.1016/S0142-9612(99)00206-9 ↗
4. R. R. WANG and A. FENTON, Quintessence Int. 27 (1996) 401.
5. S. ZINELIS, J. Prosthet. Dent. 84(2000) 575.10.1067/mpr.2000.109479 ↗
6. R. G. CRAIG, in “Restorative Dental Materials” (Mosby, Saint Louis, 1997) p. 428.
7. R. R. WANG and A. M. BOYLE, J. Prosthet. Dent. 70 (1993) 275.10.1016/0022-3913(93)90065-V ↗
8. E. LAUTENSCHLAGER and P. MONAGHAN, Int. Dent. J. 43 (1993) 245.
9. International Organization for Standardization. ISO 1562. (Geneve, 1984) p. 4.
10. T. AHMED and H. J. RACK, Mater. Sci. Engng. A 243 (1998) 206.10.1016/S0921-5093(97)00802-2 ↗
11. P. L. BOURASSA, S. YUE and J. D. BOBYN, J. Biomed. Mater. Res. 37(1997) 291.10.1002/(SICI)1097-4636(199711)37:2<291::AID-JBM20>3.0.CO;2-G ↗
12. P. J. FOPIANO and C. F. HICKEY JR., J. Testing Eval. 1 (1973) 514.10.1520/JTE10060J ↗
13. A. LASALMONIE and M. LOUBRADOU, J. Mater. Sci. 14 (1979) 2589.10.1007/BF00610627 ↗
14. P. E. MARKOVSKY, Mater. Sci. Engng. A190 (1995) L9.10.1016/0921-5093(94)02707-N ↗
15. D. J. SIMBI and J. C. SCULLY, Mater. Lett. 26 (1996) 35.10.1016/0167-577X(95)00204-9 ↗
16. G. SRIDHAR, V. V. KUTUMBARAO and D. S. SARMA, Metall. Trans. A 18A (1987) 877.10.1007/BF02646929 ↗
17. I. WEISS and S. L. SEMIATIN, Mater. Sci. Engng. A 263 (1999) 243.10.1016/S0921-5093(98)01155-1 ↗
18. G. LUTJERING, ibid. A 243 (1998) 32.10.1016/S0921-5093(97)00778-8 ↗
19. E. A. TRILLO, C. ORTIZ, P. DICKERSON, R. VILLA, S. W. STAFFORD and L. E. MURR, J. Mater. Sci. Mater. Med. 12 (2001) 283.10.1023/A:1011210101895 ↗