Infrared Brazing Zirconium using Two Silver Based Foils
Source abstract
Abstract
Ag-based brazing foils, BAg-8 (72Ag–28Cu in wt%) and Ticusil® (68.8Ag–26.7Cu–4.5Ti in wt%) were selected to braze Zr. Interfacial AgCu4Zr, CuZr2 reaction layers and Ag-rich matrix dominate BAg-8 brazed joint, and fractograph after shear test shows ductile dimple fracture with plastic sliding marks. Ticusil® joint brazed at 910 °C for 300 s is comprised of Cu9Zr11 and AgZr intermetallics, and fractograph after shear test displays brittle cleavage fracture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Metals Handbook
2. Robertson · J. Nucl. Mater. · 1981 · 100 · 10810.1016/0022-3115(81)90525-0 ↗
3. Metals Handbook
4. Wu · J. Mater. Sci. Technol. · 2010 · 26 · 31110.1016/S1005-0302(10)60051-5 ↗
5. Chang · J. Mater. Sci. Technol. · 2011 · 27 · 13110.1016/S1005-0302(11)60038-8 ↗
6. Shiue · J. Alloys Compd. · 2004 · 372 · 14810.1016/j.jallcom.2003.09.155 ↗
7. Chan · Int. J. Refract. Metals Hard Mater. · 2004 · 22 · 2710.1016/j.ijrmhm.2003.11.002 ↗
8. Villars · 1995
9. Massalski · 1990