In vitro biocompatibility of modified potassium fluorrichterite and potassium fluorrichterite-fluorapatite glass–ceramics
Source abstract
Abstract
Potassium fluorrichterite (KNaCaMg(5)Si(8)O(22)F(2)) glass-ceramics were modified by either increasing the concentration of calcium in the glass (GC5), or by the addition of P(2)O(5) to produce potassium fluorrichterite-fluorapatite (GP2). The solubility of the stoichiometric composition (GST), GC5 and GP2 were measured using the standard test described in ISO 6872:1995 (Dental Ceramics). Ion release profiles were determined for Si, Ca, Mg, Na, K and P using inductively coupled plasma mass spectrometry and fluoride ion (F(-)) concentration was measured using an ion-selective electrode. The cytotoxicity of all compositions was assessed using cultured rat osteosarcoma cells (ROS, 17/2.8). Cell response was qualitatively assessed using scanning electron microscopy (SEM) and quantitatively using the Alamar blue assay. GST was the least soluble and also released the lowest concentration of ions following immersion in water. Of the modified compositions, GC5 demonstrated intermediate solubility but the greatest ion release while GP2 exhibited the highest solubility. This was most likely due to GC5 having the greatest proportion of residual glass following crystallisation. The mass loss exhibited by GP2 may have been due in part to the partial disintegration of the surface of specimens during solubility testing. SEM demonstrated that all compositions supported the growth of healthy ROS cells on their surfaces, and this data was further supported by the quantitative Alamar blue assay.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Facial Trauma and Fracture Management · Dental materials and restorations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Brook IM, Lamb DJ. Correction of local alveolar defects by implantation of hydroxyapatite: a preliminary study. Br Dent J. 1986;161(2):68–70.10.1038/sj.bdj.4805889 ↗
2. Hench LL. The story of bioglass. J Mater Sci Mater Med. 2006;17(11):967–78.10.1007/s10856-006-0432-z ↗
3. Yoshii S, et al. Strength of bonding between A-W glass–ceramic and the surface of bone cortex. J Biomed Mater Res. 1988;22(3 Suppl):327–38.10.1002/jbm.820221410 ↗
4. Kokubo T, et al. Apatite and wollastonite containing glass-ceramics for prosthetic applications. Bull Inst Chem Res Kyoto Univ. 1982;60:260–8.
5. da Rocha Barros VM, et al. In vivo bone tissue response to a canasite glass–ceramic. Biomaterials. 2002;23:2895–9000.10.1016/S0142-9612(01)00417-3 ↗
6. da Rocha Barros VM, Liporaci JL Jr, Rosa AL, Junqueira MC, de Oliveira PT, Johnson A, van Noort R. Bone response to three different chemical compositions of fluorocanasite glass-ceramic. J Biomed Mater Res A. 2007;83(2):480–3.10.1002/jbm.a.31219 ↗
7. Miller CA, et al. Formation of apatite layers on modified canasite glass–ceramics in simulated body fluid. J Biomed Mater Res. 2002;59(3):473–80.10.1002/jbm.10018 ↗
8. Bandyopadhyay-Ghosh SFP, Johnson A, Felipucci DN, Reaney IM, Salata LA, Brook IM, Hatton PV. Osteoconductivity of modified fluorocanasite glass–ceramics for bone tissue augmentation and repair. J Biomed Mater Res A. 2010;94(3):760–8.10.1002/jbm.a.32750 ↗
9. Denry IL, Holloway JA. Effect of crystallization heat treatment on the microstructure and biaxial strength of fluorrichterite glass–ceramics. J Biomed Mater Res B. 2007;80(2):454–9.10.1002/jbm.b.30617 ↗
10. Denry IL, Holloway JA. Elastic constants, Vickers hardness, and fracture toughness of fluorrichterite-based glass–ceramics. Dent Mater. 2004;20(3):213–9.10.1016/S0109-5641(03)00094-0 ↗
11. Mirsaneh M, et al. Characterization of high-fracture toughness K-fluorrichterite–fluorapatite glass–ceramics. J Amer Ceram Soc. 2004;87(2):240–6.10.1111/j.1551-2916.2004.00240.x ↗
12. Mirsaneh M, et al. Effect of CaF2 and CaO substituted for MgO on the phase evolution and mechanical properties of K-fluorrichterite glass–ceramics. J Amer Ceram Soc. 2006;89(2):587–95.10.1111/j.1551-2916.2005.00713.x ↗
13. Beall GH and Meagles JE Jr. Potassium fluorrichterite glass ceramics and method U.S. Patent, Editor. 1984: United States.
14. Beall GH. Chain silicate glass–ceramics. J Non-Cryst Solids. 1991;129:163–73.10.1016/0022-3093(91)90092-K ↗
15. Mirsaneh M. Characterization of K-fluorrichterite based glass–ceramics for biomedical applications, in engineering materials. Sheffield: University of Sheffield; 2005. p. 211.
16. Bhakta S, Pattanayak DK, Takadama H, Kokubo T, Miller CA, Mirsaneh M, Reaney IM, Brook IM, van Noort R, Hatton PV. Prediction of osteoconductive activity of modified potassium fluorrichterite glass–ceramics by immersion in simulated body fluid. J Mater Sci. 2010;21:2979–88.10.1007/s10856-010-4145-y ↗
17. ISO 6872:1995, Dental Ceramics, International Organization for Standardisation, Geneva, Switzerland.
18. Devlin AJ, Hatton PV, Brook IM. Dependence of in vitro biocompatibility of ionomeric cements on ion release. J Mater Sci. 1998;9:737–41.10.1023/A:1008907119794 ↗
19. Wallace KE, Hill RG, Pembroke JT, Brown CJ, Hatton PV. Influence of sodium oxide content on bioactive glass properties. J Mater Sci. 1999;10:697–701.10.1023/A:1008910718446 ↗
20. Hurrell-Gillingham K, Reaney IM, Miller CA, Crawford A, Hatton PV. Devitrification of ionomer glass and its effect on the in vitro biocompatibility of glass ionomer cements. Biomaterials. 2003;24:3153–60.10.1016/S0142-9612(03)00124-8 ↗
21. Nakayama GR, Caton MC, Nova MP, Parandoosh Z. Assessment of the Alamar blue assay for cellular growth and viability in vitro. J Immunol Methods. 1997;204(2):205–8.10.1016/S0022-1759(97)00043-4 ↗
22. Stokes CW, Hand RJ, van Noort R. Investigation of the chemical solubility of mixed alkali fluorocanasite forming glasses. J Non-Cryst Solids. 2006;352:142–9.10.1016/j.jnoncrysol.2005.11.030 ↗
23. Freeman CO, et al. Crystallization modifies osteoconductivity in an apatite–mullite glass–ceramic. J Mater Sci. 2003;14:985–90.10.1023/A:1026306901058 ↗