Suppressing Al2O3 nanoparticle coarsening and Cu nanograin growth of milled nanostructured Cu-5vol.%Al2O3 composite powder particles by doping with Ti
Source abstract
Abstract
Abstract Both the coarsening of Al 2 O 3 nanoparticles and the growth of Cu nanograins of mechanically milled nanostructured Cu-5vol.%Al 2 O 3 composites with, and without, trace amounts of Ti during annealing at 973 K for 1 h were investigated. It was found that doping with a small amount of Ti (e.g. 0.2 wt%) in a nanostructured Cu-5vol.%Al 2 O 3 composite effectively suppressed the coarsening of Al 2 O 3 nanoparticles during exposure at this temperature. Further, the Ti addition also prevented the concomitant abnormal growth of the copper grains normally caused by the coarsening of the Al 2 O 3 nanoparticles. Energy dispersive X-ray spectroscopy analysis of the Al 2 O 3 nanoparticles in the annealed Cu-5vol.%Al 2 O 3 -0.2wt%Ti sample suggested that the Ti atoms either diffused into the Al 2 O 3 nanoparticles or segregated to the Cu/Al 2 O 3 interfaces to form Ti-doped Al 2 O 3 nanoparticles, which was more stable than Ti-free Al 2 O 3 nanoparticles during annealing at high homologous temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Morris · Acta Metall. · 1991 · 39 · 176310.1016/0956-7151(91)90144-P ↗
2. Humphry-Baker · J. Appl. Phys. · 2014 · 116 · 17350510.1063/1.4901235 ↗
3. Zhou · J. Alloys Compd. · 2016 · 682 · 59010.1016/j.jallcom.2016.04.321 ↗
4. Zhou · J. Mater. Res. · 2014 · 29 · 99610.1557/jmr.2014.79 ↗
5. Bréchet · Scr. Mater. · 2005 · 52 · 129910.1016/j.scriptamat.2005.02.021 ↗
6. Srinivasarao · Acta Mater. · 2009 · 57 · 327710.1016/j.actamat.2009.03.034 ↗
7. Sasaki · Acta Mater. · 2009 · 57 · 352910.1016/j.actamat.2009.04.012 ↗
8. Liu · Nat. Mater. · 2013 · 12 · 34410.1038/nmat3544 ↗
9. Yao · J. Mater. Sci. Technol. · 2016
10. Ribis · Acta Mater. · 2012 · 60 · 23810.1016/j.actamat.2011.09.042 ↗
11. Ribis · J. Nucl. Mater. · 2013 · 442 · S10110.1016/j.jnucmat.2012.10.051 ↗
12. Oono · Mater. Sci. Eng. A · 2016 · 649 · 25010.1016/j.msea.2015.09.094 ↗
13. Ratti · J. Nucl. Mater. · 2009 · 386 · 54010.1016/j.jnucmat.2008.12.171 ↗
14. Smith · Trans. AIME · 1948 · 175 · 15
15. Sergeenkova · Powder Metall. Met. Ceram. · 1967 · 6 · 70610.1007/BF00773490 ↗
16. Takahashi · Trans. Jpn. Inst. Met. · 1985 · 26 · 27110.2320/matertrans1960.26.271 ↗
17. Han · Sci. Rep. · 2015 · 5 · 1736410.1038/srep17364 ↗
18. Han · J. Alloys Compd. · 2015 · 622 · 38410.1016/j.jallcom.2014.10.031 ↗
19. Lifshitz · J. Phys. Chem. Solids · 1961 · 19 · 3510.1016/0022-3697(61)90054-3 ↗
20. Iijima · Metall. Trans. A · 1977 · 8 · 99710.1007/BF02661585 ↗
21. Matsuno · Metall. Mater. Trans. A · 1975 · 6 · 219110.1007/BF02818642 ↗
22. Narula · Metall. Trans. B · 1983 · 14 · 67310.1007/BF02653953 ↗
23. ASM Handbook, Alloy Phase Diagrams vol. 3 (1992).