Investigation of the role of Mg and Ca in the structure and durability of aluminoborosilicate glass

D.J. Backhouse, C.L. Corkhill, N.C. Hyatt, R.J. Hand

Abstract

The structure and dissolution behaviour of Na2O∙CaO∙(15–x)Al2O3∙xB2O3∙SiO2 and Na2O∙MgO∙(15–x)Al2O3∙xB2O3∙SiO2 glasses, relevant to compositions of UK nuclear waste glass, have been investigated using nuclear magnetic resonance (NMR) spectroscopy and static dissolution experiments using the PCT protocol. Structural data from 11B, 27Al and 29Si NMR analyses show that increasing the Increasing the [B2O3]/([Al2O3]+[B2O3]) ratio of the alkali-alkaline-earth aluminoborosilicate glasses led to an overall decrease in the proportion of non-silicate tetrahedral species (IVAl + IVB) and a decrease in Si – O – X bonds (X = B, Al). The Mg-containing glasses exhibited lower IVB fractions than their Ca-containing counterparts, which is thought to be due to the presence of IVMg tetrahedra in the network. The measured corrosion rates were similar for both Ca and Mg-containing glasses although unexpectedly some Ca-containing glasses exhibited higher corrosion losses than the Mg-containing ones for time periods up to 112 d. However, there was evidence of a greater tendency to rate resumption in the Mg containing than the Ca containing ones. Alteration products were found to contain Ca, Si and Al with the Ca containing glasses and Ca, Mg, Si and Al with the Mg containing glasses; Na was not detected in the alteration products although its presence cannot be ruled out based on the data obtained.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Glass properties and applications · Nuclear materials and radiation effects · Luminescence Properties of Advanced Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. International research on vitrified HLW long-term behaviour:state of the art
2. Vitrification of UK intermediate level radioactive wastes arising from site decommissioning: property modelling and selection of candidate host glass compositions
3. Alteration layer formation of Ca- and Zn-oxide bearing alkali borosilicate glasses for immobilisation of UK high level waste: a vapour hydration study10.1016/j.jnucmat.2016.06.009 ↗
4. Structural identification of a trioctahedral smectite formed by the aqueous alteration of a nuclear glass10.1016/j.clay.2010.04.016 ↗
5. The dual effect of Mg on the long-term alteration rate of AVM nuclear waste glasses10.1016/j.jnucmat.2012.05.025 ↗
6. Na, Mg, Ni and Cs distribution and speciation after long-term alteration of a simulated nuclear waste glass: a micro-XAS/XRF/XRD and wet chemical study10.1016/j.gca.2009.01.032 ↗
7. The effect of composition on the leaching of three nuclear waste glasses: R7T7, AVM and VRZ10.1016/j.jnucmat.2005.06.023 ↗
8. Glass-water interphase reactivity with calcium rich solutions10.1016/j.gca.2011.05.005 ↗
9. Dissolution of vitrified wastes in a high-pH calcium-rich solution10.1016/j.jnucmat.2012.12.032 ↗
10. Department of Energy & Climate Change · 2014
11. Research, Development and Demonstration (RD&D) “Plan for the geological disposal of high-level and/or long-lived radioactive waste including irradiated fuel of considered as waste, State-of-the-art report as of December 2012.”
12. SON 68 nuclear glass alteration kinetics between pH 7 and pH 11.510.1016/S0022-3115(01)00434-2 ↗
13. The kinetics and mechanisms of simulated British Magnox waste glass dissolution as a function of pH, silicic acid activity and time in low temperature aqueous systems10.1016/S0883-2927(99)00118-3 ↗
14. Dissolution of nepheline, jadeite and albite glasses: toward better models for aluminosilicate dissolution10.1016/S0016-7037(01)00724-4 ↗
15. An experimental study of the dissolution rates of simulated aluminoborosilicate waste glasses as a function of pH and temperature under dilute conditions10.1016/j.apgeochem.2008.05.006 ↗
16. Formation of alteration products during dissolution of vitrified ILW in a high-pH calcium-rich solution10.1016/j.jnucmat.2013.08.026 ↗
17. Dissolution of UK high-level waste glass under simulated hyperalkaline conditions of a collocated geological disposal facility10.1111/ijag.12042 ↗
18. Standard test methods for determining chemical durability of nuclear, hazardous, and mixed waste glasses and multiphase glass ceramics: the product consistency test (PCT)
19. Description of input and examples for PHREEQC version 3—a computer program for speciation, batch-reaction, one-dimensional transport, and inverse geochemical calculations
20. Mackenzie · 2002
21. Corrosion of the International Simple Glass (ISG) under acidic to hyperalkaline conditions10.1038/s41529-018-0050-5 ↗
22. The tobermorite supergroup: a new nomenclature10.1180/minmag.2015.079.2.22 ↗
23. Nuclear magnetic resonance studies of alkaline earth phosphosilicate and aluminoborosilicate glasses10.1016/S0022-3093(00)00056-9 ↗
24. Nuclear magnetic resonance studies of 0.139MO (or M′2O)·0.673SiO2·(0.188−x)Al2O3·xB2O3 (M=Mg, Ca, Sr and Ba, M′=Na and K) glasses10.1016/j.jnoncrysol.2003.08.086 ↗
25. Predicting the preference for charge compensation in silicate glasses Phys
26. Thermochemistry and structure of glasses along the join NaAlSi3O8-NaBSi3O810.1016/0016-7037(88)90297-9 ↗
27. The structure of aluminosilicate glasses: high-resolution 17O and 27Al MAS and 3QMAS NMR study10.1021/jp994273w ↗
28. The distribution of aluminum in the tetrahedra of silicates and aluminates
29. The effect of magnesium on the local structure and initial dissolution rate of simplified UK Magnox waste glasses10.1016/j.jnoncrysol.2018.03.002 ↗
30. Experimental determination of the effect of the ratio of B/Al on glass dissolution along the nepheline (NaAlSiO4)-malinkoite (NaBSiO4) join10.1016/j.gca.2009.09.006 ↗
31. Basaltic glass: alteration mechanisms and analogy with nuclear waste glasses10.1016/S0022-3115(00)00399-8 ↗
32. The immobilization of high level radioactive wastes using ceramics and glasses10.1023/A:1018646507438 ↗
33. The effect of composition on the leaching of three nuclear waste glasses: R7T7, AVM and VRZ10.1016/j.jnucmat.2005.06.023 ↗
34. Long-term corrosion of two nuclear waste reference glasses (MW and SON68): a kinetic and mineral alteration study10.1016/j.apgeochem.2006.03.010 ↗
35. Dolomite effect on borosilicate glass alteration10.1016/j.apgeochem.2013.02.019 ↗
36. HLW glass dissolution in the presence of magnesium carbonate: diffusion cell experiment and coupled modeling of diffusion and geochemical interactions10.1016/j.jnucmat.2013.07.068 ↗
37. Mineralogy and thermodynamic properties of magnesium phyllosilicates formed during the alteration of a simplified nuclear glass10.1016/j.jnucmat.2016.04.008 ↗