Abstract
Abstract Magnetic properties and magnetocaloric effect in (Fe 0.76 − x Tm x B 0.24 ) 96 Nb 4 ( x = 0, 0.01, 0.05, 0.1, 0.17 and 0.18) metallic glasses have been studied. The appropriate substitution of Fe by Tm increases the glass-forming ability of the alloys and allows tuning the Curie temperature ( T C ) to near room temperature. A linear relationship between magnetic entropy change and saturation magnetization has been observed. The formation of minority nanocrystalline Tm 2 Fe 14 B 1 phase has been observed at higher Tm additions, which could influence the magnetocaloric effect of the alloy. These Tm doped Fe-based alloys, with enhanced thermal stability, good magnetocaloric responses and tunable T C , are good candidates for near room-temperature magnetic refrigerants.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic and transport properties of perovskites and related materials · Magnetic Properties of Alloys · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Gschneidner · Rep. Prog. Phys. · 2005 · 68 · 147910.1088/0034-4885/68/6/R04 ↗
2. Smith · Adv. Energy Mater. · 2012 · 2 · 128810.1002/aenm.201200167 ↗
3. Sandeman · Scr. Mater. · 2012 · 67 · 56610.1016/j.scriptamat.2012.02.045 ↗
4. Franco · Annu. Rev. Mater. Res. · 2012 · 42 · 30510.1146/annurev-matsci-062910-100356 ↗
5. Pecharsky · Phys. Rev. Lett. · 1997 · 78 · 449410.1103/PhysRevLett.78.4494 ↗
6. Tegus · Nature · 2002 · 415 · 15010.1038/415150a ↗
7. Liu · Nat. Mater. · 2012 · 11 · 62010.1038/nmat3334 ↗
8. Caballero-Flores · J. Appl. Phys. · 2010 · 108 · 07392110.1063/1.3489990 ↗
9. Caballero-Flores · Appl. Phys. Lett. · 2010 · 96 · 18250610.1063/1.3427439 ↗
10. Mishra · Mater. Sci. Eng. B · 2010 · 175 · 25310.1016/j.mseb.2010.07.038 ↗
11. Law · J. Alloys Compd. · 2010 · 508 · 1410.1016/j.jallcom.2010.08.049 ↗
12. Law · Appl. Phys. Lett. · 2011 · 98 · 19250310.1063/1.3589353 ↗
13. Ipus · IEEE Trans. Magn. · 2011 · 47 · 249410.1109/TMAG.2011.2159781 ↗
14. Franco · Scr. Mater. · 2012 · 67 · 59410.1016/j.scriptamat.2012.05.004 ↗
15. Ucar · JOM · 2012 · 64 · 78210.1007/s11837-012-0349-6 ↗
16. Thanh · J. Appl. Phys. · 2013 · 113 · 21390810.1063/1.4809754 ↗
17. Zhang · J. Magn. Magn. Mater. · 2013 · 347 · 13110.1016/j.jmmm.2013.07.020 ↗
18. Waske · J. Magn. Magn. Mater. · 2013 · 329 · 10110.1016/j.jmmm.2012.10.003 ↗
19. Li · J. Appl. Phys. · 2014 · 116 · 06390210.1063/1.4892431 ↗
20. Podmiljsak · J. Alloys Compd. · 2014 · 591 · 2910.1016/j.jallcom.2013.12.150 ↗
21. Huo · J. Non-Cryst. Solids · 2013 · 359 · 110.1016/j.jnoncrysol.2012.09.020 ↗
22. Li · J. Alloys Compd. · 2014 · 617 · 33210.1016/j.jallcom.2014.07.222 ↗
23. Suryanarayana · Int. Mater. Rev. · 2013 · 58 · 13110.1179/1743280412Y.0000000007 ↗
24. Hirosawa · J. Appl. Phys. · 1986 · 59 · 87310.1063/1.336611 ↗
25. Gschneidner · Cryocoolers · 2003 · 12 · 45710.1007/0-306-47919-2_61 ↗
26. Legvold · 1980 · vol. 1 · 189
27. Zhang · Appl. Phys. Lett. · 2006 · 89 · 13190410.1063/1.2357160 ↗
28. Li · J. Non-Cryst. Solids · 2013 · 365 · 4210.1016/j.jnoncrysol.2013.01.033 ↗
29. Sayouty · J. Alloys Compd. · 2005 · 397 · 4710.1016/j.jallcom.2005.01.047 ↗