journal article·2011-12

Influence of topographical features on the fluoride corrosion of Ni–Ti orthodontic archwires

C. Abalos, A. Paúl, A. Mendoza, E. Solano, F. J. Gil

Publisher page

Abstract

Different manufacturing processes of Ni-Ti archwires respond differently to corrosion due to the surface conditions involved. In this study, several topographical features and their influence upon fluoride corrosion were studied. Four topographies (smooth, dimple, scratch, and crack) according to the main surface defect were characterized (n = 40). Static corrosion tests were performed in artificial saliva with fluorated prophylactic gel (12500 ppm) for 28 days. The surface was characterized by SEM and laser confocal microscopy. Standard electrochemical corrosion (open circuit potential, corrosion potential and corrosion current density) was performed. Statistical analysis was carried out using the ANOVA test (α ≤ 0.05). An increase was observed in the surface defects and/or roughness of the cracked and scratched surfaces. These defects produced an important increase in corrosion behavior. The best surfaces for the orthodontic archwires were the smooth and dimpled surfaces, respectively. The increase in defects was independent of roughness. Manufacturing processes that produce surface cracks should be avoided in orthodontic applications.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Kusy RP. A review of contemporary archwires: their properties and characteristics. Angle Orthod. 1997;67(3):197–207.
2. Torrisi L. The Ni–Ti superelastic alloy application to the dentistry field. Biomed Mater Eng. 1999;1:39–47.
3. Wever DJ, Veldhuizen AG, de Vries J, Busscher HJ, Uges DR, van Horn JR. Electrochemical and surface characterization of a nickel–titanium alloy. Biomaterials. 1998;19(7–9):761–9.10.1016/S0142-9612(97)00210-X ↗
4. Huang HH. Variation in corrosion resistance of nickel–titanium wires from different manufacturers. Angle Orthod. 2005;75(4):661–5.
5. Huang HH, Chiu YH, Lee TH, Wu SC, Yang HW, Su KH, et al. Ion release from Ni–Ti orthodontic wires in artificial saliva with various acidities. Biomaterials. 2003;20:3585–92.10.1016/S0142-9612(03)00188-1 ↗
6. Wang J, Li N, Rao G, Han EH, Ke W. Stress corrosion cracking of Ni–Ti in artificial saliva. Dent Mater. 2007;23(2):133–7.10.1016/j.dental.2006.01.001 ↗
7. Li X, Wang J, Han EH, Ke W. Influence of fluoride and chloride on corrosion behavior of Ni–Ti orthodontic wires. Acta Biomater. 2007;3(5):807–15.10.1016/j.actbio.2007.02.002 ↗
8. Huang HH. Variation in surface topography of different Ni–Ti orthodontic archwires in various commercial fluoride-containing environments. Dent Mater. 2007;23(1):24–33.10.1016/j.dental.2005.11.042 ↗
9. Lee TH, Huang TK, Lin SY, Chen LK, Chou MY, Huang HH. Corrosion resistance of different nickel–titanium archwires in acidic fluoride-containing artificial saliva. Angle Orthod. 2010;80(3):547–53.10.2319/042909-235.1 ↗
10. Kwon YH, Cheon YD, Seol HJ, Lee JH, Kim HI. Changes on Ni–Ti orthodontic wired due to acidic fluoride solution. Dent Mater J. 2004;23(4):557–65.10.4012/dmj.23.557 ↗
11. Ramalingam A, Kailasam V, Padmanabhan S, Chitharanjan A. The effect of topical fluoride agents on the physical and mechanical properties of Ni–Ti and copper Ni–Ti archwires. An in vivo study. Aust Orthod J. 2008;24(1):26–31.
12. Kwon YH, Jang CM, Jang JH, Park JH, Kim TH, Kim HI. Effect of fluoride released from fluoride-containing dental restoratives on Ni–Ti orthodontic wires. Dent Mater J. 2008;27(1):133–8.10.4012/dmj.27.133 ↗
13. Widu F, Drescher D, Junker R, Bourauel C. Corrosion and biocompatibility of orthodontic wires. J Mater Sci Mater Med. 1999;10(5):275–81.10.1023/A:1008953412622 ↗
14. Schiff N, Grosgogeat B, Lissac M, Dalard F. Influence of fluoride content and pH on the corrosion resistance of titanium and its alloys. Biomaterials. 2002;23(9):1995–2002.10.1016/S0142-9612(01)00328-3 ↗
15. Yokoyama K, Kaneko K, Moriyama K, Asaoka K, Sakai J, Nagumo M. Hydrogen embrittlement of Ni–Ti superelastic alloy in fluoride solution. J Biomed Mater Res A. 2003;65(2):182–7.10.1002/jbm.a.10457 ↗
16. Walker MP, White RJ, Kula KS. Effect of fluoride prophylactic agents on the mechanical properties of nickel–titanium-based orthodontic wires. Am J Orthod Dentofac Orthop. 2005;127(6):662–9.10.1016/j.ajodo.2005.01.015 ↗
17. Watanabe I, Watanabe E. Surface changes induced by fluoride prophylactic agents on titanium-based orthodontic wires. Am J Orthod Dentofac Orthop. 2003;123(6):653–6.10.1016/S0889-5406(03)00197-5 ↗
18. Schiff N, Boinet M, Morgon L, Lissac M, Dalard F, Grosgogeat B. Galvanic corrosion between orthodontic wires and brackets in fluoride mouthwashes. Eur J Orthod. 2006;28(3):298–304.10.1093/ejo/cji102 ↗
19. Schiff N, Grosgogeat B, Lissac M, Dalard F. Influence of fluoridated mouthwashes on corrosion resistance of orthodontics wires. Biomaterials. 2004;25(19):4535–42.10.1016/j.biomaterials.2003.11.042 ↗
20. Nakagawa M, Matsuya S, Shiraishi T, Ohta M. Effect of fluoride concentration and pH on corrosion behavior of titanium for dental use. J Dent Res. 1999;78(9):1568–72.10.1177/00220345990780091201 ↗
21. Es-Souni M, Es-Souni M, Fischer-Brandies H. On the properties of two binary Ni–Ti shape memory alloys. Effects of surface finish on the corrosion behaviour and in vitro biocompatibility. Biomaterials. 2002;23(14):2887–94.10.1016/S0142-9612(01)00416-1 ↗
22. Wichelhaus A, Geserick M, Hibst R, Sander FG. The effect of surface treatment and clinical use on friction in Ni–Ti orthodontic wires. Dent Mate. 2005;21(10):938–45.10.1016/j.dental.2004.11.011 ↗
23. Oshida Y, Sachdeva RC, Miyazaki S. Microanalytical characterization and surface modification of TiNi orthodontic archwires. Biomed Mater Eng. 1992;2(2):51–69.
24. Trepanier C, Tabrizian M, Yahia LH, Bilodeau L, Piron DL. Effect of modification of oxide layer on Ni–Ti stent corrosion resistance. J Biomed Mater Res. 1998;43(4):433–40.10.1002/(SICI)1097-4636(199824)43:4<433::AID-JBM11>3.0.CO;2-# ↗
25. Es-Souni M, Fischer-Brandies H, Kock N, Bock O, Rätzke K. Chemische Zusammensetzung, Umwandlungsverhalten und mechanische Biegeeigenschaften ausgewählter kieferorthopädischer Ni–Ti-Drahtbögen. IOK. 2001;33:87–106.
26. Paúl A, Ábalos C, Mendoza A, Solano E, Gil FJ. Relationship between the surface defects and the manufacturing process of orthodontic Ni–Ti archwires. Mater Lett. 2011;65(1):3358–3361.10.1016/j.matlet.2011.07.088 ↗
27. Shabalovskaya SA, Anderegg J, Laab F, Thiel PA, Rondelli G. Surface conditions of nitinol wires, tubing, and as-cast alloys. The effect of chemical etching, aging in boiling water, and heat treatment. J Biomed Mater Res B Appl Biomater. 2003;65(1):193–203.10.1002/jbm.b.10001 ↗
28. Prososki RR, Bagby MD, Erickson LC. Static frictional force and surface roughness of nickel–titanium arch wires. Am J Orthod Dentofac Orthop. 1991;100(4):341–8.10.1016/0889-5406(91)70072-5 ↗
29. Shabalovskaya S, Anderegg J, Van Humbeeck J. Critical overview of Nitinol surfaces and their modifications for medical applications. Acta Biomater. 2008;4(3):447–67.10.1016/j.actbio.2008.01.013 ↗
30. Grimsdottir MR, Hensten-Pettersen A. Surface analysis of nickel–titanium archwire used in vivo. Dent Mater. 1997;13(3):163–7.10.1016/S0109-5641(97)80118-2 ↗
31. Wu W, Liu X, Han H, Yang D, Lu S. Electropolishing of NiTi for improving biocompatibility. J Mater Sci Tech. 2008;24:926–30.
32. Hunt NP, Cunningham SJ, Golden CG, Sheriff M. An investigation into the effects of polishing on surface hardness and corrosion of orthodontic archwires. Angle Orthod. 1999;69(5):433–40.
33. Huang HH. Surface characterizations and corrosion resistance of nickel–titanium orthodontic archwires in artificial saliva of various degrees of acidity. J Biomed Mater Res A. 2005;74(4):629–39.10.1002/jbm.a.30340 ↗
34. Eliades T, Eliades G, Athanasiou AE, Bradley TG. Surface characterization of retrieved Ni–Ti orthodontic archwires. Eur J Orthod. 2000;22(3):317–26.10.1093/ejo/22.3.317 ↗