Laser-assisted Zr/ZrO2 coating on Ti for load-bearing implants
Source abstract
Abstract
Oxidized Zr alloys have been shown to exhibit lower friction and superior wear properties, suggesting that they could be used in hip and knee implants. However, conventional oxidation of Zr alloys above 500 degrees C, in dry air, for several hours has been shown to have detrimental effects on the substrate's properties. In this work, we deposited pure Zr on Ti, then oxidized the coating using a continuous-wave Nd:YAG laser, which facilitated localized heating to elevated temperatures without affecting the substrate. Laser-assisted oxidation resulted in a 7microm thick fully dense ZrO(2) layer on Zr in which an increase in oxidation kinetics was evident due to an increase in the laser power and/or the oxygen partial pressure. Due to its high surface energy and wettability, the wear rate of laser-oxidized Zr was two orders of magnitude less compared to that of as-deposited Zr. The oxidized coatings showed comparable in vitro biocompatibility to that of pure Ti and excellent in vitro cell-material interactions. This article reports the processing of Zr/ZrO(2) coatings on Ti using lasers, and the influence of laser parameters and oxygen partial pressure on the coating's mechanical, microstructural, wear and in vitro biological properties using human osteoblast cells.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Orthopaedic implants and arthroplasty · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Polyethylene debris-induced osteolysis and loosening in uncemented total hip arthroplasty10.1016/0883-5403(92)90050-Z ↗
2. The role of small polyethylene wear particles in inducing the release of mediators known to stimulate bone resorption
3. Implant retrieval studies of the wear and loosening of prosthetic joints: a review10.1016/S0043-1648(00)00370-7 ↗
4. Mechanical behaviour, wear surface morphology, and clinical performance of UHMWPE acetabular components after 10 years of implantation10.1016/S0043-1648(01)00616-0 ↗
5. The effect of conformity, thickness, and material on stresses in ultrahigh molecular weight components for total joint replacement10.2106/00004623-198668070-00010 ↗
6. Relationship between gravimetric wear and particle generation in hip simulators: conventional compared with cross linked polyethylene10.2106/00004623-200100022-00009 ↗
7. Cemented ceramic YMCK total knee arthroplasty in patients with severe rheumatoid arthritis10.1054/arth.2002.35826 ↗
8. In vivo tribological performance of 231 metal-on-metal hip articulations10.1177/112070000201200202 ↗
9. Metal-on-metal versus metal-on-polyethylene bearings in total hip arthroplasty: a matched case–control study
10. Davidson JA, Poggie RA, Mishra AK, Salehi A, Harbaugh M. Increased wear and contact stress from increased polyethylene stiffness in prosthetic knee and hip articulation, In: Goh J, Nather A, editors. Proceedings of the 7th international conference on biomedical engineering, 2–4 December, Singapore: 1992. p. 152–54.
11. The influence of scratches to metallic counterfaces on the wear of ultra-high molecular weight polyethylene10.1243/PIME_PROC_1995_209_353_02 ↗
12. The role of counterface imperfections in the wear of polyethylene10.1016/0043-1648(87)90036-6 ↗
13. Characteristics of metal and ceramic total hip bearing surfaces and their effect on long term ultra high molecular weight PE wear10.1097/00003086-199309000-00053 ↗
14. Tribological behaviour of DLC coatings compared with different materials used in hip joint prostheses10.1016/S0043-1648(01)00651-2 ↗
15. Adhesion properties of diamond-like coated orthopaedic biomaterials10.1016/S0925-9635(00)00567-7 ↗
16. The electrochemical and mechanical behavior of passivated and TiN/AlN-coated Co–Cr–Mo and Ti6Al4V alloys10.1016/S0142-9612(03)00606-9 ↗
17. Tribological and electrochemical performance of PVD TiN coatings on the femoral head of Ti–6Al–4V artificial hip joints10.1016/S0257-8972(02)00630-8 ↗
18. Zirconia (ZrO2)-coated zirconium–2.5Nb alloy for prosthetic knee bearing applications
19. Zirconia/zirconium: a new abrasion resistant material for orthopaedic applications10.1080/10667857.1993.11784927 ↗
20. Simulated wear with cobalt–chromium and oxidized zirconium knee femoral components
21. Wear performance of ultra-high molecular weight polyethylene against oxidized zirconium total knee femoral components10.2106/00004623-200100022-00004 ↗
22. Polyethylene wear performance of oxidized zirconium and cobalt–chromium knee components under abrasive conditions10.2106/00004623-200200002-00018 ↗
23. Oxidized zirconia for hemiarthroplasty: an in vitro assessment
24. Histological response to cylinders of low modulus titanium alloy (Ti–13Nb–13Zr) and a wear-resistant zirconium alloy (Zr–2.5Nb) implanted in the rabbit tibia10.1002/jab.770040407 ↗
25. An oxidized Zr ceramic surfaced femoral component for total knee arthroplasty10.1097/01.blo.0000093003.90435.1f ↗
26. Oxidation microstructures and interfaces in the oxidized zirconium knee10.1111/j.1744-7402.2005.02025.x ↗
27. Studies on the oxygen gradients in oxidizing metals: I. Zirconium10.1149/1.2426137 ↗
28. Oxidation properties of a zirconium–2.7 w/o niobium alloy in the temperature range 650-1000°C10.1149/1.2404037 ↗
29. Studies on the oxygen gradients in oxidizing metals: III. Kinetics of the oxidation of zirconium at high temperatures10.1149/1.2423577 ↗
30. Engineered porous metals for implants10.1007/s11837-008-0059-2 ↗
31. Functionally graded Co–Cr–Mo coating on Ti–6Al–4V alloy structures10.1016/j.actbio.2007.10.005 ↗
32. Low stiffness porous Ti structures for load-bearing implants10.1016/j.actbio.2007.03.008 ↗
33. Establishing an immortalized human osteoprecusor cell line: OPC110.1359/jbmr.1999.14.10.1721 ↗
34. Compositionally graded yttria-stabilized zirconia coating on stainless steel using laser engineered net shaping (LENS™)10.1016/j.scriptamat.2007.06.055 ↗
35. On the role of microstructure form and dimension in surface energy changes in a magnesia partially stabilized zirconia bioceramic following CO2 laser irradiation10.1088/0022-3727/37/1/014 ↗
36. Low-pressure oxidation of zirconium10.1149/1.2424546 ↗
37. Adsorption and lubrication
38. Tribochemical mechanism of alumina with water10.1080/10402008908981900 ↗
39. New prospects for a prolonged functional life-span of artificial hip joints by using the material combination polyethylene/aluminium oxide ceramic/metal10.1002/jbm.820110409 ↗
40. Preparation and cell–materials interactions of plasma sprayed strontium containing hydroxyapatite coating10.1016/j.surfcoat.2006.10.012 ↗
41. Effects of Nd:YAG laser treatment on the wettability characteristics of a zirconia-based bioceramic10.1016/j.optlaseng.2005.08.001 ↗
42. Osteoblast cell adhesion on a laser modified zirconia based bioceramic10.1007/s10856-005-2608-3 ↗
43. First-principles study of the surfaces of zirconia10.1103/PhysRevB.58.8050 ↗