journal article·2017-07

Deposition of crystalline hydroxyapatite nano-particle on zirconia ceramic: a potential solution for the poor bonding characteristic of zirconia ceramics to resin cement

Abbas Azari, Sakineh Nikzad, Arash Yazdani, Faezeh Atri, Abbas Fazel Anvari-Yazdi

Publisher page

Abstract

The poor bonding strength of zirconia to different dental substrates is one of the challenging issues in restorative dentistry. Hydroxyapatite is an excellent biocompatible material with fine bonding properties. In this study, it was hypothesized that hydroxyapatite coating on zirconia would improve its bond strength. Forty-five zirconia blocks were prepared and randomly divided into three groups: hydroxyapatite coating, sandblasting, and no preparation (control). The blocks were bonded to cement and the micro-shear bond strength was measured following load application. The bond strength values were analyzed with the Kruskal-Wallis test in 3 groups and paired comparisons were made using the Mann-Whitney U test. The failure patterns of the specimens were studied by a stereomicroscope and a scanning electron microscope and then analyzed by the chi-square test (significance level = 0.05). Deposition of hydroxyapatite on the zirconia surface significantly improved its bond strength to the resin cement in comparison with the control specimens (p < 0.0001). Also, the bond strength was similar to the sandblasted group (p = 0.34). The sandblasted and control group only showed adhesive failure, but the hydroxyapatite coated group had mixed failures, indicating the better quality of bonding (p < 0.0001). As a final point, hydroxyapatite coating on the zirconia surface improved the bond strength quality and values.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Luthardt RG, Sandkuhl O, Reitz B. Zirconia-TZP and alumina-advanced technologies for the manufacturing of single crowns. Eur J Prosthodont Restor Dent. 1999;7:113–9.
2. Blatz MB, Sadan A, Kern M. Resin-ceramic bonding: a review of the literature. J Prosthet Dent. 2003;89:268–74.10.1067/mpr.2003.50 ↗
3. Blatz MB, Sadan A, Arch GH Jr, Lang BR. In vitro evaluation of long-term bonding of procera all ceram alumina restorations with modified resin luting agent. J Prosthet Dent. 2003;89:381–7.10.1067/mpr.2003.89 ↗
4. Lung CY, Matinlinna JP. Aspects of silane coupling agents and surface conditioning in dentistry: an overview. Dent Mater. 2012;28:467–777.10.1016/j.dental.2012.02.009 ↗
5. Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent. 2002;2:139–47.
6. Wegner SM, Gerdes W, Kern M. Effect of different artificial aging conditions on ceramic-composite bond strength. Int J Prosthodont. 2002;15:267–72.
7. Dérand P, Dérand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont. 2000;13:131–5.
8. Matinlinna JP, Heikkinen T, Ozcan M, Lassila LV, Vallittu PK. Evaluation of resin adhesion to zirconia ceramic using some organosilanes. Dent Mater. 2006;22:824–31.10.1016/j.dental.2005.11.035 ↗
9. Heikkinen TT, Lassila LV, Matinlinna JP, Vallittu PK. Effect of operating air pressure on tribochemical silica-coating. Acta Odontol Scand. 2007;65:241–8.10.1080/00016350701459753 ↗
10. Bielen V, Inokoshi M, Munck JD, Zhang F, Vanmeensel K, Minakuchi S, Vleugels J, Naert I, Van Meerbeek B. Bonding effectiveness to differently sandblasted dental zirconia. J Adhes Dent. 2015;17(3):235–42.
11. Janda R, Roulet JF, Wulf M, Tiller HJ. A new adhesive technology for all-ceramics. Dent Mater. 2003;19:567–73.10.1016/S0109-5641(02)00106-9 ↗
12. Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials. J Prosthet Dent. 2007;98:379–88.10.1016/S0022-3913(07)60123-1 ↗
13. Casucci A, Monticelli F, Goracci C, Mazzitelli C, Cantoro A, Papacchini F, et al. Effect of surface pretreatments on the zirconia ceramic-resin cement microtensile bond strength. Dent Mater J. 2011;27:1024–30.10.1016/j.dental.2011.07.002 ↗
14. Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater. 1998;14:64–71.10.1016/S0109-5641(98)00011-6 ↗
15. Huang SB, Gao SS, Yu HY. Effect of Nano-hydroxyapatite concentration on remineralization of initial enamel lesion in vivo. Biomed Mater. 2009;4:314–41.
16. McGrann RTR, Greving DJ, Shadley JR, Rybicki EF, Kruecke TL, Bodger BE. The effect of coating residual stress on the fatigue life of thermal spray coated steel and aluminum. Surf Coat Tech. 1998;108-9:59–64.10.1016/S0257-8972(98)00665-3 ↗
17. Lee TM, Wang BC, Yang YC, Chang E, Yang CY. Comparison of plasma-sprayed hydroxyapatite coatings and hydroxyapatite/tricalcium phosphate composite coatings: in vivo study. J Biomed Mater Res. 2001;55:360–7.10.1002/1097-4636(20010605)55:3<360::AID-JBM1040>3.0.CO;2-Q ↗
18. Groot K, Wolke JG, Jansen JA. Calcium phosphate coatings for medical implants. Proc Inst Mech Eng H. 1998;212:137–47.10.1243/0954411981533917 ↗
19. Jin SD, Um SC, Lee JK. Surface modification of zirconia substrate by calcium phosphate particles using sol-gel method. J Nanosci Nanotechnol. 2015;15(8):5946–50.10.1166/jnn.2015.10439 ↗
20. Seo DS, Chae HC, Lee JK. Fabrication and microstructure of hydroxyapatite coatings on zirconia by room temperature spray process. J Nanosci Nanotechnol. 2015;15(8):6039–43.10.1166/jnn.2015.10440 ↗
21. Cho Y, Hong J, Ryoo H, Kim D, Park J, Han J. Osteogenic responses to zirconia with hydroxyapatite coating by aerosol deposition. J Dent Res. 2015;94(3):491–9.10.1177/0022034514566432 ↗
22. Patial SR, Dahotre NB. Calcium phosphate coatings for bio-implant applications: materials, performance factors, and methodologies. Mater Sci Eng. 2009;66:1–70.10.1016/j.mser.2009.05.001 ↗
23. Fazan F, Marquis PM. Dissolution behavior of plasma-sprayed hydroxyapatite coatings. J Mater Sci: Mater Med. 2000;11:787–92.
24. Moezzyzadeh M, Nojehdehyan H, Valizadeh Haghi H. The effect of different coating methods or resin bond strength to zirconia. J Dent Sch. 2013;31:22–30.
25. Tsukakoshi M, Shinya A, Gomi H, Lassila LV, Vallittu PK, Shinya A. Effects of dental adhesive cement and surface treatment on bond strength and leakage of zirconium oxide ceramics. Dent Mater J. 2008;27:159–71.10.4012/dmj.27.159 ↗
26. Kern M, Barloi A, Yang B. Surface conditioning influences zirconia ceramic bonding. J Dent Res. 2009;88:817–22.10.1177/0022034509340881 ↗
27. Blatz MB, Phark JH, Ozer F, Mante FK, Saleh N, Bergler M. In vitro comparative bond strength of contemporary self-adhesive resin cements to zirconium oxide ceramic with and without air-particle abrasion. Clin Oral Investig. 2010;14:187–92.10.1007/s00784-009-0278-0 ↗
28. Inokoshi M, De Munck J, Minakuchi S, Van Meerbeek B. Meta-analysis of bonding effectiveness to zirconia ceramics. J Dent Res. 2014;93(4):329–34.10.1177/0022034514524228 ↗
29. Aboushelib MN, Ghoneim M, Mirmohammadi H, Salameh Z. General principles for achieving adequate bond to all ceramic restorations. J Dent Oral Hyg. 2009;1:36–41.
30. Borges GA, Spohr AM, de Goes MF, Sobrinho LC, Chan DC. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics. J Prosthet Dent. 2003;89:479–88.10.1016/S0022-3913(02)52704-9 ↗
31. Lüthy J, Loeffel O, Hammerle CHF. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater. 2006;22:195–200.10.1016/j.dental.2005.04.016 ↗
32. Usumez A, Hamdemirci N, Koroglu BY, Simsel I, Parlar O, Sari T. Bond strength of resin cement to zirconia ceramic with different surface treatments. Lasers Med Si. 2013;28:259–66.10.1007/s10103-012-1136-x ↗
33. Sato H, Yamada K, Pezzotti G, Nowa M, Ban S. Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment. Dent Mater J. 2008;27:408–14.10.4012/dmj.27.408 ↗
34. Curtis AR, Wright AJ, Fleming GJP. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic. J Dent. 2006;34:195–206.10.1016/j.jdent.2005.06.006 ↗
35. Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of YTZP dental ceramic. J Dent. 2005;33:9–18.10.1016/j.jdent.2004.07.001 ↗
36. Zhang Y, Lawn BR, Rekow ED, Thompson VP. Effect of sandblasting on the long term performance of dental ceramics. J Mater Res B Appl Biomater. 2004;71:381–6.10.1002/jbm.b.30097 ↗
37. Liu D, Tsoi JK, Matinlinna JP, Wong HM. Effects of some chemical surface modifications on resin zirconia adhesion. J Mech Behav Biomed Mater. 2015;46:23–30.10.1016/j.jmbbm.2015.02.015 ↗
38. Labella R, Braden M, Deb S. Novel hydroxyapatite-based dental composites. Biomater. 1994;15:1197–1200.10.1016/0142-9612(94)90269-0 ↗
39. Lemons J. Hydroxyapatite coatings. Clin Orthop. 1988;235:220–30.10.1097/00003086-198810000-00021 ↗
40. Guo L, Huang M, Zhang X. Effects of sintering temperature on structure of hydroxyapatite studied with rietveld method. J Mater Sci Mater Med. 2003;14:817–22.10.1023/A:1025048724330 ↗
41. Ramos GF, Pereira GK, Amaral M, Valandro LF, Bottino MA. Effect of grinding and heat treatment on the mechanical behavior of zirconia ceramic. Brazilian Oral Res. 2016;30:22–28.10.1590/1807-3107BOR-2016.vol30.0012 ↗
42. Wang T, Nikaido T, Nakabayashi N. Photocure bonding agent containing phosphoric methacrylate. Dent Mater. 1991;7:59–62.10.1016/0109-5641(91)90029-X ↗