Effect of a plasmaelectrolytic coating on the strength retention of in vivo and in vitro degraded magnesium implants
Source abstract
Abstract
The strength decrease in magnesium implants was studied in vitro and in vivo, with and without a protective plasmaelectrolytic coating. In vivo, degradation was examined by implanting rectangular plates on top of the nasal bone of miniature pigs. The presence of gas pockets in the soft tissue surrounding the implants was evaluated with intermediate X-rays and computed X-ray tomography scans before euthanasia. After 12 and 24 weeks of in vivo degradation, the large rectangular plates were removed and mechanically tested in three-point bending. In vitro, identical plates were immersed in simulated body fluid for 4, 8 and 12 weeks. In vitro and in vivo results showed that onset of gas release can be delayed by the plasmaelectrolytic coating. Mass loss and strength retention during in vivo degradation is about four times slower than during in vitro degradation for the chosen test conditions. Despite the slow degradation of the investigated WE43 alloy, the occurrence of gas pockets could not be completely avoided. Nevertheless, uniformity of degradation and reliable strength retention make this alloy a prime candidate for the use of magnesium in cranio-maxillofacial surgery.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. L’utilisation du magnésium comme matériel perdu dans l’ostéosynthèse
2. Le Matériel métallique résorbable en chirurgie osseuse
3. Magnesium screw and nail transfixion in fractures10.1097/00007611-193805000-00010 ↗
4. The history of biodegradable magnesium implants: a review10.1016/j.actbio.2010.02.028 ↗
5. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
6. In vivo corrosion of four magnesium alloys and the associated bone response10.1016/j.biomaterials.2004.09.049 ↗
7. In vitro and in vivo evaluation of the surface bioactivity of a calcium phosphate coated magnesium alloy10.1016/j.biomaterials.2008.12.001 ↗
8. In vivo corrosion and corrosion protection of magnesium alloy LAE44210.1016/j.actbio.2009.10.012 ↗
9. Protective coatings on magnesium and its alloys – a critical review10.1016/S0925-8388(01)01899-0 ↗
10. Evaluation of short-term effects of rare earth and other elements used in magnesium alloys on primary cells and cell lines10.1016/j.actbio.2009.09.024 ↗
11. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
12. Characterization methods of bone-implant-interfaces of bioresorbable and titanium implants by fracture mechanical means10.1016/j.jmbbm.2010.08.004 ↗
13. Bone–implant interface strength and osseointegration: biodegradable magnesium alloy versus standard titanium control10.1016/j.actbio.2010.08.020 ↗
14. Diffusion coefficients and solubility coefficients for gases in biological fluids and tissues: a review
15. Degradation behaviour and mechanical properties of magnesium implants in rabbit tibiae10.1007/s10853-009-3936-3 ↗
16. Preparation of SBF with different HCO3− content and its influence on the composition of biomimetic apatites10.1016/j.actbio.2005.11.001 ↗
17. An hydrogen evolution method for the estimation of the corrosion rate of magnesium alloys
18. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
19. Micro arc/spark anodizing – what is that?
20. Shapiro O. Bend testing. In: Kuhn H, Medlin D, editors. ASM handbook, vol. 8. Mechanical testing and evaluation. Materials Park, OH: ASM, International; 2000, p. 179–180
21. Corrosion of high purity Mg, Mg2Zn0.2Mn, ZE41 and AZ91 in Hank’s solution at 37°C10.1016/j.corsci.2011.06.030 ↗