Abstract

Mechanically assisted crevice corrosion (MACC) has been associated with implant failure in vivo and is a serious concern in numerous metallic implant systems. Stainless steel medical devices may be subjected to fretting and crevice corrosion in the human body as are titanium and CoCrMo alloys due to the presence of a passive oxide film on their surface. One mechanism of MACC that has not been clearly identified and studied is fretting-initiated crevice corrosion (FICC) of stainless steel where an initial fretting event can initiate a rapid propagating crevice corrosion process even when fretting has ceased. FICC pin-on-disk experiments were performed at varying potential conditions and duration of fretting to explore the role of potential and fretting duration on the initiation of crevice corrosion. Triggering of a propagating crevice corrosion reaction on stainless steel at 250 mV vs Ag/AgCl/KCl (saturated) in PBS solution required only 2 s (2 cycles at 1 Hz) of fretting. Crevice corrosion continued to propagate under a 1.8 mm diameter pin with only 100 μm of direct contact, dissolving in both the depth and width dimension away from the fretting contact while the currents rose from 0.2 μA to 15 μA within 5 min. Three different potential-dependent FICC regions were identified that included unstable crevice corrosion (50 mV and above), metastable crevice corrosion (-100 mV to 0 mV) and stable fretting corrosion (between -500 mV and -150 mV). Crevice corrosion can be induced by fretting at potentials as low as -100 mV. Below -100 mV, there was no FICC, but rather fretting corrosion stopped immediately after fretting ceased and returned to a stable baseline current. Metastable FICC was shown at potentials between -100 mV and 0 mV, when the crevice corrosion current gradually decreased over several seconds or longer after fretting ceased. Self-sustained, unstable crevice corrosion started at 50 mV, where prior to fretting the currents were low, and after just a few cycles of fretting the crevice current rose rapidly and continued to increase after fretting stopped. Increase of potential increased the susceptibility of stainless steel to FICC. Scanning electron microscopy and digital optical microscopy revealed pitting and crevice corrosion on samples at -100 mV and higher potentials, where FICC was developing. By removing the oxide film, fretting motion significantly facilitates the critical crevice solution development, lowering the critical crevice potential and decreasing the initiation time for crevice corrosion. These results indicate that fretting initiated crevice corrosion may affect the performance of stainless steel in vivo. STATEMENT OF SIGNIFICANCE: AISI 316L stainless steel has been widely used as a metallic biomaterial for orthopaedic, spinal, dental and cardiovascular implants. Crevice corrosion has been a serious concern for stainless steel implants. For the first time we demonstrated and systematically studied the process of fretting-initiated crevice corrosion (FICC) in 316L stainless steel in simulated physiological solution of phosphate buffered saline. By removing the oxide film, fretting motion significantly facilitates the critical crevice solution development, lowering the critical crevice potential and decreasing the initiation time for crevice corrosion. Our findings indicate fundamental differences between the FICC mechanism and conventional crevice corrosion theory, showing that fretting can play a significant role in the initiation of crevice corrosion of stainless steel.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Orthopaedic implants and arthroplasty · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Metallic implant biomaterials10.1016/j.mser.2014.10.001 ↗
2. Biomaterials in orthopaedics10.1098/rsif.2008.0151 ↗
3. Electrochemical behavior of metals in the biological milieu
4. Special modes of corrosion under physiological and simulated physiological conditions10.1016/j.actbio.2007.12.003 ↗
5. The dynamics of oxide films on metallic biomaterials
6. Electrochemical and XPS studies of the passive film formed on stainless steels in borate buffer and chloride solutions10.1016/j.corsci.2006.11.001 ↗
7. Failures in stainless steel orthopaedic implant devices: A survey
8. Immuno-inflammatory tissue reaction to stainless-steel and titanium plates used for internal fixation of long bones10.1016/S0142-9612(02)00312-5 ↗
9. Late postoperative infection following spinal instrumentation: stainless steel versus titanium implants
10. Widespread dissemination of metal debris from implants10.1302/0301-620X.76B5.8083255 ↗
11. Periprosthetic osteolysis in total hip arthroplasty: the role of particulate wear debris10.2106/00004623-199509000-00022 ↗
12. Investigation of failures in stainless steel orthopaedic implant devices: pit-induced stress corrosion cracking
13. In vivo corrosion of modular hip prosthesis components in mixed and similar metal combinations. The effect of crevice, stress, motion, and alloy coupling10.1002/jbm.820271210 ↗
14. Y. Liu, The Effects of Simulated Inflammatory Conditions on the Corrosion and Fretting Corrosion of CoCrMo alloy (Ph.D thesis), Syracuse University, 2017, Retrieved from https://surface.syr.edu/etd/705/.10.1016/j.wear.2017.08.011 ↗
15. Corrosion at the cone/taper interface leads to failure of large-diameter metal-on-metal total hip arthroplasties10.1007/s11999-012-2502-5 ↗
16. Corrosion at the head-neck taper as a cause for adverse local tissue reactions after total hip arthroplasty10.2106/JBJS.K.01352 ↗
17. Fretting corrosion of CoCrMo and Ti6Al4V interfaces10.1016/j.biomaterials.2012.04.015 ↗
18. Fretting-corrosion of materials used as orthopaedic implants10.1016/j.wear.2004.11.027 ↗
19. Area-dependent impedance-based voltage shifts during tribocorrosion of Ti-6Al-4V biomaterials: theory and experiment10.1088/2051-672X/4/3/034002 ↗
20. Electrochemical effects on the fretting corrosion behaviour of Ti6Al4V in 0.9% sodium chloride solution10.1016/j.wear.2004.12.012 ↗
21. Susceptibility to crevice corrosion and metastable pitting of stainless steels
22. Crevice corrosion of stainless steels: II. Experimental studies10.1179/000705978798276258 ↗
23. Crevice corrosion of stainless steels: I. a mathematical model10.1179/000705978798358671 ↗
24. On the mechanism of localized corrosion of iron and stainless steel I. Electrochemical studies10.1149/1.2403982 ↗
25. The initial potential and current distributions of the crevice corrosion process10.1149/1.2056139 ↗
26. Sudden onset of pitting corrosion on stainless steel as a critical phenomenon10.1126/science.1101358 ↗
27. Environmental factors affecting the critical potential for pitting in 18–8 stainless steel10.1149/1.2423801 ↗
28. Crevice corrosion of stainless steels in sodium chloride solution10.1016/0010-938X(78)90030-6 ↗
29. The crevice corrosion behavior of stainless steel in sodium chloride solution10.1016/j.corsci.2011.08.012 ↗
30. Fretting corrosion accelerates crevice corrosion of modular hip tapers10.1002/jab.770060104 ↗
31. Fretting crevice corrosion of stainless steel stem–CoCr femoral head connections: comparisons of materials, initial moisture, and offset length10.1002/jbm.b.31164 ↗
32. Effect of mixed alloy combinations on fretting corrosion performance of spinal screw and rod implants10.1002/jbm.b.33661 ↗
33. Zhu · 2016
34. In situ monitoring of crevice corrosion morphology of Type 316L stainless steel and repassivation behavior induced by sulfate ions10.1016/j.corsci.2017.08.005 ↗
35. The effect of simulated inflammatory conditions and pH on fretting corrosion of CoCrMo alloy surfaces10.1016/j.wear.2017.08.011 ↗
36. Effect of simulated inflammatory conditions and potential on dissolution and surface oxide of CoCrMo alloy: In situ electrochemical atomic force microscopy study10.1016/j.electacta.2017.12.151 ↗
37. In situ investigation of crevice corrosion on UNS S32101 duplex stainless steel in sodium chloride solution10.1016/j.corsci.2013.06.039 ↗
38. Modeling fretting-corrosion wear of 316L SS against poly (methyl methacrylate) with the point defect model: Fundamental theory, assessment, and outlook10.1016/j.electacta.2012.06.028 ↗
39. The effect of crevice-opening dimension on the stability of crevice corrosion for nickel in sulfuric acid10.1149/1.1838632 ↗
40. I. Matsushima, J. Sakai, K. Masamura. Mechanism of crevice corrosion, in: Proceedings of the Seventh International Congress on Metallic Corrosion, Rio De Janeiro, Brazil, 1978.
41. Friction–corrosion of AISI 316L/bone cement and AISI 316L/PMMA contacts: Ionic strength effect on tribological behavior10.1016/j.wear.2008.12.087 ↗
42. Corrosion of spinal implants retrieved from patients with scoliosis10.1007/s00776-004-0867-3 ↗
43. In vivo corrosion of 316L stainless-steel hip implants: morphology and elemental compositions of corrosion products10.1016/S0142-9612(97)00208-1 ↗
44. Corrosion of bio implants10.1007/BF02706450 ↗
45. Characterization and cytotoxicity of ions released from stainless steel and nickel-titanium orthodontic alloys10.1016/j.ajodo.2003.09.009 ↗
46. The biological response to orthopaedic implants for joint replacement: Part I: Metals10.1002/jbm.b.33734 ↗
47. The effect of simulated inflammatory conditions and Fenton chemistry on the electrochemistry of CoCrMo alloy10.1002/jbm.b.33830 ↗
48. Effects of simulated inflammation on the corrosion of 316L stainless steel10.1016/j.msec.2016.10.012 ↗
49. No corrosion of 304 stainless steel implant after 40 years of service10.1023/B:JMSM.0000032814.20695.3c ↗
50. Direct in vivo inflammatory cell-induced corrosion of CoCrMo alloy orthopedic implant surfaces10.1002/jbm.a.35165 ↗
51. Clinical relevance of corrosion patterns attributed to inflammatory cell-induced corrosion: A retrieval study10.1002/jbm.b.33540 ↗
52. A synergistic effect of albumin and H2O2 accelerates corrosion of Ti6Al4V10.1016/j.actbio.2015.07.046 ↗
53. Evidence for the dissolution of molybdenum during tribocorrosion of CoCrMo hip implants in the presence of serum protein10.1016/j.actbio.2016.08.051 ↗