Fracture modes and hybrid toughening mechanisms in oscillated/twisted plywood structure

Zhaoqiang Song, Yong Ni, Shengqiang Cai

Acta Biomaterialia· Volume 91
Publisher page

Abstract

Twisted or oscillated plywood structure can be often found in biological composites such as claws of lobsters, bone of mammals, dactyl club of mantis shrimps, and exoskeleton of beetles, which exhibits a combination of high stiffness, high fracture toughness and low density. However, there lacks a quantitative understanding of the relationship between the fracture toughness of the composite and its internal geometry. In this article, we propose that a combination of crack tilting and crack bridging determines the effective fracture toughness of the fiber-reinforced composite with the plywood structure. During the fracturing process, a crack plane initially propagates in the matrix-fiber interface following the twisted fiber alignment. Such crack tilting mechanism can significantly enlarge the area of cracking surface and thus enhance the effective fracture toughness of the composite. With the propagation of the tilted crack plane, the local energy release rate becomes too small to maintain the growth of the tilted crack plane, leading the crack to grow into the matrix, crossing the fibers. Because of the high strength of the fiber, a few fibers can maintain unbroken behind the crack tip, corresponding to crack bridging mechanism. Based on our quantitative analysis, it is found that the effective fracture toughness of the composite can be maximized for a certain pitch angle of the oscillated/twisted plywood structure, which agrees well with experiments. STATEMENTS OF SIGNIFICANCE: Fiber-reinforced composites can be widely found in nature and engineering applications. Recently, it has been discovered that many fiber-reinforced composites in biology have twisted or oscillated plywood structure with high fracture toughness, high mechanical stiffness and low density. Detailed experiments have indicated that an optimal pitch angle may exist for the plywood structure to maximize the fracture toughness of the composites. However, there lacks a quantitative model of revealing such pitch angle-dependent fracture toughness. In this work, we propose a hybrid toughening mechanism and predict the optimal pitch angle in twisted/oscillated plywood structure for maximizing the fracture toughness. Our predictions agree reasonably well with experimental results. As such, the theory may help the design of better fiber-reinforced composites.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silk-based biomaterials and applications · Calcium Carbonate Crystallization and Inhibition · Natural Fiber Reinforced Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Callister · 2011
2. Preparation of chitin nanofibers with a uniform width as alpha-chitin from crab shells10.1021/bm900163d ↗
3. Biomimetic anisotropic reinforcement architectures by electrically assisted nanocomposite 3D printing10.1002/adma.201605750 ↗
4. The material bone: structure-mechanical function relations
5. AFM identification of beetle exocuticle: bouligand structure and nanofiber anisotropic elastic properties10.1002/adfm.201603993 ↗
6. The stomatopod dactyl club: a formidable damage-tolerant biological hammer10.1126/science.1218764 ↗
7. Bio-inspired impact-resistant composites10.1016/j.actbio.2014.03.022 ↗
8. Twisting cracks in Bouligand structures10.1016/j.jmbbm.2017.06.010 ↗
9. Crack driving force in twisted plywood structures10.1016/j.actbio.2017.04.007 ↗
10. Crack twisting and toughening strategies in Bouligand architectures10.1016/j.ijsolstr.2018.06.004 ↗
11. Revealing the mechanics of helicoidal composites through additive manufacturing and beetle developmental stage analysis10.1002/adfm.201803073 ↗
12. The influence of the interphase and associated interfaces on the deflection of matrix cracks in ceramic matrix composites10.1016/S1359-835X(00)00095-6 ↗
13. Crack deflection processes—I. Theory10.1016/0001-6160(83)90046-9 ↗
14. Binary cellulose nanocrystal blends for bioinspired damage tolerant photonic films10.1002/adfm.201800032 ↗
15. Biomimetic twisted plywood structural materials10.1093/nsr/nwy080 ↗
16. Slightly curved or kinked cracks10.1007/BF00012619 ↗
17. A general mixed-mode brittle fracture criterion for cracked materials10.1016/j.engfracmech.2005.12.011 ↗
18. Experimental investigation of the elastic–plastic deformation of mineralized lobster cuticle by digital image correlation10.1016/j.jsb.2006.06.004 ↗
19. Time-lapse three-dimensional imaging of crack propagation in beetle cuticle10.1016/j.actbio.2019.01.031 ↗
20. Novel defense mechanisms in the armor of the scales of the “living fossil” coelacanth fish10.1002/adfm.201804237 ↗
21. Discontinuous crack-bridging model for fracture toughness analysis of nacre10.1016/j.jmps.2012.04.011 ↗
22. Optimal characteristic nanosizes of mineral bridges in mollusk nacre10.1039/C4RA04902K ↗
23. Toughening by aligned, frictionally constrained fibers10.1016/0022-5096(87)90006-8 ↗
24. Broberg · 1999
25. A multiscale crack-bridging model of cellulose nanopaper10.1016/j.jmps.2017.03.004 ↗
26. Nanopaper membranes from chitin-protein composite nanofibers-structure and mechanical properties
27. Chitin nanofibers, networks and composites: preparation, structure and mechanical properties
28. Materials become insensitive to flaws at nanoscale: lessons from nature10.1073/pnas.0631609100 ↗
29. An ultrastrong nanofibrillar biomaterial: the strength of single cellulose nanofibrils revealed via sonication-induced fragmentation10.1021/bm301674e ↗
30. Processing bulk natural wood into a high-performance structural material10.1038/nature25476 ↗