Linking naturally and unnaturally spun silks through the forced reeling of Bombyx mori
Source abstract
Abstract
The forced reeling of silkworms offers the potential to produce a spectrum of silk filaments, spun from natural silk dope and subjected to carefully controlled applied processing conditions. Here we demonstrate that the envelope of stress-strain properties for forced reeled silks can encompass both naturally spun cocoon silk and unnaturally processed artificial silk filaments. We use dynamic mechanical thermal analysis (DMTA) to quantify the structural properties of these silks. Using this well-established mechanical spectroscopic technique, we show high variation in the mechanical properties and the associated degree of disordered hydrogen-bonded structures in forced reeled silks. Furthermore, we show that this disorder can be manipulated by a range of processing conditions and even ameliorated under certain parameters, such as annealing under heat and mechanical load. We conclude that the powerful combination of forced reeling silk and DMTA has tied together native/natural and synthetic/unnatural extrusion spinning. The presented techniques therefore have the ability to define the potential of Bombyx-derived proteins for use in fibre-based applications and serve as a roadmap to improve fibre quality via post-processing.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silk-based biomaterials and applications · Silkworms and Sericulture Research · Insect and Arachnid Ecology and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (68)
Show source-provided references
1. Evolution of arthropod silks10.1146/annurev.ento.42.1.231 ↗
2. Silk as a biomimetic ideal for structural polymers10.1002/adma.200801332 ↗
3. Structure and physical properties of silkworm cocoons10.1098/rsif.2011.0887 ↗
4. Effect of degumming on the tensile properties of silkworm (Bombyx mori) silk fiber10.1002/app.10366 ↗
5. Mechanism of silk processing in insects and spiders10.1038/nature01809 ↗
6. Natural and unnatural silks10.1016/j.polymer.2007.04.019 ↗
7. Preparation and characterization of regenerated Bombyx mori silk fibroin fiber with high strength10.3144/expresspolymlett.2008.103 ↗
8. Silk materials - a road to sustainable high technology10.1002/adma.201104477 ↗
9. Enhancing the toughness of regenerated silk fibroin film through uniaxial extension10.1021/bm100643q ↗
10. Silk-based biomaterials10.1016/S0142-9612(02)00353-8 ↗
11. Correlation between structural and dynamic mechanical transitions of regenerated silk fibroin10.1016/j.polymer.2010.10.046 ↗
12. Regenerated silk fibroin films: thermal and dynamic mechanical analysis10.1002/1521-3935(200207)203:10/11<1658::AID-MACP1658>3.0.CO;2-3 ↗
13. Physical properties and structure of silk 2. Dynamic mechanical and dielectric properties of silk fibroin
14. Structure and molecular conformation of tussah silk fibroin films treated with water–methanol solutions: dynamic mechanical and thermomechanical behavior10.1002/(SICI)1099-0488(19981115)36:15<2717::AID-POLB5>3.0.CO;2-O ↗
15. Thermal behavior of regenerated Antheraea pernyi silk fibroin film treated with aqueous methanol10.1016/S0032-3861(00)00100-2 ↗
16. Toughness of spider silk at high and low temperatures10.1002/adma.200400344 ↗
17. Thermally induced changes in dynamic mechanical properties of native silks10.1021/bm400012k ↗
18. Silks cope with stress by tuning their mechanical properties under load10.1016/j.polymer.2012.04.017 ↗
19. Two mechanisms for supercontraction in Nephila spider dragline silk10.1021/bm201032v ↗
20. Studies on physical-properties and structure of silk – glass-transition and crystallization of silk fibroin10.1002/app.1975.070190410 ↗
21. Physical properties and structure of silk 3. Glass-transition and conformational changes of tussah silk fibroin10.1002/app.1977.070210909 ↗
22. Physical properties and structure of silk. X1. Glass-transition temperature of wild silk fibroins10.1002/app.1986.070310319 ↗
23. Dicko C, Kenney JM, Vollrath F, Andrey Kajava JMSaDADP. Beta-Silks: Enhancing and Controlling Aggregation. New York: Academic Press; 2006. p. 17–53.10.1016/S0065-3233(06)73002-9 ↗
24. Small angle neutron scattering of native and reconstituted silk fibroin10.1039/c0sm00108b ↗
25. Concentration state dependence of the rheological and structural properties of reconstituted silk10.1021/bm900452u ↗
26. X-ray diffraction on spider silk during controlled extrusion under a synchrotron radiation X-ray beam10.1021/bm000047c ↗
27. Elucidating silk structure using solid-state NMR10.1039/c3sm52187g ↗
28. McCrum · 1967
29. Spider silk as a model biomaterial10.1007/s00339-005-3437-4 ↗
30. Spider silk as an archetypal protein elastomer10.1039/b600098n ↗
31. Porter · 1995
32. Predictive nonlinear constitutive relations in polymers through loss history10.1016/j.ijsolstr.2009.01.012 ↗
33. Dynamic protein-water relationships during beta-sheet formation10.1021/ma071551d ↗
34. Determining beta-sheet crystallinity in fibrous proteins by thermal analysis and infrared spectroscopy10.1021/ma0610109 ↗
35. Structural characteristics and properties of the regenerated silk fibroin prepared from formic acid10.1016/S0141-8130(01)00159-3 ↗
36. Time-resolved structural investigation of regenerated silk fibroin nanofibers treated with solvent vapor10.1016/j.ijbiomac.2006.02.009 ↗
37. Effect of metallic ions on silk formation the mulberry silkworm, Bombyx mori10.1021/jp050883m ↗
38. Silk self-assembly mechanisms and control from thermodynamics to kinetics10.1021/bm201731e ↗
39. Mechanical properties of robust ultrathin silk fibroin films10.1002/adfm.200601136 ↗
40. Silk fibers extruded artificially from aqueous solutions of regenerated Bombyx mori silk fibroin are tougher than their natural counterparts10.1002/adma.200800582 ↗
41. Using solvents with different molecular sizes to investigate the structure of Antheraea pernyi silk10.1021/bm401056x ↗
42. There are many more lessons still to be learned from spider silks10.1039/c1sm05812f ↗
43. Surprising strength of silkworm silk10.1038/418741a ↗
44. Tensile properties of silkworm silk obtained by forced silking10.1002/app.2038 ↗
45. Forced reeling of Bombyx mori silk: separating behaviour and processing conditions10.1021/bm401013k ↗
46. Structural characteristics and properties of Bombyx mori silk fiber obtained by different artificial forcibly silking speeds10.1016/j.ijbiomac.2007.12.001 ↗
47. Some observations on the structure and function of the spinning apparatus in the silkworm Bombyx mori10.1021/bm060874z ↗
48. Extended wet-spinning can modify spider silk properties10.1039/b500319a ↗
49. Beta transition and stress-induced phase separation in the spinning of spider dragline silk10.1016/S0141-8130(00)00124-0 ↗
50. Relationships between supercontraction and mechanical properties of spider silk10.1038/nmat1534 ↗
51. Structure development in biaxially stretched polystyrene film. I. Property-orientation correlation10.1002/pen.760292105 ↗
52. Structure of oriented polystyrene monofilaments and its relationship to brittle-to-ductile transition10.1002/app.1978.070220613 ↗
53. Brittle-to-ductile transition based upon amorphous orientation of polystyrene monofilaments10.1002/app.1978.070220927 ↗
54. Biaxial orientation behavior of polystyrene: Orientation and properties10.1002/app.12268 ↗
55. Investigation of rheological properties and conformation of silk fibroin in the solution of AmimCl10.1021/bm300387z ↗
56. Wet-spinning of regenerated silk fiber from aqueous silk fibroin solution: Discussion of spinning parameters10.1021/bm900840h ↗
57. Kinetics of thermally-induced conformational transitions in soybean protein films10.1016/j.polymer.2010.03.032 ↗
58. Sample selection, preparation methods, and the apparent tensile properties of silkworm (B. mori) cocoon silk10.1002/bip.22005 ↗
59. The impact behaviour of silk cocoons10.1242/jeb.082545 ↗
60. In situ tensile tests of single silk fibres in an environmental scanning electron microscope10.1007/s10853-013-7293-x ↗
61. The crystal modulus and structure of oriented poly(ethylene terephthalate)10.1016/0032-3861(88)90201-7 ↗
62. Spider silk protein refolding is controlled by changing pH10.1021/bm034307c ↗
63. Metal element contents in silk gland and silk fiber of Bombyx mori silkworm
64. Copper in the silk formation process of Bombyx mori silkworm10.1016/S0014-5793(03)01184-0 ↗
65. Further Investigation on potassium-induced conformation transition of Nephila spidroin film with two-dimensional infrared correlation spectroscopy10.1021/bm049598j ↗
66. Role of pH and charge on silk protein assembly in insects and spiders10.1007/s00339-005-3426-7 ↗
67. Effect of sodium chloride on the structure and stability of spider silk’s N-terminal protein domain10.1039/c2bm00140c ↗
68. Spidroin N-terminal domain promotes a pH-dependent association of silk proteins during self-assembly10.1074/jbc.M110.163121 ↗