journal article·2008-09

In vitro dissolution behavior of SiO2–MgO–Al2O3–K2O–B2O3–F glass–ceramic system

Shibayan Roy, Bikramjit Basu

Publisher page

Abstract

Herein, we report the results of the in vitro dissolution tests, which were carried out by immersing the selected glass-ceramic samples in artificial saliva (AS) for various time periods of up to 42 days. In our experiments, the SiO(2)-MgO-Al(2)O(3)-K(2)O-B(2)O(3)-F glass ceramics with different crystal morphology and crystal content were used and a comparison is also made with the baseline glass samples (without any crystals). The bioactivity of the samples was probed by measuring the changes in pH, ionic conductivity and ionic concentration of AS following in vitro dissolution experiments. High resistance of the selected glass-ceramic samples against in vitro leaching has been demonstrated by minimal weight loss (<1%) and insignificant density change, even after 6 weeks of dissolution in artificial saliva. While XRD analysis reveals the change in surface texture of the crystalline phase, FT-IR analysis weakly indicated the Ca-P compound formation on the leached surface. The experimental measurements further indicate that the leaching of F(-), Mg(2+) ions from the sample surface commonly causes the change in the surface chemistry. Furthermore, the presence of (Ca, P, O)-rich mineralized deposits on the leached glass-ceramic surface as well as the decrease in Ca(2+) ion concentrations in the leaching solutions (compared to that in the initial AS solution) provide evidences of the moderate bioactive or mild biomineralisation behaviour of investigated glass-ceramics.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Bone Tissue Engineering Materials · Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. H.-M. Kim, Ceramic bioactivity and related biomimetic strategy. Curr. Opin. Solid State Mater. Sci. 7, 289–299 (2003)10.1016/j.cossms.2003.09.014 ↗
2. D.C. Cluppera, J.J. Mecholsky Jra, G.P. LaTorreb, D.C. Greenspan, Bioactivity of tape cast and sintered bioactive glass-ceramic in simulated body fluid. Biomaterials 23, 2599–2606 (2002)10.1016/S0142-9612(01)00398-2 ↗
3. Y. Ebisawa, F. Miyaii, T. Kokubo, K. Ohura, T. Nakamura, Bioactivity of ferrimagnetic glass-ceramics in the system FeO-Fe2O3-CaO-SiO2. Biomaterials 18, 1277–1284 (1997)10.1016/S0142-9612(97)00067-7 ↗
4. D.M. Liu, Bioactive glass-ceramic: formation, characterization and bioactivity, Mater. Chem. Phy. 36, 294–303 (1994)10.1016/0254-0584(94)90045-0 ↗
5. J.M. Oliveira, R.N. Correia, M.H. Fernandes, Surface modifications of a glass and a glass-ceramic of the MgO-3CaO · P2O5-SiO2 system in a simulated body fluid. Biomaterials 16, 649–654 (1995)10.1016/0142-9612(95)94146-C ↗
6. A.J. Salinas, J. Roman, M. Vallet-Regi, J.M. Oliveira, R.N. Correia, M.H. Fernandes, In vitro bioactivity of glass and glass-ceramics of the 3CaO · P2O5-CaO · SiO2-CaO · MgO · 2SiO2 system. Biomaterials 21, 251–257 (2000)10.1016/S0142-9612(99)00150-7 ↗
7. S. Agathopoulosa, D.U. Tulyaganova, P. Valeriob, J.M.F. Ferreira, A new model formulation of the SiO2–Al2O3–B2O3–MgO–CaO–Na2O–F glass-ceramics. Biomaterials 26, 2255–2264 (2005)10.1016/j.biomaterials.2004.07.030 ↗
8. S. Padilla, J. Roman, A. Carenas, M. Vallet-Regi, The influence of the phosphorus content on the bioactivity of sol–gel glass-ceramics. Biomaterials 26, 475–483 (2005)10.1016/j.biomaterials.2004.02.054 ↗
9. M.I. Alemany, P. Velasquez, M.A. de la Casa-Lillo, P.N. De Aza, Effect of materials processing methods on the ‘in vitro’ bioactivity of wollastonite glass-ceramic materials. J. Non-Cryst. Solid. 351, 1716–1726 (2005)10.1016/j.jnoncrysol.2005.04.062 ↗
10. R. Xina, Y. Lenga, J. Chenb, Q. Zhang, A comparative study of calcium phosphate formation on bioceramics in vitro and in vivo. Biomaterials 26, 6477–6486 (2005)10.1016/j.biomaterials.2005.04.028 ↗
11. O. Peitl, E. Dutra Zanotto, L.L. Hench, Highly bioactive P2O5-Na2O-CaO-SiO2 glass-ceramics. J. Non-Cryst. Solid. 292, 115–126 (2001)10.1016/S0022-3093(01)00822-5 ↗
12. Y. Zhang, J.D. Santos, Microstructural characterization and in vitro apatite formation in CaO-P2O5-TiO2-MgO-Na2O glass-ceramics. J. Euro. Ceram. Soc. 21, 169–175 (2001)10.1016/S0955-2219(00)00202-8 ↗
13. W. Vogel, W. Höland, K. Kaumann, Development of machinable bioactive glass-ceramics for medical uses. J. Non-Cryst. Solid. 80, 34–51 (1986)10.1016/0022-3093(86)90377-7 ↗
14. W. Höland, W. Vogel, K. Kaumann, Interface reaction between machinable bioactive glass-ceramic and bone. J. Biomed. Mater. Res. 19, 303–312 (1985)10.1002/jbm.820190311 ↗
15. S. Roy, Microstructure development and in-vitro properties of Macor Glass-ceramics. Masters dissertation, IIT Kanpur, India, May 2005
16. A. Guedes, A.M.P. Pinto, M. Vieira, F. Viana, Multilayered interface in Ti/Macor® machinable glass-ceramic joints. Mat. Sci. Eng. A 301, 118–124 (2001)10.1016/S0921-5093(00)01804-9 ↗
17. L.A. Flanders, J.B. Quinn, O.C. Wilson Jr, J.K. Lloyd, Scratch hardness and chipping of dental ceramics under different environments. Dental Mater. 19, 716–724 (2003)10.1016/S0109-5641(03)00018-6 ↗
18. H. Li, Z.R. Zhou, Wear behaviour of human teeth in dry and artificial saliva conditions. Wear 249, 980–984 (2002)10.1016/S0043-1648(01)00835-3 ↗
19. A.C. Queiroz, J.D. Santos, F.J. Monterio, M.H. Prado da Silva, Dissolution studies of Hydroxyapatite and glass-reinforced Hydroxyapatite ceramics. Mater. Char. 50, 197–102 (2003)10.1016/S1044-5803(03)00092-5 ↗
20. A.G. Dias, M.A. Lopes, I.R. Gibson, J.D. Santos, In vitro degradation studies of calcium phosphate glass ceramics prepared by controlled crystallization. J. Non-Cryst. Solid. 330, 81–89 (2003)