Effects of phase constitution on magnetic susceptibility and mechanical properties of Zr-rich Zr–Mo alloys
Source abstract
Abstract
The effects of the microstructures and phases of Zr-rich Mo alloys on their magnetic susceptibilities and mechanical properties were investigated in order to develop a Zr alloy with low magnetic susceptibility for use in magnetic resonance imaging (MRI). The magnetic susceptibility was measured with a magnetic susceptibility balance, while mechanical properties were evaluated by a tensile test. The microstructure was evaluated with an X-ray diffractometer, an optical microscope, and a transmission electron microscope. Evaluation of the microstructures revealed that the α' phase was the dominant form at less than 2% Mo content in the as-cast alloy. The ω phase was formed in as-cast Zr-3Mo but disappeared with aging at 973 K. Magnetic susceptibility was reflected in the phase constitution: the susceptibility showed a local minimum at Zr-(0.5-1)Mo with mostly α' phase and a minimum at Zr-3Mo with mostly β and ω phases. The magnetic susceptibility of as-cast Zr-3Mo increased at 973 K due to disappearance of the ω phase. However, the susceptibility was still as low as that of as-cast Zr-1Mo. The ultimate tensile strength of α'-based Zr-Mo alloys was tailored from 674 to 970 MPa, and the corresponding elongation varied from 11.1% to 2.9%. Because Zr-Mo alloys containing ω phase were found, through tensile tests, to be brittle this phase should be avoided, irrespective of the low magnetic susceptibility, in order to maintain mechanical reliability. Elongation of the Zr-3Mo alloy was dramatically improved when the phase constitution was changed to α and β phases by aging at 973 K for 86.4 ks. The magnetic susceptibilities of the α'-based Zr-Mo alloys are one-third those of Ti-6Al-4V and Ti-6Al-7Nb, and thus these Zr alloys are useful for medical devices under MRI.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Titanium Alloys Microstructure and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Magnetic resonance imaging artifacts caused by aneurysm clips and shunt valves: dependence on field strength (1.5 and 3T) and imaging parameters10.1002/jmri.20391 ↗
2. Artifacts from dental casting alloys in magnetic resonance imaging10.1177/154405910308200806 ↗
3. Quantification of susceptibility artifacts produced on high-field magnetic resonance images by various biomaterials used for neurosurgical implants10.3171/jns.2002.97.6.1472 ↗
4. Quantitative analysis of magnetic resonance imaging susceptibility artifacts caused by neurosurigical biomaterials: comparison of 0.5, 1.5, and 3.0Tesla magnetic fields10.2176/nmc.45.395 ↗
5. The interobserver-validated relevance of intervertebral spacer materials in MRI artifacting10.1007/s00586-006-0064-5 ↗
6. Ride DR. Magnetic susceptibility of the elements and inorganic compounds. In: CRC Handbook of Chemistry and Physics, 87th edn, Vol. 4. [Q?]: CRC Press, 2006. p. 142–7.
7. Cytotoxicity evaluation of 43 metal salts using murine fibroblasts and osteoblastic cells10.1002/(SICI)1097-4636(199802)39:2<331::AID-JBM22>3.0.CO;2-E ↗
8. Heat treatment, transformation reactions and mechanical properties of two high strength zirconium alloys10.1016/0022-5088(78)90215-1 ↗
9. Microstructure and magnetic susceptibility of as-cast Zr–Mo alloys10.1016/j.actbio.2009.09.013 ↗
10. Effects of phase constitution of Zr–Nb alloys on their magnetic susceptibility10.2320/matertrans.M2009187 ↗
11. Svechnikov VN, Spektor AC. Phase Transformations. Kiev, Ukraine: Nauk Dumka, 1967. p. 123–8 (in Russian).
12. Ω-Assist nucleation and growth of α precipitates in the Ti–6Al–5Mo–5V–3Cr–0.5Fe β titanium alloy10.1016/j.actamat.2009.01.007 ↗
13. Mechanism of ω→α transformation in β-Ti alloy10.2320/jinstmet1952.57.3_261 ↗
14. Magnetic studies of phase equilibria in Ti–Al (30–57at. pct) alloys10.1007/BF02697074 ↗
15. The formation of omega phase in titanium and zirconium alloys: a review10.1007/BF00550217 ↗
16. Age hardening of Zr–2.5wt% Nb slowly cooled from the (α+β) phase field10.1016/0022-3115(72)90004-9 ↗
17. Magnetic studies of omega-phase precipitation and aging in titanium–vanadium alloys10.1016/0022-5088(75)90218-0 ↗
18. Effects of metallic concentrations other than Ti, Al and V on cell viability10.2320/matertrans1989.39.1070 ↗
19. Acute toxicity of metal ions in cultures of osteogenic cells derived from bone marrow stromal cells10.1002/jab.770060205 ↗
20. Release of metal ions from dental implant materials in vivo: determination of Al, Co, Cr, Mo, Ni, V, and Ti in organ tissue10.1002/jbm.820251204 ↗