Abstract

The susceptibility to the fouling of the NiTi and Ti6Al4V alloys due to the adhesion of microorganisms and the biofilm formation is very significant, especially in the context of an inflammatory state induced by implants contaminated by bacteria, and the implants corrosion stimulated by bacteria. The aim of this work was to examine the differences between the sulphur-oxidizing bacteria (SOB) and sulphate-reducing bacteria (SRB) strains in their affinity for NiTi and Ti6Al4V alloys. The biofilms formed on alloy surfaces by the cells of five bacterial strains (aerobic SOB Acidithiobacillus thiooxidans and Acidithiobacillus ferrooxidans, and anaerobic SRB Desulfovibrio desulfuricans-3 strains) were studied using scanning electron microscopy (SEM) and confocal laser scanning microscopy (CLSM). The protein concentrations in liquid media have also been analyzed. The results indicate that both alloys tested may be colonized by SOB and SRB strains. In the initial stage of the biofilm formation, the higher affinity of SRB to both the alloys has been documented. However, the SOB strains have indicated the higher (although differentiated) adaptability to changing environment as compared with SRB. Stimulation of the SRB growth on the alloys surface was observed during incubation in the liquid culture media supplemented with artificial saliva, especially of lower pH (imitated conditions under the inflammatory state, for example in the periodontitis course). The results point to the possible threat to the human health resulting from the contamination of the titanium implant alloys surface by the SOB (A. thiooxidans and A. ferrooxidans) and SRB (D. desulfuricans).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Corrosion Behavior and Inhibition · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Leyens C, Peters M, editors. Titanium and titanium alloys. Fundamentals and applications. Weinheim: Wiley; 2003. https://doi.org/10.1002/3527602119.10.1002/3527602119 ↗
2. Oryshchenko AS, Gorynin IV, Leonov VP, Kudryavtsev AS, Mikhailov VI, Chudakov EV. Marine titanium alloys: present and future. Inorg Mater Appl Res. 2015;6:571–7910.1134/S2075113315060106 ↗
3. Williams JC. Titanium alloys: processing, properties, and applications. In: Encyclopedia of aerospace engineering, Online ©, Wiley; 2010. https://doi.org/10.1002/9780470686652.eae214.10.1002/9780470686652.eae214 ↗
4. Singh R, Dahotre NB. Corrosion degradation and prevention by surface modification of biometallic materials. J Mater Sci Mater Med. 2007;18:725–51.10.1007/s10856-006-0016-y ↗
5. Liu X, Chu PK, Ding C. Surface modification of titanium, titanium alloys, and related materials for biomedical applications. Mater Sci Eng. 2004;R 47:49–121. https://doi.org/10.1016/j.mser.2004.11.001 .10.1016/j.mser.2004.11.001 ↗
6. Beech IB, Sunner J. Biocorrosion: towards understanding interactions between biofilms and metals. Curr Opin Biotechnol. 2004;15:181–6.10.1016/j.copbio.2004.05.001 ↗
7. Li K, Whitfield M, Van Vliet KJ. Beating the bugs: roles of microbial biofilms in corrosion. Corros Rev. 2013;31:73–84.10.1515/corrrev-2013-0019 ↗
8. Zhang SM, Qiu J, Tian F, Guo XK, Zhang FQ, Huang QF. Corrosion behavior of pure titanium in the presence of Actinomyces naeslundii. J Mater Sci Mater Med. 2013;24:1229–37.10.1007/s10856-013-4888-3 ↗
9. Scarano A, Piattelli M, Caputi S, Favero GA, Piattelli A. Bacterial adhesion on commercially pure titanium and zirconium oxide disks: an in vivo human study. J Periodontol. 2004;75:292–6.10.1902/jop.2004.75.2.292 ↗
10. Souza JCM, Henriques M, Teughels W, Ponthiaux P, Celis J-P, Rocha LA. Wear and corrosion interactions on titanium in oral environment: literature review. J Bio Tribo Corros. 2015; 1–13. https://doi.org/10.1007/s40735-015-0013-010.1007/s40735-015-0013-0 ↗
11. Ramya S, George RP, Subba Rao RV, Dayal RK. Detection of algae and bacterial biofilms formed on titanium surfaces using micro-Raman analysis. Appl Surf Sci. 2010;256:5108–15.10.1016/j.apsusc.2010.03.079 ↗
12. Chaturvedi TP. An overview of the corrosion aspect of dental implants (titanium and its alloys). Indian J Dent Res. 2009;20:91–8.10.4103/0970-9290.49068 ↗
13. Jorand FPA, Debuy S, Kamagate SF, Engels-Deutsch M. Evaluation of a biofilm formation by Desulfovibrio fairfieldensis on titanium implants. Lett Appl Microbiol. 2014. https://doi.org/10.1111/lam.12370 .10.1111/lam.12370 ↗
14. Huber B, Herzog B, Drewes JE, Koch K, Müller E. Characterization of sulfur oxidizing bacteria related to biogenic sulfuric acid corrosion in sludge digesters. BMC Microbiol. 2016;16:1–11.10.1186/s12866-016-0767-7 ↗
15. Horn J, Martin S, Masterson B. Evidence of biogenic corrosion of titanium after exposure to a continuous culture of Thiobacillus ferrooxidans grown in thiosulfate medium. NACE International, Corrosion; 2001. Paper No. 01259.10.5006/C2001-01259 ↗
16. Barton LL, Fauque GD. Biochemistry, physiology and biotechnology of sulfate-reducing bacteria. Adv Appl Microbiol. 2009;68:41–98.10.1016/S0065-2164(09)01202-7 ↗
17. Enning D, Garrelfs J. Corrosion of iron by sulfate-reducing bacteria: new views of an old problem. Appl Environ Microbiol. 2014;80:1226–36.10.1128/AEM.02848-13 ↗
18. Coetser SE, Cloete TE. Biofouling and biocorrosion in industrial water systems. Crit Rev Microbiol. 2005;31:213–32.10.1080/10408410500304074 ↗
19. Tang K, Baskaran V, Nemati M. Bacteria of the sulphur cycle: an overview of microbiology, biokinetics and their role in petroleum and mining industries. Biochem Eng J. 2009;44:73–94.10.1016/j.bej.2008.12.011 ↗
20. Rao TS, Kora AJ, Anupkumar SV, Narasimhan SV, Feser R. Pitting corrosion of titanium by a freshwater strain of sulphate reducing bacteria (Desulfovibrio vulgaris). Corros Sci. 2005;47:1071–1084.10.1016/j.corsci.2004.07.025 ↗
21. Maruthamuthu S, Rajasekar A, Sathiyanarayanan S, Muthukumar N, Palaniswamy N. Electrochemical behaviour of microbes on orthodontic wires. Curr Sci. 2005;89:988–96.
22. Simka W, Kaczmarek M, Baron-Wiecheć A, Nawrat G, Marciniak J, Żak J. Electropolishing and passivation of NiTi shape memory alloy. Electrochim Acta. 2010;55:2437–41.10.1016/j.electacta.2009.11.097 ↗
23. Cwalina B, Jaworska-Kik M. Sulphur- and iron-oxidizing activities of bacteria isolated from zinc-lead flotation tailings. Ecol Chem Eng A. 2008;15:35–9.
24. Dzierżewicz Z, Cwalina B, Gawlik B, Wilczok T, Gonciarz Z. Isolation and evaluation of susceptibility to sulphasalazine of Desulfovibrio desulfuricans strains from the human digestive tract. Acta Microbiol Pol. 1997;46:175–87.
25. Bisson-Boutelliez C, Massin F, Dumas D, Miller N, Lozniewski A. Desulfovibrio spp. survive within KB cells and modulate inflammatory responses. Mol Oral Microbiol. 2010;25:226–35.10.1111/j.2041-1014.2009.00550.x ↗
26. Langendijk PS, Hanssen JTJ, Van der Hoeven JS. Sulfate-reducing bacteria in association with human periodontitis. J Clin Periodontol. 2000;27:943–50.10.1034/j.1600-051x.2000.027012943.x ↗
27. Duffo GS, Quezada Castillo EQ. Development of an artificial saliva solution for studying the corrosion behavior of dental alloys. Corrosion. 2004;60:594–602.10.5006/1.3287764 ↗
28. Mareci D, Chelariu R, Gordin DM, Ungureanu G, Gloriant T. Comparison corrosion study of Ti-Ta alloys for dental applications. Acta Biomater. 2009;5:3625–39.10.1016/j.actbio.2009.05.037 ↗
29. Karnovsky MJ. A formaldehyde-glutaraldehyde fixative of high osmolality for use in electron microscopy. J Cell Biol. 1965;27:137A.
30. Ismail F, Eisenburger M, Grade S, Stiesch M. In situ biofilm formation on titanium, gold alloy and zirconia abutment materials. Dentistry. 2016;6:400.10.4172/2161-1122.1000400 ↗
31. Bergey’s Manual of Systematics of Archaea and Bacteria, Online © Bergey’s Manual Trust. Genus Acidithiobacillus. In: Proteobacteria, Gammaproteobacteria, Acidithiobacillales, Acidithiobacillaceae; 2015. https://doi.org/10.1002/9781118960608.gbm01079 .10.1002/9781118960608.gbm01079 ↗
32. Bergey’s Manual of Systematics of Archaea and Bacteria, Online © Bergey’s Manual Trust. Genus Desulfovibrio. In: Proteobacteria, Deltaproteobacteria, Desulfovibrionales, Desulfovibrionaceae; 2015. https://doi.org/10.1002/9781118960608.gbm01035 .10.1002/9781118960608.gbm01035 ↗
33. Young KD. The selective value of bacterial shape. Microbiol Mol Biol Rev. 2006;70:660–703.10.1128/MMBR.00001-06 ↗
34. Lemire JA, Joe J, Harrison JJ, Turner RJ. Antimicrobial activity of metals: mechanisms, molecular targets and applications. Nat Rev Microbiol. 2013;11:371–84.10.1038/nrmicro3028 ↗
35. Rawlings DE. Characteristics and adaptability of iron- and sulfur-oxidizing microorganisms used for the recovery of metals from minerals and their concentrates. Microb Cell Fact. 2005;4(13):1–15. https://doi.org/10.1186/1475-2859-4-13 .10.1186/1475-2859-4-13 ↗
36. Robichaux M, Howell M, Boopathy R. Growth and activities of sulfate-reducing and methanogenic bacteria in human oral cavity. Curr Microbiol. 2003;47:12–16.10.1007/s00284-002-3930-3 ↗
37. Cwalina B, Dec W, Simka W, Michalska J, Jaworska-Kik M. Biofilm formation on NiTi surface by different strains of sulphate reducing bacteria (Desulfovibrio desulfuricans). Solid State Phenom. 2015;227:302–05. www.scientific.net/SSP.227.302.10.4028/www.scientific.net/SSP.227.302 ↗
38. Lopes FA, Morin P, Oliveira R, Melo LF. The influence of nickel on the adhesion ability of Desulfovibrio desulfuricans. Colloids Surf B. 2005;46:127–33.10.1016/j.colsurfb.2005.07.020 ↗
39. Dzierżewicz Z, Cwalina B, Chodurek E, Wilczok T. The relationship between microbial metabolic activity and biocorrosion of carbon steel. Res Microbiol. 1997;148:785–93.10.1016/S0923-2508(97)82454-0 ↗
40. Eliades T, Athanasiou AE. In vivo aging of orthodontic alloys: implications for corrosion potential, nickel release, and biocompatibility. Angle Orthod. 2002;72:222–37. https://doi.org/10.1043/0003-3219(2002)072<0222:IVAOOA>2.0.CO;2.
41. Drescher K, Dunkel J, Nadell CD, van Teeffelen S, Grnja I, Wingreen NS, Stone HA, Bassler BL. Architectural transitions in Vibrio cholerae biofilms at single-cell resolution. Proc Natl Acad Sci. 2016;113:E2066–72.10.1073/pnas.1601702113 ↗
42. Lambert G, Bergman A, Zhang Q, Bortz D, Austin R. Physics of biofilms: the initial stages of biofilm formation and dynamics. New J Phys. 2014;16:045005.10.1088/1367-2630/16/4/045005 ↗
43. Marshall KC, Cruickshank RS. Cell surface hydrophobicity and the orientation of certain bacteria at interfaces. Arch Microbiol. 1973;91:29–40.
44. Katsikogianni M, Missirlis YF. Concise review of mechanisms of bacterial adhesion to biomaterials and of techniques used in estimating bacteria–material interactions. Eur Cell Mater. 2004;8:37–57.10.22203/eCM.v008a05 ↗
45. Goldstein EJ, Citron DM, Peraino VA, Cross SA. Desulfovibrio desulfuricans bacteremia and review of human Desulfovibrio infections. J Clin Microbiol. 2003;41:2752–4.10.1128/JCM.41.6.2752-2754.2003 ↗
46. Hagiwara S, Yoshida A, Omata Y, Tsukada Y, Takahashi H, Kamewada H, Koike S, Okuzumi K, Hishinuma A, Kobayashi K, Nakano M. Desulfovibrio desulfuricans bacteremia in a patient hospitalized with acute cerebral infarction: case report and review. J Infect Chemother. 2014;20:274–7.10.1016/j.jiac.2013.10.009 ↗
47. Singh SB, Lin HC. Hydrogen sulfide in physiology and diseases of the digestive tract. Microorganisms. 2015;3:866–89.10.3390/microorganisms3040866 ↗
48. Kroes I, Leep PW, Relman DA. Bacterial diversity within the human subgingival crevice. Proc Natl Acad Sci. 1999;96:14547–52. PMCID:PMC24473.10.1073/pnas.96.25.14547 ↗
49. Hunter MC, Pozhitkov AE, Noble PA. Microbial signatures of oral dysbiosis, periodontitis and edentulism revealed by gene meter methodology. J Microbiol Methods. 2016;131:85–101.10.1016/j.mimet.2016.09.019 ↗
50. Gopal J, Muraleedharan P, Sarvamangala H, George RP, Dayal RK, Tata BVR, Khatak HS, Natarajan KA. Biomineralisation of manganese on titanium surfaces exposed to seawater. Biofouling. 2008;24:275–82.10.1080/08927010802056467 ↗