Influence of the microstructure and topography on the barrier properties of oxide scales generated on blasted Ti6Al4V surfaces
Source abstract
Abstract
The long-term interfacial bond between an implant and bone may be improved by creating a rough surface on the implant in order to increase the surface area available for bone/implant apposition. A natural consequence of surface roughening is an increase in metal ion release, which is itself a surface dominated process. Based on this fact, the aim of this work is to study the influence of the microstructure and topography on the barrier properties of oxide scales thermally generated at 700 °C for 1h on Ti6Al4V surfaces after blasting with Al(2)O(3) particles (coarse) or SiO(2) and ZrO(2) particles (fine). The microstructural and topographical characterization of the thermally treated blasted surfaces has been studied by means of scanning electron microscopy coupled with energy dispersive X-ray analysis, contact profilometry and X-ray diffraction. The barrier properties and corrosion behaviour of the oxide layers have been studied by means of electrochemical impedance spectroscopy (EIS) in Hank's solution. Thermal treatment at 700 °C for 1h promotes the formation of oxide scales with different morphologies and crystalline structures depending on the degree of deformation of the blasted surface. The oxide scale grown on the finely blasted sample has a pine needle-like morphology which is mainly formed of anatase TiO(2). In contrast, the oxide scale grown on the coarsely blasted sample has a globular morphology formed mainly of rutile TiO(2). The differences in morphology, i.e. fine or coarse, of the oxide scales influence the corrosion response of the blasted thermally treated samples in Hank's solution. The EIS results permit evaluation of the different oxide scales from the capacitance and resistance values obtained in the high-frequency region and show a good correlation between the morphology and barrier properties. Oxidation treatment at 700 °C for 1h of Ti6Al4V samples coarsely blasted with Al(2)O(3) improves the corrosion behaviour due to an increase in the thickness of a compact, ordered and more structurally stable oxide scale. This is due to the globular morphology of the rutile (TiO(2)) structure maintaining an average surface roughness suitable for optimal osseo-integration with long-term interfacial bonding between the implant and bone.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Metal wear particle characterization from metal on metal total hip replacements: transmission electron microscopy study of periprosthetic tissues and isolated particles10.1002/(SICI)1097-4636(199810)42:1<103::AID-JBM13>3.0.CO;2-M ↗
2. Repassivation of titanium and surface oxide film regenerated in simulated bioliquid10.1002/(SICI)1097-4636(19980615)40:4<530::AID-JBM3>3.0.CO;2-G ↗
3. Titanium alloys as implant materials
4. Cellular Ti–6Al–4V structures with interconnected macro porosity for bone implants fabricated by selective electron beam melting10.1016/j.actbio.2008.03.013 ↗
5. Effect of mechanical surface pre-treatment on metal ion release10.1016/S0142-9612(99)00200-8 ↗
6. Characterization of roughness and pitting corrosion of surfaces modified by blasting and thermal oxidation10.1016/j.surfcoat.2010.04.051 ↗
7. 3D, chemical and electrochemical characterization of blasted Ti6Al4V surfaces: its influence on the corrosion behaviour10.1016/j.electacta.2006.12.031 ↗
8. Surface modification of titanium alloy implants10.1016/0142-9612(94)90113-9 ↗
9. Effect of the surface treatment on the dissolution of titanium based implant materials10.1016/0142-9612(91)90144-Y ↗
10. Stability of titanium and zirconium anodic films in nitric-acid solutions – EIS comparative investigation
11. Examination of clinical surface preparations on titanium and Ti6Al4V by X-ray photoelectron-spectroscopy and nuclear reaction analysis10.1016/0079-6816(95)00061-5 ↗
12. Nitric-acid passivation of Ti6Al4V reduces thickness of surface oxide layer and increases trace-element release10.1002/jbm.820290302 ↗
13. A histomorphometric analysis of the effects of various surface treatment methods on osseointegration
14. In vitro corrosion behaviour and osteoblast response of thermally oxidised Ti6Al4V alloy10.1016/S0142-9612(02)00237-5 ↗
15. Concentration dependent effect of titanium and aluminium ions released from thermally oxidized Ti6Al4V alloy on human osteoblasts10.1002/jbm.a.30599 ↗
16. Thermal oxidation enhances early interactions between human osteoblasts and alumina blasted Ti6Al4V alloy10.1002/jbm.a.30994 ↗
17. Effect of titanium surface roughness on proliferation, differentiation, and protein synthesis of human osteoblast-like cells (MG63)10.1002/jbm.820290314 ↗
18. Topography effects of pure titanium substrates on human osteoblast long-term adhesion10.1016/j.actbio.2004.11.009 ↗
19. Response of MG63 osteoblast-like cells to titanium and titanium alloy is dependent on surface roughness and composition10.1016/S0142-9612(98)00144-6 ↗
20. The effects of implant surface nanoscale features on osteoblast-specific gene expression10.1016/j.biomaterials.2009.04.010 ↗
21. Quantitative evaluation of residual grits under angled blasting10.1016/S0257-8972(98)00482-4 ↗
22. Corrosion behaviour of commercially pure titanium shot blasted with different materials and sizes of shot particles for dental implant applications10.1016/S0142-9612(02)00314-9 ↗
23. High-temperature oxidation behavior of pure Ni3Al10.1007/BF01046884 ↗
24. Characterization of implant materials in fetal bovine serum and sodium sulfate by electrochemical impedance spectroscopy. I. Mechanically polished samples10.1002/jbm.10329 ↗
25. Correlation of morphology and barrier properties of thin microwave plasma polymer films on metal substrate10.1016/j.electacta.2003.12.030 ↗
26. Corrosion of protected aluminum and zinc10.1016/0010-938X(93)90152-7 ↗
27. Geenen FM, van Westing EPM, de Wit JHW. An impedance spectroscopy study of the degradation mechanism for a model coated surface. In: Proceedings of the 11th International Corrosion Congress, Florence; 1990. p. 2.231.
28. A review of impedance plot methods used for corrosion performance analysis10.1016/0010-938X(86)90033-8 ↗
29. Recording and analysis of AC impedance data for corrosion studies 2. Experimental approach and results10.5006/1.3577304 ↗
30. The application of impedance methods to study the effects of water uptake and chloride ion concentration on the degradation of films – I. Attached films10.1016/0010-938X(91)90094-6 ↗
31. Electrochemical impedance spectroscopy on 3-D inhomogeneous surfaces – corrosion in neutral aerated solutions10.1149/1.2095610 ↗
32. An interpretation of electrical impedance diagrams for galvanized steel10.1016/0033-0655(89)80020-2 ↗