Microchemical transformation of bioactive glass particles of narrow size range, a 0–24 months study
Source abstract
Abstract
Previous studies demonstrated the capacity of bioactive glass particles of narrow size range (300-355 microm, Biogran) to stimulate bone tissue formation without contact with pre-existing bone tissue. Chemical interactions between the bioactive glass and the surrounding tissue fluids caused the glass transformation. This study quantifies the time-dependent transformation process. Particles were implanted in the jaws of beagle dogs and resected after 1, 2, 3, 6, 12 and 24 months. Microchemical analysis was performed using a scanning electron microscope equipped with an energy dispersive X-ray analysis system. After one month, Na-ions were leached out and the particles transformed into two layers. In the center, a Si-rich gel was found on the outer surface, a Ca- and P-rich shell. After two months, the concentration levels of the outer Ca- and P-rich shell remained. In the center the Si-concentration decreased and the Ca and P concentration increased. After three months, Si disappeared completely from the center of the particle, while the Ca and P concentration increased. At one and two years, the Ca and P concentrations in the transformed particles equalled those of bone tissue, turning the transformed particle into a chemical equivalent of the bone mineral phase.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Spine and Intervertebral Disc Pathology · Facial Trauma and Fracture Management
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. E. J. G. Schepers, M. Declercq, P. Ducheyne and R. J. Kempeneers, J. Oral Rehab. 18 (1991) 439-452.10.1111/j.1365-2842.1991.tb01689.x ↗
2. P. Ducheyne, A. El-Ghannam and I. Shapiro, J. Cell. Biochem. 56 (1994) 162-167.10.1002/jcb.240560207 ↗
3. P. Ducheyne, P. Bianco, S. Radin and E. Schepers, in “Bone Bonding Biomaterials” (Kokubo & Van Blitterswijk, Leidorp, 1992) 1-12.
4. E. Schepers and P. Ducheyne, J. Oral Rehab 24 (1997) 171-181.10.1111/j.1365-2842.1997.tb00311.x ↗
5. A. J. Garcia and P. J. Ducheyne, J. Biomed. Mater. Res. 28 (1994) 947-960.10.1002/jbm.820280814 ↗
6. T. Furasawa and K. Mizunuma, Implant. Dent. 6 (1997) 93-101.10.1097/00008505-199700620-00003 ↗
7. A. M. Gatti and D. Zaffe, Biomaterials 12 (1991) 497-504.10.1016/0142-9612(91)90149-5 ↗
8. G. Daculsi and R. Z. Legeros, Scan. Micros. 4 (1990) 309-314.
9. T. Furusawa and K. Mizunuma, Implant. Dent. 6 (1997) 93-101.10.1097/00008505-199700620-00003 ↗
10. S. Radin, P. Ducheyne, S. Falaize and A. Hammond, in “Bioceramics” (Sedel & Rey, Cambridge, 1997) 45-48.
11. I. M. O. Kangasniemi, E. Vedel, J. De Blick-Hogerworst, A. U. Yli-Urpo and K. De Groot, J. Biomed. Mater. Res. 27 (1993) 1225-1233.10.1002/jbm.820271003 ↗
12. A. El-Ghannam, P. Ducheyne and I. M. Shapiro, Biomaterials 18 (1997) 295-303.10.1016/S0142-9612(96)00059-2 ↗
13. T. Kokubo, J. Non-Cryst. Sol. 120 (1990) 138-151.10.1016/0022-3093(90)90199-V ↗
14. O. P. Filho, G. P. Latorre and L. L. Hench, J. Biomed. Mater. Res. 30 (1996) 509-514.10.1002/(SICI)1097-4636(199604)30:4<509::AID-JBM9>3.0.CO;2-T ↗
15. E. Schepers, L. Barbier and P. Ducheyne, Int. J. Oral. Maxillofac. Implants. 13 (1998) 655-665
16. L. Barbier, J. Vander Sloten, G. Krzesinsnski, E. Schepers and G. Van Der Perre, J. Oral Rehab. 25 (1998) 847-858.10.1046/j.1365-2842.1998.00318.x ↗