A.C impedance, XRD, DSC, FTIR studies on PbTiO3 dispersoid pristine PVdF-co-HFP and PEMA blended PVdF-co-HFP microcomposite electrolytes
Source abstract
Abstract
Abstract A.C impedance, XRD and thermal and FTIR studies were carried out for pristine PVdF-co-HFP(30 wt.%)/PbTiO 3 (5 wt.%) polymer microcomposite electrolyte membranes (PMCEs) by varying three EC:DMC–LiBETI compositions (62.5:2.5 (NP2), 60.0:5.0 (NP3) and 57.5:7.5 (NP4) wt.%). The higher conductivity was noted 7.99 × 10 − 5 S cm − 1 for NP4 and this account for better mobility of Li + free cations. The studies were repeated by blending PEMA with PVdF-co-HFP in three blend ratios i.e., 7.5:22.5 (NP6) wt.% (1:3), 15:15 (NP7) wt.% (1:1) and 22.5:7.5 (NP8) wt.% (3:1) for the same EC/DMC–LiBETI compositions. While blending, the conductivity was decreased in general, and among the blend ratio, higher conductivity noted 4.60 × 10 − 5 S cm − 1 for 3:1 (NP8) however it was lower than the pristine NP4. The temperature dependence of PMCE pristine and blended systems obeys Arrhenius behavior. The XRD diffractogram registers the dominance of lead titanate in pristine and blended systems albeit intensity variations. In DSC studies, variation of ΔH m and T m was noted due to PEMA, and hindrance of VdF crystallites was observed within its melting endotherm T m range due to fixed dispersoid PbTiO 3 which suggests that 3:1 ratio with 2.5 wt.% LiBETI with 5 wt.% PbTiO 3 showed better thermal stability. DSC studies had not registered the effect of PEMA in the thermal scale scanned than pristine PMCEs. FTIR investigation confirms molecular interactions in the vibrational range 400–2000 cm − 1 w.r.t. C O, C–F and C–H stretchings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advanced Battery Technologies Research · Advancements in Battery Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Ramesh · Solid State Ionics · 2002 · 152–153 · 29110.1016/S0167-2738(02)00311-9 ↗
2. Kufian · Solid State Ionics · 2012 · 208 · 3610.1016/j.ssi.2011.11.032 ↗
3. Shanmukaraj · J. Phys. Chem. Solids · 2008 · 69 · 24310.1016/j.jpcs.2007.08.072 ↗
4. Voigt · Solid State Ionics · 2012 · 208 · 810.1016/j.ssi.2011.11.031 ↗
5. Johan · Solid State Ionics · 2011 · 196 · 4110.1016/j.ssi.2011.06.001 ↗
6. Young · Macromolecules · 2009 · 42 · 267210.1021/ma802799p ↗
7. Magistris · Solid State Ionics · 2002 · 152-153 · 34710.1016/S0167-2738(02)00335-1 ↗
8. Phase Inversion Membranes
9. Tarascon · Solid State Ionics · 1996 · 86 · 4910.1016/0167-2738(96)00330-X ↗
10. Abraham · J. Electrochem. Soc. · 1990 · 137 · 165710.1149/1.2086749 ↗
11. Choe · Electrochim. Acta · 1995 · 40 · 228910.1016/0013-4686(95)00180-M ↗
12. Liu · J. Membr. Sci. · 2011 · 375 · 110.1016/j.memsci.2011.03.014 ↗
13. Ding · J. Membr. Sci. · 2009 · 329 · 5610.1016/j.memsci.2008.12.024 ↗
14. Pandey · Indian J. Chem. · 2010 · 49A · 743
15. Sukeshini · Solid State Ionics · 1996 · 86–88 · 38510.1016/0167-2738(96)00156-7 ↗
16. Appetechi · J. Electrochem. Soc. · 1996 · 143 · 610.1149/1.1836379 ↗
17. Rudhziah · Solid State Sci. Technol. · 2009 · 17 · 73
18. Han · J. Power Sources · 2002 · 112 · 46110.1016/S0378-7753(02)00436-6 ↗
19. 2003 · 3 · 253
20. Rajendran · Int. J. Electrochem. Sci. · 2008 · 3 · 28210.1016/S1452-3981(23)15453-8 ↗
21. Al-Saigh · Macromolecules · 1991 · 24 · 378810.1021/ma00013a008 ↗
22. Kwei · Macromolecules · 1976 · 9 · 78010.1021/ma60053a018 ↗
23. Sivakumar · Eur. Polym. J. · 2007 · 43 · 446610.1016/j.eurpolymj.2007.08.001 ↗
24. Vickraman · Ionics · 2010 · 16 · 76310.1007/s11581-010-0467-5 ↗
25. Ramesh · J. Mol. Struct. · 2011 · 994 · 40310.1016/j.molstruc.2011.03.065 ↗
26. Sim · Vib. Spectrosc. · 2012 · 58 · 5710.1016/j.vibspec.2011.11.005 ↗