journal article·2015-10

In vivo evaluation of a magnesium-based degradable intramedullary nailing system in a sheep model

Christina Rössig, Nina Angrisani, Patrick Helmecke, Silke Besdo, Jan-Marten Seitz, Bastian Welke, Nickolay Fedchenko, Heiko Kock, Janin Reifenrath

Acta Biomaterialia· Volume 25
Publisher page

Abstract

The biocompatibility and the degradation behavior of the LAE442 magnesium-based intramedullary interlocked nailing system (IM-NS) was assessed in vivo in a comparative study (stainless austenitic steel 1.4441LA) for the first time. IM-NS was implanted into the right tibia (24-week investigation period; nails/screws diameter: 9 mm/3.5 mm, length: 130 mm/15-40 mm) of 10 adult sheep (LAE442, stainless steel, n=5 each group). Clinical and radiographic examinations, in vivo computed tomography (CT), ex vivo micro-computed tomography (μCT), mechanical and histological examinations and element analyses of alloying elements in inner organs were performed. The mechanical examinations (four-point bending) revealed a significant decrease of LAE442 implant stiffness, force at 0.2% offset yield point and maximum force. Periosteal (new bone formation) and endosteal (bone decline) located bone alterations occurred in both groups (LAE442 alloy more pronounced). Moderate gas formation was observed within the LAE442 alloy group. The CT-measured implant volume decreased slightly (not significant). Histologically a predominantly direct bone-to-implant interface existed within the LAE442 alloy group. Formation of a fibrous tissue capsule around the nail occurred in the steel group. Minor inflammatory infiltration was observed in the LAE442 alloy group. Significantly increased quantities of rare earth elements were detected in the LAE442 alloy group. μCT examination showed the beginning of corrosion in dependence of the surrounding tissue. After 24 weeks the local biocompatibility of LAE442 can be considered as suitable for a degradable implant material. Statement of significance An application oriented interlocked intramedullary nailing system in a comparative study (degradable magnesium-based LAE442 alloy vs. steel alloy) was examined in a sheep model for the first time. We focused in particular on the examination of implant degradation by means of (μ-)CT, mechanical properties (four-point bending), clinical compatibility, local bone reactions (X-ray and histology) and possible systemic toxicity (histology and element analyses of inner organs). A significant decrease of magnesium (LAE442 alloy) implant stiffness and maximum force occurred. Moderate not clinically relevant gas accumulation was determined. A predominantly direct bone-to-implant contact existed within the magnesium (LAE442 alloy) group compared to an indirect contact in the steel group. Rare earth element accumulation could be observed in inner organs but H&E staining was inconspicuous.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Magnesium Alloys: Properties and Applications · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Comparison of stainless steel and titanium alloy orthodontic miniscrew implants: a mechanical and histologic analysis10.1016/j.ajodo.2013.12.022 ↗
2. Randomized controlled trial comparing stabilization of fresh close femoral shaft fractures in children with titanium elastic nail system versus stainless steel elastic nail system
3. A review on nickel-free nitrogen containing austenitic stainless steels for biomedical applications10.1016/j.msec.2013.06.002 ↗
4. Stainless steel in bone surgery10.1016/S0020-1383(00)80015-7 ↗
5. The effects on bone of the presence of metals; based upon electrolysis: an experimental study10.1097/00000658-193706000-00006 ↗
6. Immuno-inflammatory tissue reaction to stainless-steel and titanium plates used for internal fixation of long bones10.1016/S0142-9612(02)00312-5 ↗
7. The effect of retained intramedullary nails on tibial bone mineral density10.1016/j.clinbiomech.2008.02.003 ↗
8. Long-term residual musculoskeletal deficits after femoral shaft fractures treated with intramedullary nailing10.1097/00005373-200009000-00010 ↗
9. Magnesium implant alloy with low levels of strontium and calcium: the third element effect and phase selection improve bio-corrosion resistance and mechanical performance10.1016/j.msec.2013.11.011 ↗
10. Enhanced antimicrobial properties, cytocompatibility, and corrosion resistance of plasma-modified biodegradable magnesium alloys10.1016/j.actbio.2013.10.012 ↗
11. Microstructure, mechanical properties, corrosion behavior and cytotoxicity of Mg–Zn–Al–Ca alloys as biodegradable materials10.1016/j.jallcom.2014.04.059 ↗
12. Influence of aluminium on the corrosion behaviour of binary magnesium–aluminium alloys in saline solutions10.1002/maco.201206531 ↗
13. Effects of alloying elements on the corrosion behavior and biocompatibility of biodegradable magnesium alloys: a review10.1039/C3TB21746A ↗
14. The effect of selected alloying element additions on properties of Mg-based alloy as bioimplants: a literature review10.1007/s11706-013-0210-z ↗
15. New, fast corroding high ductility Mg–Bi–Ca and Mg–Bi–Si alloys, with no clinically observable gas formation in bone implants10.1016/j.mseb.2011.07.011 ↗
16. A method of quantification of stress shielding in the proximal femur using hierarchical computational modeling10.1080/10255840600564959 ↗
17. Resorbierbare Implantate für Frakturfixierungen10.1007/s001130050519 ↗
18. Femoral bone loss in total knee arthroplasty. A review
19. Zirconium, calcium, and strontium contents in magnesium based biodegradable alloys modulate the efficiency of implant-induced osseointegration
20. Bone-implant interface strength and osseointegration: biodegradable magnesium alloy versus standard titanium control10.1016/j.actbio.2010.08.020 ↗
21. Effect of alloying elements on the elastic properties of Mg from first-principles calculations10.1016/j.actamat.2009.04.038 ↗
22. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
23. Kaese · 2002
24. Eigenschaften von reinem Magnesium
25. On the mechanisms of biocompatibility10.1016/j.biomaterials.2008.04.023 ↗
26. Immunological response to biodegradable magnesium implants10.1007/s11837-014-0874-6 ↗
27. Ductile biodegradable mg-based metallic glasses with excellent biocompatibility10.1002/adfm.201203738 ↗
28. Magnesium alloys for temporary implants in osteosynthesis: in vivo studies of their degradation and interaction with bone10.1016/j.actbio.2011.11.008 ↗
29. Biocompatibility of bio-Mg–Zn alloy within bone with heart, liver, kidney and spleen10.1007/s11434-009-0080-z ↗
30. Evaluation of the skin sensitizing potential of biodegradable magnesium alloys
31. Magnesium ion stimulation of bone marrow stromal cells enhances osteogenic activity, simulating the effect of magnesium alloy degradation10.1016/j.actbio.2014.02.002 ↗
32. Effect of implantation of biodegradable magnesium alloy on BMP-2 expression in bone of ovariectomized osteoporosis rats10.1016/j.msec.2013.05.042 ↗
33. In vivo testing of a bioabsorbable magnesium alloy serving as total ossicular replacement prostheses10.1177/0885328212472246 ↗
34. In vivo stimulation of bone formation by aluminum and oxygen plasma surface-modified magnesium implants10.1016/j.biomaterials.2013.08.052 ↗
35. A review of the biological response to ionic dissolution products from bioactive glasses and glass-ceramics10.1016/j.biomaterials.2011.01.004 ↗
36. Biomimetic Mg-substituted hydroxyapatite: from synthesis to in vivo behaviour10.1007/s10856-006-0032-y ↗
37. Biodegradable magnesium scaffolds: Part II: peri-implant bone remodeling10.1002/jbm.a.31293 ↗
38. Biodegradable magnesium-based screw clinically equivalent to titanium screw in hallux valgus surgery: short term results of the first prospective, randomized, controlled clinical pilot study10.1186/1475-925X-12-62 ↗
39. In vivo degradation behavior and biocompatibility of Mg–Nd–Zn–Zr alloy at early stage
40. In vivo and in vitro degradation behavior of magnesium alloys as biomaterials10.1016/S1005-0302(12)60051-6 ↗
41. In vivo evaluation of biodegradable magnesium alloy bone implant in the first 6months implantation10.1002/jbm.a.32132 ↗
42. Research on the biocompatibility of the new magnesium alloy LANd442 – an in vivo study in the rabbit tibia over 26weeks10.1002/adem.201180066 ↗
43. Evaluation of the biocompatibility of two magnesium alloys as degradable implant materials in comparison to titanium as non resorbable material in the rabbit10.1016/j.msec.2012.08.046 ↗
44. Influence of the grain size on the in vivo degradation behaviour of the magnesium alloy LAE 44210.1177/0954411912471495 ↗
45. In vivo corrosion and corrosion protection of magnesium alloy LAE44210.1016/j.actbio.2009.10.012 ↗
46. A. Krause, Ergebnisse, in: A. Krause (Ed.), Untersuchung der Degradation und Biokompatibilität von degradablen, intramedullären Implantaten auf Magnesiumbasis im Kaninchenmodell, Hannover, 2008, pp. 85–166.
47. M. Thomann, Ergebnisse, in: M. Thomann (Ed.), Untersuchungen zur Degradation und Biokompatibilität von intramedullären Implantaten auf Magnesiumbasis im Kaninchenmodell: Prüfung der Degradation im Langzeitversuch und Untersuchung des Einflusses einer Fluoridbeschichtung, Hannover, 2008, pp. 65–109.
48. The effect of different sterilization methods on the mechanical strength of magnesium based implant materials10.1002/adem.201100074 ↗
49. C. Rössig, et al., Magnesium-based intramedullary nailing system in a sheep model: Biomechanic evaluation and first in vivo results, J. Vet. Sci. Med. Diagn., in press. http://dx.doi.org/10.4172/2325-9590.1000150.10.4172/2325-9590.1000150 ↗
50. J.-M. Seitz, Ergebnisse und Interpretationen, in: J.-M. Seitz (Ed.), Beitrag zur Legierungsentwicklung von neodymiumhaltigen Magnesiumlegierungen für die Biomedizintechnik, Hannover, 2013, pp. 68–130.
51. Standard Specification and Test Methods for Intramedullary Fixation Devices. ASTM 1264-03:2003, Philadelphia: ASTM International.
52. YaDiV—an open platform for 3D visualization and 3D segmentation of medical data10.1007/s00371-010-0539-6 ↗
53. Characterization of MgNd2 alloy for potential applications in bioresorbable implantable devices10.1016/j.actbio.2012.05.024 ↗
54. Corrosion of metals and alloys-Removal of corrosion products from corrosion test specimens. ISO 8407-1991E:1991, ISO, Geneva.
55. B. Vollmerhaus, H. Roos, Speiseröhre, Magen, Darm, Darmanhangsdrüsen. Milz, in: R. Nickel, A. Schummer, E. Seiferle (Ed.), Lehrbuch der Anatomie der Haustiere Band 2, Stuttgart, Parey, 2004, pp. 191–221.
56. Die Trenn-Dünnschliff-Technik zur Herstellung histologischer Präparate von nicht schneidbaren Geweben und Materialien
57. Eigene Untersuchungen
58. Biological evaluation of medical devices-Tests for local effects after implantation, ISO 10993-6:2009, ISO, Geneva.
59. Semi-quantitative and qualitative histologic analysis method for the evaluation of implant biocompatibility10.3109/08941939409015356 ↗
60. The effects of handling and storage on magnesium based implants — first results10.1016/j.msec.2013.03.034 ↗
61. Fluoride and calcium-phosphate coated sponges of the magnesium alloy AX30 as bone grafts: a comparative study in rabbits10.1007/s10856-012-4812-2 ↗
62. In vivo assessment of the host reactions to the biodegradation of the two novel magnesium alloys ZEK100 and AX30 in an animal model10.1186/1475-925X-11-14 ↗
63. Evaluation of the soft tissue biocompatibility of MgCa0.8 and surgical steel 316L in vivo: a comparative study in rabbits10.1186/1475-925X-9-63 ↗
64. Investigation on the use of a magnesium alloy as a new resorbable implant material for orthopaedic surgery
65. Development of a bone nonunion in a noncritical segmental tibia defect model in sheep utilizing interlocking nail as an internal fixation system10.1016/j.jss.2013.02.060 ↗
66. Comparison of a new braid fixation system to an interlocking intramedullary nail for tibial osteotomy repair in an ovine model10.1111/j.1532-950X.2009.00517.x ↗
67. Comparison of unreamed nailing and external fixation of tibial diastases–mechanical conditions during healing and biological outcome10.1016/j.orthres.2004.02.006 ↗
68. Biodegradable metals for cardiovascular stent application: interests and new opportunities10.3390/ijms12074250 ↗
69. In vivo study of magnesium plate and screw degradation and bone fracture healing10.1016/j.actbio.2015.02.010 ↗
70. Fracture healing after reamed and unreamed intramedullary nailing in sheep tibia10.1016/j.injury.2010.10.004 ↗
71. Unreamed or RIA reamed nailing: an experimental sheep study using comparative histological assessment of affected bone tissue in an acute fracture model10.1016/S0020-1383(10)70006-1 ↗
72. Cortical perfusion and local fat occlusion after intramedullary nailing of the ovine tibia-comparison of different surgical procedures10.1016/j.injury.2009.01.106 ↗
73. Effect of limited and standard reaming on cortical bone blood flow and early strength of union following segmental fracture10.1097/00005131-199808000-00006 ↗
74. Cortical bone blood flow in reamed and unreamed locked intramedullary nailing: a fractured tibia model in sheep10.1097/00005131-199410000-00002 ↗
75. Optimization of intramedullary nailing by numerical simulation of fracture healing10.1002/jor.21568 ↗
76. Should the tibia be reamed when nailing?10.1016/j.injury.2004.09.030 ↗
77. In vivo degradation and tissue compatibility of ZK60 magnesium alloy with micro-arc oxidation coating in a transcortical model10.1016/j.msec.2013.05.023 ↗
78. In vivo behavior of biodegradable Mg–Nd–Y–Zr–Ca alloy10.1007/s10856-011-4536-8 ↗
79. In vivo corrosion of four magnesium alloys and the associated bone response10.1016/j.biomaterials.2004.09.049 ↗
80. Absorbable metal in bone surgery10.1001/jama.1938.02790530018007 ↗
81. The development of binary Mg–Ca alloys for use as biodegradable materials within bone10.1016/j.biomaterials.2007.12.021 ↗
82. Biodegradable magnesium scaffolds: Part 1: appropriate inflammatory response10.1002/jbm.a.31170 ↗
83. Degradation behaviour and mechanical properties of magnesium implants in rabbit tibiae10.1007/s10853-009-3936-3 ↗
84. Comparison of the resorbable magnesium alloys LAE442 und MgCa0.8 concerning their mechanical properties, their progress of degradation and the bone-implant-contact after 12months implantation duration in a rabbit model
85. The biocompatibility of degradable magnesium interference screws: an experimental study with sheep10.1155/2015/943603 ↗
86. In vivo degradation behaviour of the magnesium alloy LANd442 in rabbit tibiae10.3390/ma4122197 ↗
87. The corrosion of magnesium in aqueous solution containing chloride ions10.1016/0010-938X(77)90059-2 ↗
88. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
89. Biomechanical testing and degradation analysis of MgCa0.8 alloy screws: a comparative in vivo study in rabbits10.1016/j.actbio.2010.10.031 ↗
90. Profound differences in the in-vivo-degradation and biocompatibility of two very similar rare-earth containing Mg-alloys in a rabbit model10.1002/mawe.201000709 ↗
91. Animal models for implant biomaterial research in bone: a review10.22203/eCM.v013a01 ↗
92. Die Wertigkeit verschiedener Versuchstierspecies für experimentelle Untersuchungen am Knochen
93. Degradable magnesium-based implant materials with anti-inflammatory activity10.1002/jbm.a.34494 ↗
94. Short-term and long-term effects of orthopedic biodegradable implants10.1615/JLongTermEffMedImplants.v21.i2.10 ↗
95. Augmentation of bone defect healing using a new biocomposite scaffold: an in vivo study in sheep10.1016/j.actbio.2010.03.028 ↗
96. Effects of mechanical compression of a fibrous tissue interface on bone with or without high-density polyethylene particles in a rabbit model of prosthetic loosening
97. Bonding of chemically treated titanium implants to bone10.1002/(SICI)1097-4636(199711)37:2<267::AID-JBM17>3.0.CO;2-B ↗
98. Biocompatibility issues with modern implants in bone – a review for clinical orthopedics10.2174/1874325000802010066 ↗
99. Fast escape of hydrogen from gas cavities around corroding magnesium implants10.1016/j.actbio.2012.10.008 ↗
100. Tissue restoration after implantation of polyglycolide, polydioxanone, polylevolactide, and metallic pins in cortical bone: an experimental study in rabbits10.1007/s00223-010-9374-z ↗