Synthesis, extrusion and rheological behaviour of PU/HA composites for biomedical applications
Source abstract
Abstract
Biostable polyurethane/hydroxyapatite (PU/HA) composites with potential application as bone replacement materials were synthesized in bulk and processed in a screw extruder. The polyurethanes (PU) were prepared by reacting an aliphatic diisocyanate, 4-methylene-bis-diisocyanate (MDI), with poly-(epsilon-caprolactone) (PCL) diols and polytetramethylene oxide (PTMO) of different molecular weights, extended with 1, 4-butanediol (BDO). Glass-transition temperatures were measured by differential scanning calorimetry (DSC). The specific PU groups were assessed by total reflectance-Fourier transform infrared spectroscopy (ATR-FTIR). The effects of polymer chemistry and filler content on the rheological behaviour were studied by oscillatory rheometry. Polymers with larger chain lengths showed higher viscosity and, for identical chain lengths, polyether urethanes seem to have higher viscosities than polyester based urethanes. A lubricating effect was found for composites containing 50% weight of filler, whereas at higher filler contents a solid-like behaviour was measured. Polymer chemistry seems to be affected by ageing but not so by the presence of filler. Ageing is characterized by a decrease in the concentration of hydrogen bonds involving between urethane linkages.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Polymer composites and self-healing · biodegradable polymer synthesis and properties · Polymer Nanocomposites and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Liu Q, de Wijn JR, van Blitterswijk CA. A study on the grafting reaction of isocyanates with hydroxyapatite particles. J Biomed Mater Res. 1998;40:358–64.10.1002/(SICI)1097-4636(19980605)40:3<358::AID-JBM3>3.0.CO;2-E ↗
2. That PT, Tanner KE, Bonfield W. Fatigue characterization of a hydroxyapatite-reinforced polyethylene composite. I. Uniaxial fatigue. J Biomed Mater Res. 2000;51:453–60.10.1002/1097-4636(20000905)51:3<453::AID-JBM20>3.0.CO;2-Q ↗
3. Di Silvio L, Dalby MJ, Bonfield W. Osteoblast behaviour on HA/PE composite surfaces with different HA volumes. Biomaterials. 2002;23:101–7.10.1016/S0142-9612(01)00084-9 ↗
4. Dalby MJ, Bonfield W, Di Silvio L. Enhanced HAPEX topography: comparison of osteoblast response to established cement. J Mater Sci Mater Med. 2003;14:693–7.10.1023/A:1024959632082 ↗
5. Ladizesky NH, Ward IM, Bonfield W. Hydrostatic extrusion of polyethylene filled with hydroxyapatite. Polym Adv Technol. 1997;8:496–504.10.1002/(SICI)1099-1581(199708)8:8<496::AID-PAT676>3.0.CO;2-R ↗
6. Wang M, Hench LL, Bonfield W. Bioglass/hight density polyethylene composite for soft tissue applications: preparation and evaluation. J Biomed Mater Res. 1998;42:577–86.10.1002/(SICI)1097-4636(19981215)42:4<577::AID-JBM14>3.0.CO;2-2 ↗
7. Matheson LA, Labow RS, Santerre JP. Biodegradation of polycarbonate-based polyurethanes by the human monocyte-derived macrophage and U937 cell systems. J Biomed Mater Res. 2002;61:505–13.10.1002/jbm.10286 ↗
8. Guan J, Sacks MS, Beckman EJ, Wagner WR. Synthesis, characterization, and cytocompatibility of elastomeric, biodegradable poly(ester-urethane)ureas based on poly(caprolactone) and putrescine. J Biomed Mater Res. 2002;61:493–503.10.1002/jbm.10204 ↗
9. Pinto UA, Visconte LLY, Nunes RCR. Mechanical properties of thermoplastic polyurethane elastomers with mica and aluminium trihydrate. Eur Polym J. 2001;37:1935–7.10.1016/S0014-3057(01)00069-6 ↗
10. Finnigan B, Martin D, Halley P, Truss R, Campbell K. Morphology and properties of thermoplastic polyurethane nanocomposites incorporating hydrophilic layered silicates. Polymer. 2004;45:2249–60.10.1016/j.polymer.2004.01.049 ↗
11. Farè S, Valtulina V, Petrini P, Alessandrini E, Pietrocola G, Tanzi MC, Speziale P, Visai L. In vitro interaction of human fibroblasts and platelets with a shape memory polyurethane. J Biomed Mater Res. 2005;73A:1–11.10.1002/jbm.a.30193 ↗
12. Christenson EM, Anderson JM, Hiltner A. Oxidative mechanisms of poly(carbonate urethane) and poly(ether urethane) biodegradation: in vivo and in vitro correlations. J Biomed Mater Res. 2004;70A:245–55.10.1002/jbm.a.30067 ↗
13. Veleva AN, Khan SA, Cooper SL. Oxidative and hydrolytic stability of a novel acrylic thermopolymer for biomedical applications. J Biomed Mater Res. 2005;74A:117–23.10.1002/jbm.a.30349 ↗
14. Schubert MA, Wiggins MJ, Anderson JM, Hiltner A. Role of oxygen in biodegradation of poly(etherurethaneurea) elastomers. J Biomed Mater Res. 1997;34:519–30.10.1002/(SICI)1097-4636(19970315)34:4<519::AID-JBM12>3.0.CO;2-7 ↗
15. Roeder RK, Sproul MM, Turner CH. Hydrpxyapatie whiskers provide improved mechanical properties in reinforced polymer composites. J Biomed Mater Res. 2003;67A:801–12.10.1002/jbm.a.10140 ↗
16. Yu R, Tan TH, Kong AN. Butylated hydroxyanisole and its metabolite tert-butylhydroquinone differentially regulate mitogen-activated protein kinases. The role of oxidative stress in the activation of mitogen-activated protein kinases by phenolic antioxidants. J Biol Chem. 1997;272:28962–70.10.1074/jbc.272.46.28962 ↗
17. Yu R, Mandlekar S, Kong AN. Molecular mechanisms of butylated hydroxylanisole-induced toxicity: induction of apoptosis through direct release of cytochrome c. Mol Pharmacol. 2000;58:431–7.10.1124/mol.58.2.431 ↗
18. US. Food and Drug Administration (2006).
19. Kalus WH , Münzner R, Filby WG. The reaction of butylated hydroxyanisole and its metabolites with some arylamines: investigations of product mutagenicity. Environ Health Persp. 1994;102:1.10.1289/ehp.9410296 ↗
20. Kahl R. Synthetic antioxidants: biochemical actions and interference with radiation, toxic compounds, chemical mutagens and chemical carcinogens. Toxicology 1984;33:185–228.10.1016/0300-483X(84)90038-6 ↗
21. Kahl R, Weinke S, Kappus H. Production of reactive oxygen species due to metabolic activation of butylated hydroxyanisole. Toxicology (1989);59:179–94.10.1016/0300-483X(89)90056-5 ↗
22. Szycher M. Szycher’s handbook of polyurethanes. New York, Washington: CRC Press; 1999.10.1201/9781482273984 ↗
23. Gorna K, Gogolewski S. Synthesis and characterization of biodegradable poly(-caprolactone urethane)s. I. Effect of the polyol molecular weight, catalyst, and chain extender on the molecular and physical characteristics. J Polym Sci A Polym Chem. 2002;40:156–70.10.1002/pola.10096 ↗
24. Gorna K, Gogolewski S. Biodegradable polyurethanes for implants. II. In vitro degradation and calcification of materials from poly(ε-caprolactone)-poly(ethylene oxide) diols and various chain extenders. J Biomed Mater Res. 2002;60:592–606.10.1002/jbm.10100 ↗
25. Srichatrapimuk VW, Cooper SL. Infrared thermal analysis of polyurethane block polymers. J Macromol Sci B Phys. 1978;15:267–311.10.1080/00222347808212599 ↗
26. Bellamy LJ. The infrared spectra of complex molecules. London: Chapman and Hall; 1975.10.1007/978-94-011-6017-9 ↗
27. Khan I, Smith N, Jones E, Finch DS, Cameron RE. Analysis and evaluation of a biomedical polycarbonate urethane tested in an in vitro study and an ovine arthoplasty model. Part I: materials selection and evaluation. Biomaterials. 2005;26:621–31.10.1016/j.biomaterials.2004.02.065 ↗
28. Ho SP, Nakabayashi N, Iwasaki Y, Boland T, LaBerge M. Frictional properties of poly(MPC-co-BMA) phospholipid polymer for catheter applications. Biomaterials. 2003;24:5121–9.10.1016/S0142-9612(03)00450-2 ↗
29. Chen H, Jiang X, He L, Zhang T, Xu M, Yu X. Novel biocompatible waterborne polyurethane using L-Lysine as an extender. J Appl Polym Sci. 2002;84:2474–80.10.1002/app.10568 ↗
30. Skarja GA, Woodhouse KA. Structure-property relationships of degradable polyurethane elastomers containing an amino acid-based chain extender. J Appl Polym Sci. 2000;75:1522–34.10.1002/(SICI)1097-4628(20000321)75:12<1522::AID-APP11>3.0.CO;2-A ↗
31. Macosko C. Rheology—principles, measurements and applications. New York: Wiley-VCH; 1994.
32. Chryss AG, Bhattacharya SN, Pullum L. Rheology of shear thickening suspensions and the effects of wall slip in torsional flow. Rheol Acta. 2005;45:124.10.1007/s00397-005-0001-2 ↗
33. Denn MM. Extrusion instabilities and wall slip. Annu Rev Fluid Mech. 2001;33:265.10.1146/annurev.fluid.33.1.265 ↗
34. Mooney M, Wolstenholme WE. The rheological unit in raw elastomers. J Appl Phys. 1954;25:1098.10.1063/1.1721821 ↗
35. Bernardo CA, Van Hattum FWJ, Carneiro OS, Maia JM. The role of rheology in the processing of vapor grown carbon fiber/thermoplastic composites, NATO ASI series: carbon filaments and nanotubes: common origins, differing applications. Dordrecht: Kluwer Academic Publishers; 2001. p. 289.10.1007/978-94-010-0777-1_21 ↗
36. Joseph R, Martyn MT, Tanner KE, Coates PD. Interfacial stick-slip transition in hydroxyapatite filled high density polyethylene composite. Bull Mater Sci. 2006;29:85–9.10.1007/BF02709361 ↗
37. McGeary K. Mechanical packing of spherical particles. J Am Ceram Soc. 1961;44:513–22.10.1111/j.1151-2916.1961.tb13716.x ↗